(EN) The invention relates to a hydrocarbon polymer with polyether and polyolefin blocks, which is liquid or solid at room temperature, comprising at least one alkoxysilane end group, the silylated polymer of formula (I), containing a weight percentage of polyether blocks ranging from 3.5 to 98.7%, preferably from 5 to 95%, preferably from 10 to 90%, preferably from 10 to 85%, preferably from 10 to 80%, preferably from 10 to 75%, preferably from 10 to 70%, preferably from 10 to 65%, preferably from 10 to 60%, preferably from 10 to 55%, preferably from 10 to 50%, preferably from 10 to 45%, preferably from 10 to 40%, preferably from 10 to 35%, and preferably from 10 to 30%.
(FR) L'invention porte sur un polymère hydrocarboné à blocs polyéther et polyoléfine, liquide ou solide à température ambiante, comprenant au moins un groupement terminal alcoxysilane, le polymère silylé de formule (I), contenant un pourcentage massique en blocs polyéther allant de 3,5 à 98,7 %, de préférence 5 à 95 %, de préférence 10 à 90 %, de préférence 10 à 85 %, de préférence 10 à 80 %, de préférence 10 à 75 %, de préférence 10 à 70 %, de préférence 10 à 65 %, de préférence 10 à 60 %, de préférence 10 à 55 %, de préférence 10 à 50 %, de préférence de 10 à 45 %, de préférence de 10 à 40 %, de préférence de 10 à 35 %, et de préférence de 10 à 30%.