1. (WO2003085140) PROCEDE ET INSTALLATION POUR PRODUIRE DE L'ACIER INOXYDABLE, NOTAMMENT DE L'ACIER FIN RENFERMANT DU CHROME OU DU NICKEL-CHROME
Dernières données bibliographiques dont dispose le Bureau international   

N° de publication :    WO/2003/085140    N° de la demande internationale :    PCT/EP2003/002133
Date de publication : 16.10.2003 Date de dépôt international : 01.03.2003
Demande présentée en vertu du Chapitre 2 :    29.10.2003    
CIB :
C21C 1/02 (2006.01), C21C 5/00 (2006.01), C21C 5/52 (2006.01), C21C 7/064 (2006.01), F27B 3/06 (2006.01), F27B 3/08 (2006.01), F27B 19/04 (2006.01), F27D 3/15 (2006.01), F27D 3/16 (2006.01)
Déposants : SMS DEMAG AKTIENGSELLSCHAFT [DE/DE]; Eduard-Schloemann-Strasse 4, 40237 Düsseldorf (DE) (Tous Sauf US).
PLESCHIUTSCHNIGG, Fritz-Peter [DE/DE]; (DE) (US Seulement).
MEIERLING, Peter [DE/DE]; (DE) (US Seulement).
SCHNEIDER, Karl-Josef [DE/DE]; (DE) (US Seulement).
PETRY, Jochen [DE/DE]; (DE) (US Seulement)
Inventeurs : PLESCHIUTSCHNIGG, Fritz-Peter; (DE).
MEIERLING, Peter; (DE).
SCHNEIDER, Karl-Josef; (DE).
PETRY, Jochen; (DE)
Mandataire : VALENTIN, Ekkehard; Valentin, Gihske, Grosse, Hammerstrasse 2, 57072 Siegen (DE)
Données relatives à la priorité :
102 15 828.2 10.04.2002 DE
Titre (DE) VERFAHREN UND EINRICHTUNG ZUM ERZEUGEN VON NICHTROSTENDEM STAHL, INSBESONDERE VON CHROM- ODER CHROMNICKELHALTIGEM EDELSTAHL
(EN) METHOD AND INSTALLATION FOR PRODUCING STAINLESS STEEL, ESPECIALLY HIGH-QUALITY STEEL CONTAINING CHROMIUM OR NICKEL CHROMIUM
(FR) PROCEDE ET INSTALLATION POUR PRODUIRE DE L'ACIER INOXYDABLE, NOTAMMENT DE L'ACIER FIN RENFERMANT DU CHROME OU DU NICKEL-CHROME
Abrégé : front page image
(DE)Ein Verfahren und eine Einrichtung zum Erzeugen von nichtrostendem Stahl, insbesondere von chrom- oder chromnickelhaltigem Edelstahl, unmittelbar aus phosphorreichem, flüssigen Roheisen, ermöglicht die auf einer Stranggiessanlage notwendigen Zeitabstände für das Beschicken mit Schmelze und erspart ein Verfahren aufgrund eines Mehr-Gefäss-Systems dadurch, dass in einem einzigen Gefäss (1; 2) eine Vorbehandlung zum Entphosphoren über einen Sauerstoffaufblas-Schritt bei gleichzeitigem Eisenverschlacken, Entkohlen und Entsilizieren unter Zugabe von Schlackenbildnern und / oder festen Kühlstoffen durchgeführt wird, dass die phosphorreiche Schlacke (19) abgeführt wird und dass danach Chrom und / oder Schrott sowie andere Legierungselemente chargiert werden.
(EN)The invention relates to a method and an installation for producing stainless steel, especially high-quality steel containing chromium or nickel, directly from high-phosphorus, liquid pig iron. The aim of the invention is to provide a method and an installation which enable the necessary time intervals in a continuous casting installation to be created for the loading of the melt, and render superfluous a method based on a multiple vessel system. To this end, the inventive method involves carrying out a pre-treatment for dephosphorisation in a single vessel (1; 2) by means of an oxygen blowing step, at the same time as iron slagging, decarburisation and desilication with addition of slag forming agents and/or solid coolants, and the high-phosphorus slag (19) is carried off and chromium and/or scrap iron and other alloy elements are loaded.
(FR)L'invention concerne un procédé et une installation pour produire de l'acier inoxydable, notamment de l'acier fin renfermant du chrome ou du nickel-chrome, directement à partir de fonte brute liquide, riche en phosphore. L'objectif de l'invention est de créer un procédé et une installation permettant de disposer des intervalles de temps nécessaires dans une installation de coulée continue pour le chargement de la fonte et d'économiser un procédé faisant appel à un système multi-cuves. A cet effet, le procédé selon l'invention consiste à effectuer, dans une seule cuve (1 ; 2), un traitement préalable de déphosphoration par l'intermédiaire d'une étape d'affinage à l'oxygène, effectuée simultanément à l'élimination des scories de fer, à la décarburation et à l'élimination du silicium par addition de fondants de scorification et/ou de matières de refroidissement solides. Il consiste en outre à évacuer les scories riches en phosphore (19) et à charger ensuite le chrome et/ou les mitrailles ainsi que d'autres éléments d'alliage.
États désignés : AE, AG, AL, AM, AT, AU, AZ, BA, BB, BG, BR, BY, BZ, CA, CH, CN, CO, CR, CU, CZ, DE, DK, DM, DZ, EC, EE, ES, FI, GB, GD, GE, GH, GM, HR, HU, ID, IL, IN, IS, JP, KE, KG, KP, KR, KZ, LC, LK, LR, LS, LT, LU, LV, MA, MD, MG, MK, MN, MW, MX, MZ, NO, NZ, OM, PH, PL, PT, RO, RU, SC, SD, SE, SG, SK, SL, TJ, TM, TN, TR, TT, TZ, UA, UG, US, UZ, VC, VN, YU, ZA, ZM, ZW.
Organisation régionale africaine de la propriété intellectuelle (ARIPO) (GH, GM, KE, LS, MW, MZ, SD, SL, SZ, TZ, UG, ZM, ZW)
Office eurasien des brevets (OEAB) (AM, AZ, BY, KG, KZ, MD, RU, TJ, TM)
Office européen des brevets (OEB) (AT, BE, BG, CH, CY, CZ, DE, DK, EE, ES, FI, FR, GB, GR, HU, IE, IT, LU, MC, NL, PT, RO, SE, SI, SK, TR)