1. WO1988002410 - PROCEDE POUR L'OBTENTION D'UN ALLIAGE D'ALUMINO-SILICIUM CONTENANT 2-22 % EN POIDS DE SILICIUM

Numéro de publication WO/1988/002410
Date de publication 07.04.1988
N° de la demande internationale PCT/SU1986/000095
Date du dépôt international 29.09.1986
CIB
C22C 1/02 2006.01
CCHIMIE; MÉTALLURGIE
22MÉTALLURGIE; ALLIAGES FERREUX OU NON FERREUX; TRAITEMENT DES ALLIAGES OU DES MÉTAUX NON FERREUX
CALLIAGES
1Fabrication des alliages non ferreux
02par fusion
CPC
C22C 1/026
CCHEMISTRY; METALLURGY
22METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
CALLOYS
1Making alloys
02by melting
026Alloys based on aluminium
Déposants
  • VSESOJUZNY NAUCHNO-ISSLEDOVATELSKY I PROEKTNY INST [SU]/[SU]
  • SPETSIALNOE KONSTRUKTORSKOE BJURO MAGNITNOI GIDROD [SU]/[SU]
Inventeurs
  • IVCHENKOV, Vadim Petrovich
  • KALUZHSKY, Nikolai Andreevich
  • ISIDOROV, Eduard Alexeevich
  • SIROTENKO, Viktor Georgievich
  • SHUSTEROV, Viktor Semenovich
  • PAKHOMOV, Gennady Alexandrovich
  • TEPLYAKOV, Fedor Konstantinovich
  • KHROMOVSKIKH, Oleg Sergeevich
Mandataires
  • THE USSR CHAMBER OF COMMERCE AND INDUSTRY
Données relatives à la priorité
Langue de publication russe (RU)
Langue de dépôt russe (RU)
États désignés
Titre
(EN) METHOD OF OBTAINING ALUMINOSILICON ALLOY CONTAINING 2-22 PER CENT BY WEIGHT OF SILICON
(FR) PROCEDE POUR L'OBTENTION D'UN ALLIAGE D'ALUMINO-SILICIUM CONTENANT 2-22 % EN POIDS DE SILICIUM
Abrégé
(EN)
The method consists in charging in the form of a cone, crystalline silicon on the hearth of a reverberatory furnace, pouring the liquid aluminium into the bath of the furnace at a temperature of 780-820°C while continually mixing the aluminosilicon melt by means of a jet formed of the same melt, which is directed to the base of the cone of the charged silicon at a speed of the jet, along its axis, of 0.5-0.8 m/sec; simultaneously with the start of the mixing the temperature of the melt in the bath of the furnace is cooled down to 670-750°C and mixing is continued at this temperature. The alloy may be used in the automobile and tractor industry, as well as for production of consumer goods.
(FR)
Le procédé consiste à charger du silicium cristallin, sous forme d'un cône, sur le foyer d'un four à réverbères, à verser l'aluminium liquide dans le bain du four à une température de 780-800°C en brassant la coulée d'alumino-silicium au moyen d'un jet formé par ladite coulée, le jet étant dirigé vers la base du cône de silicium chargé à une vitesse axiale du jet de 0,5 à 0,8 m/sec; en même temps que le démarrage du brassage, la température de la coulée du bain du four est abaissée à 670-750°C et on continue le brassage à cette température. L'alliage peut être utilisé dans l'industrie des automobiles et des tracteurs, ainsi que pour la production de biens de consommation.
Également publié en tant que
NO19882212