1. WO2019034259 - METHOD FOR PROCESSING A MATERIAL LAYER USING ENERGETIC RADIATION HAVING VARIABLE ENERGY DISTRIBUTION

公布号 WO/2019/034259
公布日 21.02.2019
国际申请号 PCT/EP2017/070916
国际申请日 18.08.2017
国际专利分类
B 作业;运输
23
机床;其他类目中不包括的金属加工
K
钎焊或脱焊;焊接;用钎焊或焊接方法包覆或镀敷;局部加热切割,如火焰切割;用激光束加工
26
用激光束加工,例如焊接,切割,打孔
02
在激光焊接或切割中的工件
06
激光束的成形,例如,利用掩膜或多次聚焦
[IPC code unknown for B23K 26/342]
B23K 26/06 (2014.01)
B23K 26/342 (2014.01)
CPC
B22F 2003/1057
B22F 2203/00
B22F 2999/00
B22F 3/1055
B22F 5/10
B23K 15/004
申请人
  • FRAUNHOFER-GESELLSCHAFT ZUR FÖRDERUNG DER ANGEWANDTEN FORSCHUNG E. V.; Hansastr. 27c 80686 München, DE
发明人
  • EIBL, Florian; DE
  • MEINERS, Wilhelm; DE
代理人
  • GAGEL, Roland; DE
优先权数据
公布语言 德语 (DE)
申请语言 德语 (DE)
指定国
标题
(DE) VEFAHREN ZUR BEARBEITUNG EINER WERKSTOFFSCHICHT MIT ENERGETISCHER STRAHLUNG VARIABLER ENERGIEVERTEILUNG
(EN) METHOD FOR PROCESSING A MATERIAL LAYER USING ENERGETIC RADIATION HAVING VARIABLE ENERGY DISTRIBUTION
(FR) PROCÉDÉ D'USINAGE D'UNE COUCHE DE MATÉRIAU AVEC UN RAYONNEMENT ÉNERGÉTIQUE À DISTRIBUTION D'ÉNERGIE VARIABLE
摘要
(DE)
Bei einem Verfahren zur Bearbeitung einer Werkstoffschicht mit energetischer Strahlung werden mehrere voneinander getrennte energetische Strahlen 2 zumindest zeitweise auf die Werkstoffschicht gerichtet und in einer Bewegungsrichtung über die Werkstoffschicht geführt, wobei die Werkstoffschicht innerhalb eines zu bearbeitenden Bereiches unter Erzeugung wenigstens eines zusammenhängenden Schmelzbades lokal aufgeschmolzen wird. Durch eine Variation der Strahlungsleistung und/oder des Spotabstands und/oder der Spotgröße von jeweils in den zu bearbeitenden Bereich gerichteten energetischen Strahlen 2 und/oder durch Einstellung eines gegenseitigen Versatzes von jeweils in den zu bearbeitenden Bereich gerichteten energetischen Strahlen in Bewegungsrichtung werden eine oder mehrere Eigenschaften des Schmelzbades und/oder einer durch Erstarren des Schmelzbades erzeugten Schmelzspur gezielt beeinflusst. Dadurch lässt sich bei generativen Fertigungsverfahren die Herstellungsdauer der Bauteile ohne Verringerung der Oberflächenqualität erhöhen und auch eine bessere Anpassung an die Bauteilgeometrie erreichen.
(EN)
The invention relates to a method for processing a material layer using energetic radiation, in which method a plurality of separate energetic beams 2 are directed, at least intermittently, onto the material layer and are guided in a movement direction over the material layer, the material layer being locally melted within a region to be processed while producing at least one continuous melt pool. By varying the radiated power and/or the spot spacing and/or the spot size of energetic beams 2 directed in each case into the region to be processed and/or by adjusting a mutual offset of energetic beams directed in each case into the region to be processed, one or more properties of the melt pool and/or of a melt track produced by solidification of the melt pool are influenced in a targeted manner. As a result, in generative manufacturing methods, the length of the production process of the components can be increased without reducing the surface quality, and improved adaptation to the component geometry can also be achieved.
(FR)
L'invention concerne un procédé d'usinage d'une couche de matériau avec un rayonnement énergétique, lors duquel plusieurs rayons énergétiques (2) séparés les uns des autres sont dirigés au moins temporairement sur la couche de matériau et guidés dans un sens de déplacement au-dessus de la couche de matériau. La couche de matériau est fondue localement à l'intérieur d'une zone à usiner en produisant au moins un bain de fusion cohérent. Une ou plusieurs propriétés du bain de fusion et/ou d'une trace de fusion produite par solidification du bain de fusion sont influencées de manière ciblée par une variation de la puissance du rayonnement et/ou de la distance de point et/ou de la taille du point de rayons énergétiques (2) respectivement dirigés dans la zone à usiner et/ou par réglage d'un décalage réciproque dans le sens de déplacement entre les rayons énergétiques respectivement dirigés dans la zone à usiner. La durée de fabrication des éléments structuraux lors d'un procédé de fabrication additive peut ainsi être augmentée sans diminution de la qualité de la surface et une meilleure adaptation à la géométrie des éléments structuraux peut en outre être obtenue.