1. (WO2018227740) LOW YIELD STRENGTH RATIO, HIGH STRENGTH AND DUCTILITY THICK GAUGE STEEL PLATE AND MANUFACTURING METHOD THEREFOR
Dados bibliográficos mais recentes no arquivo da Secretaria Internacional    Submeter observação

№ de pub.: WO/2018/227740 № do pedido internacional: PCT/CN2017/096430
Data de publicação: 20.12.2018 Data de depósito internacional: 08.08.2017
CIP:
C22C 38/58 (2006.01) ,C22C 38/02 (2006.01) ,C22C 38/06 (2006.01) ,C22C 38/44 (2006.01) ,C22C 38/50 (2006.01) ,C21D 8/02 (2006.01)
C QUÍMICA; METALURGIA
22
METALURGIA; LIGAS FERROSAS OU NÃO-FERROSAS; TRATAMENTO DE LIGAS OU DE METAIS NÃO-FERROSOS
C
LIGAS
38
Ligas ferrosas, p. ex., ligas de aço
18
contendo cromo
40
com níquel
58
com mais de 1,5% em peso de manganês
C QUÍMICA; METALURGIA
22
METALURGIA; LIGAS FERROSAS OU NÃO-FERROSAS; TRATAMENTO DE LIGAS OU DE METAIS NÃO-FERROSOS
C
LIGAS
38
Ligas ferrosas, p. ex., ligas de aço
02
contendo silício
C QUÍMICA; METALURGIA
22
METALURGIA; LIGAS FERROSAS OU NÃO-FERROSAS; TRATAMENTO DE LIGAS OU DE METAIS NÃO-FERROSOS
C
LIGAS
38
Ligas ferrosas, p. ex., ligas de aço
06
contendo alumínio
C QUÍMICA; METALURGIA
22
METALURGIA; LIGAS FERROSAS OU NÃO-FERROSAS; TRATAMENTO DE LIGAS OU DE METAIS NÃO-FERROSOS
C
LIGAS
38
Ligas ferrosas, p. ex., ligas de aço
18
contendo cromo
40
com níquel
44
com molibdênio ou tungstênio
C QUÍMICA; METALURGIA
22
METALURGIA; LIGAS FERROSAS OU NÃO-FERROSAS; TRATAMENTO DE LIGAS OU DE METAIS NÃO-FERROSOS
C
LIGAS
38
Ligas ferrosas, p. ex., ligas de aço
18
contendo cromo
40
com níquel
50
com titânio ou zircônio
C QUÍMICA; METALURGIA
21
METALURGIA DO FERRO
D
MODIFICAÇÃO DA ESTRUTURA FÍSICA DE METAIS FERROSOS; DISPOSITIVOS GERAIS PARA O TRATAMENTO TÉRMICO DE METAIS OU LIGAS FERROSAS OU NÃO FERROSAS; MALEABILIZAÇÃO DE METAIS POR DESCARBURIZAÇÃO, REVENIMENTO, OU OUTROS TRATAMENTOS
8
Modificação das propriedades físicas por deformação combinada com, ou seguida de, tratamento térmico
02
durante a manufatura de chapa grossa ou tiras
Requerentes:
南京钢铁股份有限公司 NANJING IRON & STEEL CO., LTD. [CN/CN]; 中国江苏省南京市 六合区卸甲甸 Xie Jia Dian Liuhe District Nanjing, Jiangsu 210035, CN
Inventores:
孙超 SUN, Chao; CN
李强 LI, Qiang; CN
单以刚 SHAN, Yigang; CN
王从道 WANG, Chongdao; CN
党军 DANG, Jun; CN
Mandatário:
南京利丰知识产权代理事务所(特殊普通合伙) NANJING IRON & STEEL CO., LTD.; 中国江苏省南京市 秦淮区中华路50号江苏国际经贸大厦1801室 Room 1801, Jiangsu International Economic and Trade Building, No.50, Zhonghua Road, Qinhuai District Nanjing, Jiangsu 210001, CN
Dados da prioridade:
201710445091.313.06.2017CN
Título (EN) LOW YIELD STRENGTH RATIO, HIGH STRENGTH AND DUCTILITY THICK GAUGE STEEL PLATE AND MANUFACTURING METHOD THEREFOR
(FR) PLAQUE D'ACIER DE FORTE ÉPAISSEUR À BAS RAPPORT DE LIMITE D'ÉLASTICITÉ ET RÉSISTANCE ET DUCTILITÉ ÉLEVÉES, ET SON PROCÉDÉ DE FABRICATION
(ZH) 一种低屈强比高强韧厚规格钢板及其制造方法
Resumo:
(EN) A low yield strength ratio, high strength and ductility thick gauge steel plate, the content of the chemical components thereof in terms of percentage by mass being: C: 0.060-0.080%, Mn: 5.5-6.0%, Si: 0.10-0.30%, Al: 0.015-0.040%, Mo: 0.15-0.30%, Cr: 0.20-0.40%, Ni: 0.15-0.40%, Ti: 0.01-0.03%, S ≤ 0.006%, P ≤ 0.010%, the remainder being Fe and unavoidable impurity elements. The steel plate is provided with increased yield strength, reduced yield strength ratio, and great low-temperature impact toughness. A manufacturing method for the steel plate comprises: heating, rolling, and heat treatment. The method requires only one heat treatment and has a simple process.
(FR) Cette invention concerne une plaque d'acier de forte épaisseur à bas rapport de limite d'élasticité et résistance et ductilité élevées, la teneur en constituants chimiques de ladite plaque étant, en termes de pourcentage en masse, C : 0,060 à 0,080 %, Mn : 5,5 à 6,0 %, Si : 0,10 à 0,30 %, Al : 0,015-0,040 %, Mo : 0,15 à 0,30 %, Cr : 0,20 à 0,40 %, Ni : 0,15 à 0,40 %, Ti : 0,01 à 0,03 %, S ≤ 0,006 %, P ≤ 0,010 %, le reste étant du Fe et des éléments d'impuretés inévitables. La plaque d'acier est dotée d'une limite d'élasticité accrue, d'un rapport de limite d'élasticité réduit et d'une grande ténacité à l'impact à basse température. Un procédé de fabrication de la plaque d'acier comprend un chauffage, un laminage et un traitement thermique. Le procédé ne nécessite qu'un seul traitement thermique, et sa mise en œuvre est simple.
(ZH) 一种低屈强比高强韧厚规格钢板,其化学组分的质量百分比含量为:C:0.060-0.080%、Mn:5.5-6.0%、Si:0.10-0.30%、Al:0.015-0.040%、Mo:0.15-0.30%、Cr:0.20-0.40%、Ni:0.15-0.40%、Ti:0.01-0.03%、S≤0.006%、P≤0.010%,余量为Fe和不可避免的杂质元素;该钢板具有较高的屈服强度、较低的屈强比和良好的低温冲击韧性。钢板的制造方法包括:加热、轧制和热处理;该方法仅需要一次热处理,工艺简单。
front page image
Estados designados: AE, AG, AL, AM, AO, AT, AU, AZ, BA, BB, BG, BH, BN, BR, BW, BY, BZ, CA, CH, CL, CN, CO, CR, CU, CZ, DE, DJ, DK, DM, DO, DZ, EC, EE, EG, ES, FI, GB, GD, GE, GH, GM, GT, HN, HR, HU, ID, IL, IN, IR, IS, JO, JP, KE, KG, KH, KN, KP, KR, KW, KZ, LA, LC, LK, LR, LS, LU, LY, MA, MD, ME, MG, MK, MN, MW, MX, MY, MZ, NA, NG, NI, NO, NZ, OM, PA, PE, PG, PH, PL, PT, QA, RO, RS, RU, RW, SA, SC, SD, SE, SG, SK, SL, SM, ST, SV, SY, TH, TJ, TM, TN, TR, TT, TZ, UA, UG, US, UZ, VC, VN, ZA, ZM, ZW
Organização Regional Africana da Propriedade Intelectual (ARIPO) (BW, GH, GM, KE, LR, LS, MW, MZ, NA, RW, SD, SL, ST, SZ, TZ, UG, ZM, ZW)
Instituto Eurasiático de Patentes (AM, AZ, BY, KG, KZ, RU, TJ, TM)
Instituto Europeu de Patentes (AL, AT, BE, BG, CH, CY, CZ, DE, DK, EE, ES, FI, FR, GB, GR, HR, HU, IE, IS, IT, LT, LU, LV, MC, MK, MT, NL, NO, PL, PT, RO, RS, SE, SI, SK, SM, TR)
Organização Africana da Propriedade Intelectual (OAPI) (BF, BJ, CF, CG, CI, CM, GA, GN, GQ, GW, KM, ML, MR, NE, SN, TD, TG)
Língua de publicação: chinês (ZH)
Língua de depósito: chinês (ZH)