1. (WO2009109333) PROCÉDÉ DE TRAITEMENT D'UNE MOUSSE DE POLYURÉTHANNE À L'AIDE D'UN RAYONNEMENT MICRO-ONDES
Dernières données bibliographiques dont dispose le Bureau international   

N° de publication :    WO/2009/109333    N° de la demande internationale :    PCT/EP2009/001404
Date de publication : 11.09.2009 Date de dépôt international : 27.02.2009
CIB :
C08J 3/28 (2006.01), C08J 3/24 (2006.01), B29C 35/08 (2006.01)
Déposants : BAYER MATERIALSCIENCE AG [DE/DE]; 51368 Leverkusen (DE) (Tous Sauf US).
HANNIG, Frithjof [DE/DE]; (DE) (US Seulement).
ULBRICH, Dagmar [DE/DE]; (DE) (US Seulement).
NORDMANN, Peter [DE/DE]; (DE) (US Seulement).
JAEGER, Martina [DE/DE]; (DE) (US Seulement).
BEAUJEAN, Joern [DE/DE]; (DE) (US Seulement).
FRIEDERICHS, Wolfgang [DE/DE]; (DE) (US Seulement)
Inventeurs : HANNIG, Frithjof; (DE).
ULBRICH, Dagmar; (DE).
NORDMANN, Peter; (DE).
JAEGER, Martina; (DE).
BEAUJEAN, Joern; (DE).
FRIEDERICHS, Wolfgang; (DE)
Mandataire : LIPTAU, Patrick; Michalski Hüttermann & Partner Neuer Zollhof 2 40221 Düsseldorf (DE)
Données relatives à la priorité :
10 2008 013 181.4 07.03.2008 DE
Titre (DE) VERFAHREN ZUR BEHANDLUNG VON POLYURETHANSCHAUM MITTELS MIKROWELLENSTRAHLUNG
(EN) METHOD FOR TREATING POLYURETHANE FOAM USING MICROWAVE RADIATION
(FR) PROCÉDÉ DE TRAITEMENT D'UNE MOUSSE DE POLYURÉTHANNE À L'AIDE D'UN RAYONNEMENT MICRO-ONDES
Abrégé : front page image
(DE)Die vorliegende Erfindung betrifft ein Verfahren zur Behandlung von Polyurethanschaum, wobei der Polyurethanschaum erhältlich ist aus einem Reaktionsgemisch umfassend eine Ethylenoxid/Propylenoxid-Polyolkomponente mit einer OH-Zahl von ≥ 20 mg KOH/g bis ≤ 45 mg KOH/g und eine Isocyanatkomponente mit einem NCO-Gehalt von ≥ 20 Gewichts-% bis ≤ 49 Gewichts-%, welche ausgewählt ist aus der Gruppe umfassend Diphenylmethandiisocyanat, Toluylendiisocyanat, deren Prepolymere mit einem Ethylenoxid/Propylenoxid-Polyol, dessen OH- Zahl von ≥ 20 mg KOH/g bis ≤ 45 mg KOH/g beträgt und/oder deren Allophanate, Harnstoffe, Biurete, Uretdione, Isocyanurate oder Carbodiimide. Sie betrifft weiterhin ein nach diesem Verfahren behandelten Polyurethanschaum. Der Polyurethanschaum wird nach Beenden der Schaumbildung mit Mikrowellenstrahlung bestrahlt, wobei die auf das Volumen des von der Mikrowellenstrahlung erreichbaren Bereichs bezogene eingestrahlte Energie ≥ 1,0 Kilojoule/Liter bis ≤ 2,23 Kilojoule/Liter beträgt. Sie betrifft weiterhin ein nach diesem Verfahren behandelten Polyurethanschaum. Solche Polyurethanschäume eignen sich beispielsweise als Möbelformschäume.
(EN)The present invention relates to a method for treating polyurethane foam, wherein said polyurethane foam can be obtained from a reaction mixture which comprises an ethylene oxide/propylene oxide polyol component having a hydroxyl number of ≥ 20 mg KOH/g to ≤ 45 mg KOH/g and an isocyanate component having an NCO content of ≥ 20 wt.-% to ≤ 49 wt.-%, which is selected from the group comprising diphenylmethane diisocyanate, toluylene diisocyanate, the pre-polymers thereof with an ethylene oxide/propylene oxide polyol, the hydroxyl number thereof being from ≥ 20 mg KOH/g to ≤ 45 mg KOH/g and/or the allophanates, ureas, biurets, uretediones, isocyanurates, or carbodiimides thereof. Furthermore, the invention relates to a polyurethane foam treated according to said method. The polyurethane foam is irradiated with microwave radiation after ending the foaming, wherein the energy irradiated on the volume of the area which can be reached by the microwave radiation is ≥ 1.0 kilojoules/liter to ≤ 2.23 kilojoules/liter. Furthermore, the invention relates to a polyurethane foam treated according to said method. Such polyurethane foams are suitable, for example, as furniture molding foams.
(FR)La présente invention concerne un procédé pour le traitement d'une mousse de polyuréthanne, la mousse de polyuréthanne pouvant être obtenue à partir d'un mélange réactionnel comprenant un composant oxyde d'éthylène/oxyde de propylène-polyol ayant un indice d'hydroxyle ≥ 20 mg KOH/g et allant jusqu'à ≤ 45 mg KOH/g et un composant isocyanate ayant une teneur en groupes NCO ≥ 20 % en poids et allant jusqu'à ≤ 49 % en poids, qui est choisi dans le groupe comprenant le diisocyanate de diphénylméthane, le diisocyanate de toluylène, leurs prépolymères avec un oxyde d'éthylène/oxyde de propylène-polyol dont l'indice d'hydroxyle est ≥ 20 mg KOH/g jusqu'à ≤ 45 mg KOH/g, et/ou leurs allophanates, urées, biurets, uretdiones, isocyanurates ou carbodiimides. Elle concerne en outre une mousse de polyuréthanne traitée par ce procédé. La mousse de polyuréthane, après la fin de la formation de la mousse, est exposée à un rayonnement micro-ondes, l'énergie de rayonnement, rapportée au volume de la zone pouvant être atteinte par le rayonnement micro-ondes, étant ≥ 1,0 kilojoules/litre jusqu'à ≤ 2,23 kilojoules/litre. Elle concerne en outre une mousse de polyuréthane traitée par ce procédé. Ces mousses de polyuréthane conviennent par exemple en tant que mousses moulées pour ameublement.
États désignés : AE, AG, AL, AM, AO, AT, AU, AZ, BA, BB, BG, BH, BR, BW, BY, BZ, CA, CH, CN, CO, CR, CU, CZ, DE, DK, DM, DO, DZ, EC, EE, EG, ES, FI, GB, GD, GE, GH, GM, GT, HN, HR, HU, ID, IL, IN, IS, JP, KE, KG, KM, KN, KP, KR, KZ, LA, LC, LK, LR, LS, LT, LU, LY, MA, MD, ME, MG, MK, MN, MW, MX, MY, MZ, NA, NG, NI, NO, NZ, OM, PG, PH, PL, PT, RO, RS, RU, SC, SD, SE, SG, SK, SL, SM, ST, SV, SY, TJ, TM, TN, TR, TT, TZ, UA, UG, US, UZ, VC, VN, ZA, ZM, ZW.
Organisation régionale africaine de la propriété intellectuelle (ARIPO) (BW, GH, GM, KE, LS, MW, MZ, NA, SD, SL, SZ, TZ, UG, ZM, ZW)
Office eurasien des brevets (OEAB) (AM, AZ, BY, KG, KZ, MD, RU, TJ, TM)
Office européen des brevets (OEB) (AT, BE, BG, CH, CY, CZ, DE, DK, EE, ES, FI, FR, GB, GR, HR, HU, IE, IS, IT, LT, LU, LV, MC, MK, MT, NL, NO, PL, PT, RO, SE, SI, SK, TR)
Organisation africaine de la propriété intellectuelle (OAPI) (BF, BJ, CF, CG, CI, CM, GA, GN, GQ, GW, ML, MR, NE, SN, TD, TG).
Langue de publication : allemand (DE)
Langue de dépôt : allemand (DE)