Traduction automatique
1. (WO2002079526) TUBE EN ACIER A HAUTE RESISTANCE POUR COUSSIN D'AIR ET PROCEDE POUR LA PRODUCTION DE CE TUBE
Dernières données bibliographiques dont dispose le Bureau international   

N° de publication :    WO/2002/079526    N° de la demande internationale :    PCT/JP2002/003164
Date de publication : 10.10.2002 Date de dépôt international : 29.03.2002
CIB :
C21D 8/10 (2006.01), C22C 38/20 (2006.01), C22C 38/22 (2006.01), C22C 38/26 (2006.01), C22C 38/28 (2006.01), C22C 38/40 (2006.01), C22C 38/42 (2006.01), C22C 38/48 (2006.01), C22C 38/50 (2006.01), C22C 38/58 (2006.01), B60R 21/268 (2011.01), C21D 1/18 (2006.01), C21D 9/08 (2006.01)
Déposants : SUMITOMO METAL INDUSTRIES, LTD. [JP/JP]; 5-33, Kitahama 4-chome Chuo-ku Osaka-shi, Osaka 541-0041 (JP) (Tous Sauf US).
KONDO, Kunio [JP/JP]; (JP) (US Seulement).
YAMAMOTO, Miyuki [JP/JP]; (JP) (US Seulement).
TAKANO, Takashi [JP/JP]; (JP) (US Seulement).
BEPPU, Kenichi [JP/JP]; (JP) (US Seulement).
HIRANO, Susumu [JP/JP]; (JP) (US Seulement).
HITOSHIO, Keisuke [JP/JP]; (JP) (US Seulement).
KURATA, Hidetoshi [JP/JP]; (JP) (US Seulement)
Inventeurs : KONDO, Kunio; (JP).
YAMAMOTO, Miyuki; (JP).
TAKANO, Takashi; (JP).
BEPPU, Kenichi; (JP).
HIRANO, Susumu; (JP).
HITOSHIO, Keisuke; (JP).
KURATA, Hidetoshi; (JP)
Mandataire : HIROSE, Shoichi; Tozan Building 4-2, Nihonbashi Honcho 4-chome Chuo-ku, Tokyo 103-0023 (JP)
Données relatives à la priorité :
2001-95484 29.03.2001 JP
2001-371409 05.12.2001 JP
Titre (EN) HIGH STRENGTH STEEL TUBE FOR AIR BAG AND METHOD FOR PRODUCTION THEREOF
(FR) TUBE EN ACIER A HAUTE RESISTANCE POUR COUSSIN D'AIR ET PROCEDE POUR LA PRODUCTION DE CE TUBE
Abrégé : front page image
(EN)A method for producing a high strength steel tube, which comprises manufacturing a tube by the use of a steel having a chemical composition in mass %: C: 0.05 to 0.20 %; Si: 0.1 to 1.0; Mn: 0.20 to 2.0 %; P: 0.025 % or less; S: 0.010 % or less, Cr: 0.05 to 1.0 %, Al: 0.10 % or less; optionally, at least one of Mo: 0.050 % or less, Ni: 1.5 % or less, Cu: 0.5 % or less, V: 0.2 % or less, Ti: 0.1 % or less, Nb: 0.1 % or less, and B: 0.005 % or less; and also optionally, at least one of Ca: 0.01 % or less, Mg: 0.01 % or less, REM (rare earth element): 0.01 % or less; balance Fe and impurities; and then subjecting the tube to a cold working to form it so as to have predetermined dimensions, and thereafter, heating it to a temperature of the A¿C1? transformation temperature thereof or higher, followed by quenching, and then, tempering it at a temperature of the A¿C1? transformation temperature or lower. The steel tube is capable of corresponding to the increase in the pressure of a gas blowing out into an air bag and the reduction in the wall-thickness of an accumulator.
(FR)L'invention concerne un procédé pour la production d'un tube en acier à haute résistance. Le procédé selon l'invention comprend la fabrication d'un tube en utilisant un acier de composition chimique suivante en pourcentage en masse : C pour 0,05 à 0,20 %, Si pour 0,1 à 1,0 %, Mn pour 0,20 à 2,0 %, P pour 0,025 % ou moins, S pour 0,010 % ou moins, Cr pour 0,05 à 1,0 %, Al pour 0,10 % ou moins, facultativement, au moins un parmi Mo pour 0,050 % ou moins, Ni pour 1,5 % ou moins, Cu pour 0,5 % ou moins, V pour 0,2 % ou moins, Ti pour 0,1 % ou moins, Nb pour 0,1 % ou moins et B pour 0,005 % ou moins, ainsi que facultativement au moins un parmi Ca pour 0,01 % ou moins, Mg pour 0,01 % ou moins, élément du groupe des terres rares pour 0,01 % ou moins, le reste étant constitué de fer et d'impuretés. Le tube est ensuite soumis à un façonnage à froid afin de lui donner des dimensions prédéfinies, puis il est chauffé à la température du point de transformation A¿C1? ou plus, trempé, puis revenu à la température du point de transformation A¿C1? ou moins. Le tube d'acier selon l'invention peut supporter l'augmentation de pression d'un gaz jaillissant dans un coussin d'air et la diminution dans l'épaisseur de paroi d'un accumulateur.
États désignés : US.
Office européen des brevets (OEB) (AT, BE, CH, CY, DE, DK, ES, FI, FR, GB, GR, IE, IT, LU, MC, NL, PT, SE, TR).
Langue de publication : japonais (JA)
Langue de dépôt : japonais (JA)