1. (WO2000055092) PROCEDE DE PRODUCTION D'ADSORBANTS MOULES HAUTEMENT PERFORMANTS
Dernières données bibliographiques dont dispose le Bureau international   

N° de publication :    WO/2000/055092    N° de la demande internationale :    PCT/DE2000/000823
Date de publication : 21.09.2000 Date de dépôt international : 15.03.2000
Demande présentée en vertu du Chapitre 2 :    16.10.2000    
CIB :
B01J 20/20 (2006.01), C01B 31/08 (2006.01), C01B 31/10 (2006.01)
Déposants : CARBOTEX PRODUKTIONS- UND VEREDELUNGSBETRIEBE GMBH [DE/DE]; Salegaster Chausee 1, D-06803 Bitterfeld-Greppin (DE)
Inventeurs : SPEIKER, Hubertus; (DE).
GIEBELHAUSEN, Jann-Michael; (DE)
Mandataire : GAGEL, Roland; Landsberger Strasse 480a, D-81241 München (DE)
Données relatives à la priorité :
199 12 153.2 18.03.1999 DE
Titre (DE) VERFAHREN ZUR HERSTELLUNG VON GEFORMTEN HOCHLEISTUNGSADSORBENZIEN
(EN) METHOD FOR PRODUCING SHAPED HIGH-PERFORMANCE ADSORBING MATERIALS
(FR) PROCEDE DE PRODUCTION D'ADSORBANTS MOULES HAUTEMENT PERFORMANTS
Abrégé : front page image
(DE)Die Erfindung betrifft die Herstellung von geformten Hochleistungsadsorbenzien durch Wasserdampfaktivierung in einem diskontinuierlich arbeitenden Drehrohrofen, in dem sphärisch vorgeformte Materialien in einem Drehrohrtrockner bei 4 - maliger Produktumwälzung je Ofenumdrehung und bei einem Raum/ZeitKoeffizienten von 1 bis 2,5 m?3¿/h mit Heißgas schonend vorgetrocknet, anschließend in einem indirekt beheizten Drehrohrofen bei 6 - maliger Produktumwälzung je Ofenumdrehhung und bei einem Raum/Zeit - Koeffizienten von 5 bis 10 m?3¿/h im Inertgasstrom karbonisiert und die karbonisierten Formlinge in einem indirekt beheizten Drehrohrofen bei 8 - maliger Produktumwälzung je Ofenumdrehung und bei einem Raum/Zeit-Koeffizienten von 1 bis 5 m?3¿/h unter Zugabe von Wasserdampf im Inertgasstrom diskontinuierlich aktiviert werden. Man erhält hochwertige, geformte Hochleistungsadsorbenzien, die vielseitig verwendet werden können und insbesondere für den Einsatz zur Lufttrennung, zur adsorptiven Kühlung und als adsorptive Komponente in textilen und synthetischen Flächengebilden geeignet sind.
(EN)The invention relates to the production of shaped high-performance adsorbing materials by means of steam activation in a rotary kiln which operates discontinuously. Spherically pre-formed materials are gently pre-dried with hot gas in a rotary dryer in said kiln, with the product being turned 4 times per kiln rotation and at a space/time coefficient of 1 to 2.5 m?3¿/h, then carbonized in an indirectly heated rotary kiln with the product being turned 6 times per kiln rotation and at a space/time coefficient of 5 to 10 m?3¿/h in a stream of inert gas. The carbonized shaped bodies are then activated in a discontinuous manner in an indirectly heated rotary kiln with the product being turned 8 times per kiln rotation and at a space/time coefficient of 1 to 5 m?3¿/h, steam being added, in a stream of inert gas. The resulting shaped, high-performance, adsorbing materials are of a high quality and have diverse application possibilities. They can be used especially for separating air, for adsorptive cooling and as an adsorptive component in flat textile and synthetic materials .
(FR)L'invention concerne la production d'adsorbants moulés hautement performants par activation à la vapeur dans un four tubulaire tournant fonctionnant par intermittence, dans lequel des matériaux prémoulés sphériques sont doucement préséchés par du gaz chaud dans un tambour à sécher à raison de 4 rotations du produit par révolution du four et pour un coefficient espace/temps de 1 à 2,5 m?3¿/h. Ensuite, ils sont carbonisés dans un flux de gaz inerte dans un four tubulaire tournant chauffé indirectement à raison de 6 rotations du produit par révolution du four et pour un coefficient espace/temps de 5 à 10 m?3¿/h. Les corps moulés carbonisés sont activés par intermittence dans le flux de gaz inerte avec apport de vapeur d'eau dans un four tubulaire tournant chauffé indirectement à raison de 8 rotations du produit par révolution du four et pour un coefficient espace/temps de 1 à 5 m?3¿/h. Ainsi on obtient des absorbants moulés hautement performants, de haute qualité, d'utilisation universelle et particulièrement adaptés à la séparation de l'air, au refroidissement adsorbant et comme composante adsorbante dans les produits plats textiles et synthétiques.
États désignés : JP.
Office européen des brevets (OEB) (AT, BE, CH, CY, DE, DK, ES, FI, FR, GB, GR, IE, IT, LU, MC, NL, PT, SE).
Langue de publication : allemand (DE)