1. (WO1986005529) PROCEDE DE PREPARATION DE PATE A PAPIER BLANCHIE A PARTIR DE MATIERES PREMIERES LIGNOCELLULOSIQUES
Dernières données bibliographiques dont dispose le Bureau international   

N° de publication :    WO/1986/005529    N° de la demande internationale :    PCT/FI1986/000028
Date de publication : 25.09.1986 Date de dépôt international : 24.03.1986
CIB :
D21C 3/00 (2006.01), D21C 9/16 (2006.01)
Déposants : OY KESKUSLABORATORIO - CENTRALLABORATORIUM AB [FI/FI]; Tekniikantie 2, SF-01280 Espoo (FI) (Tous Sauf US).
LAAMANEN, Lauri, Aukusti [FI/FI]; (FI) (US Seulement).
SUNDQUIST, Jorma, Juhani [FI/FI]; (FI) (US Seulement).
WARTIOVAARA, Ilkka, Yrjö, Paavo [FI/FI]; (FI) (US Seulement).
KAULIOMÄKI, Seppo, Veli-Matti [FI/FI]; (FI) (US Seulement).
POPPIUS, Kristiina, Johanna [FI/FI]; (FI) (US Seulement)
Inventeurs : LAAMANEN, Lauri, Aukusti; (FI).
SUNDQUIST, Jorma, Juhani; (FI).
WARTIOVAARA, Ilkka, Yrjö, Paavo; (FI).
KAULIOMÄKI, Seppo, Veli-Matti; (FI).
POPPIUS, Kristiina, Johanna; (FI)
Mandataire : SUNDMAN, Christoffer @; Seppo Laine Ky, Kasarmikatu 23 A, SF-00130 Helsinki (FI)
Données relatives à la priorité :
851156 22.03.1985 FI
860609 11.02.1986 FI
Titre (EN) PROCESS FOR PREPARING BLEACHED PULP OUT OF LIGNOCELLULOSIC RAW MATERIAL
(FR) PROCEDE DE PREPARATION DE PATE A PAPIER BLANCHIE A PARTIR DE MATIERES PREMIERES LIGNOCELLULOSIQUES
Abrégé : front page image
(EN)Lignocellulosic raw material is pulped with a cooking liquor containing organic peroxyacids, such as peroxyformic acid or peroxyacetic acid, and the defibred pulp is bleached with an alkaline solution containing hydrogen peroxide, the pH of which is at least 10 in the beginning of the treatment, and which is provided by adding to a sodium hydroxide solution hydrogen peroxide in an amount which calculated as per cents of the dry weight of the matter coming to the treatment corresponds to from 0.20 to 0.80, preferably from 0.25 to 0.70 and most preferably from 0.45 to 0.65 times the kappa number of the pulp obtained from the previous stage of the process.
(FR)Des matières premières lignocellulosiques sont réduites en pulpe avec une solution de cuisson contenant des peroxyacides organiques tels que l'acide peroxyformique ou l'acide peroxyacétique. La pulpe défibrée est blanchie avec une solution alcaline contenant du peroxyde d'hydrogène dont le pH est égal à au moins 10 au début du traitement et qui est obtenue en ajoutant à une solution d'hydroxyde de sodium une quantité de peroxyde d'hydrogène comprise entre 0,20 et 0,80 pour cent du poids à sec de la matière à traiter, de préférence entre 0,25 et 0,70 pour cent, ou, ce qui est encore préféreable, entre 0,45 et 0,65 fois le numéro kappa de la pulpe obtenue à l'issue de l'étape précédente du procédé.
États désignés : AU, JP, NO, SU, US.
Office européen des brevets (OEB) (AT, BE, CH, DE, FR, GB, IT, LU, NL, SE).
Langue de publication : anglais (EN)
Langue de dépôt : anglais (EN)