1. WO2022010494 - WORK METHOD TO DESIGN FOR THICKENING TIME BY TAILORING ADDITIVES

Publication Number WO/2022/010494
Publication Date 13.01.2022
International Application No. PCT/US2020/042275
International Filing Date 16.07.2020
IPC
C09K 8/467 2006.1
CCHEMISTRY; METALLURGY
09DYES; PAINTS; POLISHES; NATURAL RESINS; ADHESIVES; COMPOSITIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
KMATERIALS FOR APPLICATIONS NOT OTHERWISE PROVIDED FOR; APPLICATIONS OF MATERIALS NOT OTHERWISE PROVIDED FOR
8Compositions for drilling of boreholes or wells; Compositions for treating boreholes or wells, e.g. for completion or for remedial operations
42Compositions for cementing, e.g. for cementing casings into boreholes; Compositions for plugging, e.g. for killing wells
46containing inorganic binders, e.g. Portland cement
467containing additives for specific purposes
E21B 33/13 2006.1
EFIXED CONSTRUCTIONS
21EARTH OR ROCK DRILLING; MINING
BEARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
33Sealing or packing boreholes or wells
10in the borehole
13Methods or devices for cementing, for plugging holes, crevices, or the like
Applicants
  • HALLIBURTON ENERGY SERVICES, INC. [US]/[US]
Inventors
  • JANDHYALA, Siva Rama Krishna
  • SINGH, John Paul Bir
Agents
  • TUMEY, Corey S.
Priority Data
16/923,71808.07.2020US
Publication Language English (en)
Filing Language English (EN)
Designated States
Title
(EN) WORK METHOD TO DESIGN FOR THICKENING TIME BY TAILORING ADDITIVES
(FR) PROCÉDÉ DE TRAVAIL POUR LA CONCEPTION D'UN TEMPS D'ÉPAISSISSEMENT PAR ADAPTATION D'ADDITIFS
Abstract
(EN) A method of designing a cement slurry may include: (a) selecting at least a cement and concentration thereof, a water and concentration thereof, and one or more chemical additives and a concentration thereof such that a cement slurry formed from the cement, water, and the one or more chemical additives meet a density requirement; (b) calculating a thickening time of the cement slurry using a thickening time model; (c) comparing the thickening time of the cement slurry to a thickening time requirement, wherein steps (a)-(c) are repeated if the thickening time of the cement slurry does not meet or exceed the thickening time requirement, wherein the step of selecting comprises selecting concentrations and/or different chemical identities for the one or more chemical additives, cement, or water, or step (d) is performed if the thickening time of the cement slurry meets or exceeds the thickening time requirement; and (d) preparing the cement slurry.
(FR) Un procédé de conception d'une suspension de ciment peut comprendre: (A) sélectionner au moins un ciment et une concentration de celui-ci, une eau et une concentration de celui-ci, et un ou plusieurs additifs chimiques et une concentration de ceux-ci de telle sorte qu'une suspension de ciment formée à partir du ciment, de l'eau et du ou des additifs chimiques correspondent à une exigence de densité ; (b) calculer un temps d'épaississement de la suspension de ciment à l'aide d'un modèle de temps d'épaississement ; (c) comparer le temps d'épaississement de la suspension de ciment à une exigence de temps d'épaississement, lesdites étapes (a)- (c) étant répétées si le temps d'épaississement de la suspension de ciment ne satisfait pas ou ne dépasse pas l'exigence de temps d'épaississement, l'étape de sélection comprenant la sélection de concentrations et/ou d'identités chimiques différentes pour l'additif chimique ou les additifs chimiques, le ciment ou l'eau, ou bien l'étape (d) est effectuée si le temps d'épaississement de la suspension de ciment satisfait ou dépasse l'exigence de temps d'épaississement ; et (d) préparer la suspension de ciment.