1. WO2022004058 - METHOD FOR PRODUCING FLAME RETARDANT POLYCARBONATE RESIN COMPOSITION PELLET

Publication Number WO/2022/004058
Publication Date 06.01.2022
International Application No. PCT/JP2021/008902
International Filing Date 08.03.2021
IPC
B29B 9/06 2006.1
BPERFORMING OPERATIONS; TRANSPORTING
29WORKING OF PLASTICS; WORKING OF SUBSTANCES IN A PLASTIC STATE IN GENERAL
BPREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
9Making granules
02by dividing preformed material
06in the form of filamentary material, e.g. combined with extrusion
B29B 7/94 2006.1
BPERFORMING OPERATIONS; TRANSPORTING
29WORKING OF PLASTICS; WORKING OF SUBSTANCES IN A PLASTIC STATE IN GENERAL
BPREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
7Mixing; Kneading
80Component parts, details or accessories; Auxiliary operations
88Adding charges
94Liquid charges
Applicants
  • 三菱エンジニアリングプラスチックス株式会社 MITSUBISHI ENGINEERING-PLASTICS CORPORATION [JP]/[JP]
Inventors
  • 吉野 崇史 YOSHINO, Takafumi
  • 田尻 敏之 TAJIRI, Toshiyuki
  • 田島 寛之 TAJIMA, Hiroyuki
Agents
  • 小野 尚純 ONO, Hisazumi
  • 奥貫 佐知子 OKUNUKI, Sachiko
Priority Data
2020-11260330.06.2020JP
Publication Language Japanese (ja)
Filing Language Japanese (JA)
Designated States
Title
(EN) METHOD FOR PRODUCING FLAME RETARDANT POLYCARBONATE RESIN COMPOSITION PELLET
(FR) PROCÉDÉ DE PRODUCTION D'UNE PASTILLE COMPOSÉE DE RÉSINE DE POLYCARBONATE IGNIFUGE
(JA) 難燃性ポリカーボネート樹脂組成物ペレットの製造方法
Abstract
(EN) Provided is a method for producing a polycarbonate resin composition pellet with a twin-screw extruder, the polycarbonate resin composition pellet comprising: 30-95 mass% of (A) a resin pellet including more than 40 mass% of a polycarbonate resin in the pellet; 5-40 (exclusive of 40) mass% (B) a phosphate ester flame retardant that is liquid at room temperature; 0-50 mass% of (C) polycarbonate resin flakes; 0-30 mass% of (D) an ABS resin; and 0-15 mass% of (E) an additive other than (B). The method is characterized by including a first step for putting (A), (C), (D), and (E) into a twin-screw extruder and kneading with a first kneading unit, a second step for adding (B) to a downstream part in the first kneading unit and kneading with a second kneading unit, and a third step for decompressing a vent in the downstream part in the second kneading unit to devolatilize and extrude, wherein the first kneading unit has a specific screw configuration in which the length thereof is 2.4-6.0 D, and the second kneading unit has a specific screw configuration in which the length thereof is 1.3-4.0 D.
(FR) L'invention concerne un procédé de production d'une pastille composée de résine de polycarbonate au moyen d'une extrudeuse à double vis, la pastille composée de résine de polycarbonate comprenant : de 30 à 95 % en masse (A) d'une pastille de résine comprenant plus de 40 % en masse d'une résine de polycarbonate dans la pastille ; de 5 à moins de 40 % (40 % étant exclus) en masse (B) d'un retardateur de flamme à base d'ester de phosphate qui est liquide à température ambiante ; de 0 à 50 % en masse (C) de flocons de résine de polycarbonate ; de 0 à 30 % en masse (D) d'une résine ABS ; et de 0 à 15 % en masse (E) d'un additif autre que (B). Le procédé est caractérisé en ce qu'il comprend une première étape consistant à introduire (A), (C), (D) et (E) dans une extrudeuse à double vis et à effectuer un malaxage à l'aide d'une première unité de malaxage, une deuxième étape consistant à ajouter (B) au niveau d'une partie aval de la première unité de malaxage et à effectuer un malaxage à l'aide d'une seconde unité de malaxage, et une troisième étape consistant à décompresser un évent dans la partie aval de la seconde unité de malaxage pour effectuer une dévolatilisation et une extrusion, la première unité de malaxage ayant une configuration de vis spécifique dans laquelle la longueur de celle-ci va de 2,4 à 6,0 D, et la seconde unité de malaxage ayant une configuration de vis spécifique dans laquelle sa longueur va de 1,3 à 4,0 D.
(JA) ポリカーボネート樹脂をペレット中に40質量%超含む樹脂ペレット(A)30~95質量%、室温で液状のリン酸エステル難燃剤(B)5質量%以上40質量%未満、ポリカーボネート樹脂フレーク(C)0~50質量%、ABS樹脂(D)0~30質量%、及び(B)以外の他の添加剤(E)0~15質量%からなるポリカーボネート樹脂組成物ペレットを二軸押出機で製造する方法であって、 前記(A)、(C)、(D)及び(E)を二軸押出機に入れ、 第1混練部で混練する第1工程、第1混練部の下流部に前記(B)を添加し第2混練部で混練する第2工程、第2混練部の下流部でベントを減圧にして脱揮し押出する第3工程を含み、第1混練部は、特定のスクリュー構成で長さが2.5D~6.0Dの構成からなり、第2混練部は、特定のスクリュー構成で長さが1.3D~4.0Dの構成よりなることを特徴とする。