1. WO2020140358 - METHOD FOR PREPARING SILICA MICROSPHERES FOR ACIDIFIER CARRIER

Publication Number WO/2020/140358
Publication Date 09.07.2020
International Application No. PCT/CN2019/085748
International Filing Date 07.05.2019
IPC
A23K 20/20 2016.01
AHUMAN NECESSITIES
23FOODS OR FOODSTUFFS; THEIR TREATMENT, NOT COVERED BY OTHER CLASSES
KFEEDING-STUFFS SPECIALLY ADAPTED FOR ANIMALS; METHODS SPECIALLY ADAPTED FOR PRODUCTION THEREOF
20Accessory food factors for animal feeding-stuffs
20Inorganic substances, e.g. oligo-elements
C01B 33/12 2006.01
CCHEMISTRY; METALLURGY
01INORGANIC CHEMISTRY
BNON-METALLIC ELEMENTS; COMPOUNDS THEREOF
33Silicon; Compounds thereof
113Silicon oxides; Hydrates thereof
12Silica; Hydrates thereof, e.g. lepidoic silicic acid
CPC
A23K 20/20
AHUMAN NECESSITIES
23FOODS OR FOODSTUFFS; TREATMENT THEREOF, NOT COVERED BY OTHER CLASSES
KFODDER
20Accessory food factors for animal feeding-stuffs
20Inorganic substances, e.g. oligoelements
Applicants
  • 山东联科科技股份有限公司 SHANDONG LINK SCIENCE AND TECHNOLOGY CO., LTD [CN]/[CN]
Inventors
  • 胡金星 HU, Jinxing
  • 吴晓林 WU, Xiaolin
  • 高海明 GAO, Haiming
  • 柴金鉴 CHAI, Jinjian
  • 李祥凯 LI, Xiangkai
  • 孙玉军 SUN, Yujun
Agents
  • 北京德崇智捷知识产权代理有限公司 JW IP LAW FIRM
Priority Data
201910005833.X03.01.2019CN
Publication Language Chinese (ZH)
Filing Language Chinese (ZH)
Designated States
Title
(EN) METHOD FOR PREPARING SILICA MICROSPHERES FOR ACIDIFIER CARRIER
(FR) PROCÉDÉ DE PRÉPARATION DE MICROSPHÈRES DE SILICE POUR SUPPORT D'ACIDIFIANT
(ZH) 一种酸化剂载体用二氧化硅微球的制备方法
Abstract
(EN)
Disclosed is a method for preparing silica microspheres for an acidifier carrier, comprising the following steps: adding sodium silicate into a synthetic kettle, introducing steam while stirring and raising the temperature, adding water and stirring same to obtain a reaction base material A, adding sulfuric acid to the reaction base material A and acidifying same to a certain pH so as to obtain a reaction solution B into which sulfuric acid and sodium silicate are simultaneously added for a synthesis reaction to obtain a reaction solution C; then stopping the addition of sodium silicate, adding sulfuric acid alone for post-acidification until a certain pH, and curing same to obtain a dilute slurry D; and subjecting the dilute slurry D to filtration, washing, slurrying, thickening, and drying, thereby obtaining the silica microspheres for an acidifier carrier. The silica microspheres thus prepared have a uniform particle size, are difficult to break, do not agglomerate, have a fast adsorption rate, and have good free-flowing and adsorption properties.
(FR)
L'invention concerne un procédé de préparation de microsphères de silice pour un support d'acidifiant, comprenant les étapes suivantes : ajout de silicate de sodium dans une bouilloire synthétique, introduction de vapeur tout en agitant et en élevant la température, ajout d'eau et agitation de celle-ci pour obtenir un matériau de base de réaction A, ajout d'acide sulfurique au matériau de base de réaction A et acidification de celui-ci à un certain pH afin d'obtenir une solution de réaction B dans laquelle de l'acide sulfurique et du silicate de sodium sont ajoutés simultanément pour une réaction de synthèse en vue d'obtenir une solution de réaction C ; puis arrêt de l'ajout de silicate de sodium, ajout d'acide sulfurique seul pour une post-acidification jusqu'à un certain pH, et durcissement de celui-ci pour obtenir une barbotine diluée D ; et soumission de la barbotine diluée D à la filtration, au lavage, à la mise en suspension, à l'épaississement et au séchage, ce qui permet d'obtenir les microsphères de silice pour un support d'acidifiant. Les microsphères de silice ainsi préparées présentent une taille de particules uniforme, sont difficiles à casser, ne s'agglomèrent pas, ont un taux d'adsorption rapide et ont de bonnes propriétés d'écoulement et d'adsorption.
(ZH)
一种酸化剂载体用二氧化硅微球的制备方法,包括以下步骤:将硅酸钠加入到合成釜中,在搅拌的条件下通入蒸汽升温,加入水搅拌得到反应底料A,向反应底料A中加入硫酸,先酸化至一定pH,向得到的反应液B中同时加入硫酸和硅酸钠进行合成反应,得到反应液C;然后停止加入硅酸钠,只加入硫酸进行后酸化至一定pH,熟化后得到稀浆料D;稀浆料D经过滤、洗涤、制浆、增稠,干燥后,即得到所述的酸化剂载体用二氧化硅微球。由此制备的二氧化硅微球,微球的粒径均一,不易破碎,不结团,吸附速度快,流散性和吸附性好。