Processing

Please wait...

Settings

Settings

Goto Application

1. WO2020116643 - CARBURIZER AND CARBURIZATION METHOD USING SAME

Publication Number WO/2020/116643
Publication Date 11.06.2020
International Application No. PCT/JP2019/047930
International Filing Date 06.12.2019
IPC
C21C 7/00 2006.01
CCHEMISTRY; METALLURGY
21METALLURGY OF IRON
CPROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
7Treating molten ferrous alloys, e.g. steel, not covered by groups C21C1/-C21C5/118
C21C 5/52 2006.01
CCHEMISTRY; METALLURGY
21METALLURGY OF IRON
CPROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
5Manufacture of carbon steel, e.g. plain mild steel, medium carbon steel, or cast-steel
52Manufacture of steel in electric furnaces
Applicants
  • 日本製鉄株式会社 NIPPON STEEL CORPORATION [JP]/[JP]
Inventors
  • 宗岡 均 MUNEOKA, Hitoshi
  • 浅原 紀史 ASAHARA, Norifumi
  • 坂元 基紘 SAKAMOTO, Motohiro
  • 山▲崎▼ 強 YAMAZAKI, Tsuyoshi
Agents
  • 特許業務法人太陽国際特許事務所 TAIYO, NAKAJIMA & KATO
Priority Data
2018-23010807.12.2018JP
Publication Language Japanese (JA)
Filing Language Japanese (JA)
Designated States
Title
(EN) CARBURIZER AND CARBURIZATION METHOD USING SAME
(FR) CÉMENT ET PROCÉDÉ DE CÉMENTATION UTILISANT CELUI-CI
(JA) 加炭材およびそれを用いた加炭方法
Abstract
(EN)
This carburizer for carburizing molten iron housed in an electric furnace or a ladle, is a mixture of calcined lime and a carbon material having an ash content of 5-18 mass%, and satisfies the conditions 0.6≤(mc+Mc)/ms≤2.7 and 0.7≤(mc+Mc)/ma≤6.5. This carburization method uses said carburizer. Here, mc represents the mass of CaO in the carbon material, ms represents the mass of SiO2 in the carbon material, ma represents the mass of Al2O3 in the carbon material, and Mc represents the mass of the calcined lime.
(FR)
La présente invention concerne un cément pour cémenter du fer fondu logé dans un four électrique ou une poche de coulée, qui est un mélange de chaux calcinée et d’un matériau carboné ayant une teneur en cendres de 5 à 18 % en masse, et satisfait aux conditions 0,6≤(mc+Mc)/ms≤2,7 et 0,7≤(mc+Mc)/ma≤6,5. Ce procédé de cémentation utilise ledit cément. Selon l’invention, mc représente la masse de CaO dans le matériau carboné, ms représente la masse de SiO2 dans le matériau carboné, ma représente la masse de Al2O3 dans le matériau carboné, et Mc représente la masse de la chaux calcinée.
(JA)
電気炉または取鍋に収容された溶鉄に対して加炭を行う加炭材であって、灰分が5質量%以上18質量%以下の炭素材料と生石灰との混合物であり、0.6≦(mc+Mc)/ms≦2.7、かつ0.7≦(mc+Mc)/ma≦6.5の条件を満たす加炭材およびそれを用いた加炭方法。ここで、mcは前記炭素材料中のCaOの質量を表し、msは前記炭素材料中のSiO2の質量を表し、maは前記炭素材料中のAl23の質量を表し、Mcは前記生石灰の質量を表す。