Processing

Please wait...

Settings

Settings

Goto Application

1. WO2020090417 - COATING METHOD

Publication Number WO/2020/090417
Publication Date 07.05.2020
International Application No. PCT/JP2019/040158
International Filing Date 11.10.2019
IPC
G02B 1/10 2015.01
GPHYSICS
02OPTICS
BOPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
1Optical elements characterised by the material of which they are made; Optical coatings for optical elements
10Optical coatings produced by application to, or surface treatment of, optical elements
G02B 1/115 2015.01
GPHYSICS
02OPTICS
BOPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
1Optical elements characterised by the material of which they are made; Optical coatings for optical elements
10Optical coatings produced by application to, or surface treatment of, optical elements
11Anti-reflection coatings
113using inorganic layer materials only
115Multilayers
G02B 7/02 2006.01
GPHYSICS
02OPTICS
BOPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
7Mountings, adjusting means, or light-tight connections, for optical elements
02for lenses
Applicants
  • 日本電産サンキョー株式会社 NIDEC SANKYO CORPORATION [JP]/[JP]
  • 日本電産株式会社 NIDEC CORPORATION [JP]/[JP]
Inventors
  • 山本 明典 YAMAMOTO Akinori
  • 加本 貴則 KAMOTO Takanori
  • 中川 小百合 NAKAGAWA Sayuri
  • 塩原 秀 SHIOHARA Suguru
  • ダマスコティ ジェニファー トレス DAMASCO TY Jennifer Torres
  • 渡邉 友啓 WATANABE Tomohiro
Priority Data
2018-20477331.10.2018JP
Publication Language Japanese (JA)
Filing Language Japanese (JA)
Designated States
Title
(EN) COATING METHOD
(FR) PROCÉDÉ DE REVÊTEMENT
(JA) コーティング方法
Abstract
(EN)
The present invention provides a coating method which enables adequate coating of a function film on a first surface of a light-transmitting member. According to the present invention, when a hydrophilic film is formed on the surface of an antireflection film 8 by coating, after the formation of the antireflection film 8 on a first lens surface 11a of a first lens 11, the surface of the antireflection film 8 is irradiated with a plasma P, thereby enhancing the hydrophilicity of the surface. Subsequently, after immersing the first lens surface 11a in an aqueous treatment liquid 90 in an immersion step ST3, the first lens surface 11a is pulled up and then the first lens 11 is rotated, while keeping the first lens surface 11a face down, thereby removing excess treatment liquid 95 from the first lens surface 11a in a liquid removal step ST5. Consequently, the area where the treatment liquid 90 is applied and the thickness of the treatment liquid 90 can be controlled by the immersion depth of the first lens surface 11a in the immersion step ST2, the rotational speed of the first lens 11 in the liquid removal step ST5, and the like.
(FR)
La présente invention concerne un procédé de revêtement qui permet un revêtement adéquat d'un film fonctionnel sur une première surface d'un élément de transmission de lumière. Selon la présente invention, lorsqu'un film hydrophile est formé sur la surface d'un film antireflet 8 par revêtement, après la formation du film antireflet 8 sur une première surface de lentille 11a d'une première lentille 11, la surface du film antireflet est irradiée avec un plasma P, ce qui améliore l'hydrophilie de la surface. Ensuite, après immersion de la première surface de lentille 11a dans un liquide de traitement aqueux 90 dans une étape d'immersion ST3, la première surface de lentille 11a est tirée, puis la première lentille 11 est mise en rotation, tout en maintenant la première surface de lentille 11a vers le bas, ce qui permet d'éliminer le liquide de traitement excédentaire 95 de la première surface de lentille 11a dans une étape d'élimination de liquide ST5. Par conséquent, la zone où le liquide de traitement 90 est appliqué et l'épaisseur du liquide de traitement 90 peuvent être commandées par la profondeur d'immersion de la première surface de lentille 11a dans l'étape d'immersion ST2, la vitesse de rotation de la première lentille 11 dans l'étape d'élimination de liquide ST5, et analogues.
(JA)
透光性部材の第1面に機能膜を適正にコーティングすることのできるコーティング方法を提供すること。第1レンズ11の第1レンズ面11aに反射防止膜8を形成した後、反射防止膜8の表面に親水膜をコーティングするにあたって、反射防止膜8の表面にプラズマPを照射して親水性を高める。次に、浸漬工程ST3において第1レンズ面11aを水系の処理液90に浸漬した後、第1レンズ面11aを引き上げ、その後、脱液工程ST5では、第1レンズ面11aを下向きにした状態で第1レンズ11を回転させ、余剰な処理液95を第1レンズ面11aから離脱させる。従って、浸漬工程ST2における第1レンズ面11aの浸漬深さ、および脱液工程ST5における第1レンズ11の回転速度等によって、処理液90が塗布される範囲や処理液90の厚さを制御することができる。
Latest bibliographic data on file with the International Bureau