1. WO2020089781 - HIGH FLOW POLY(PHTHALAMIDE) COMPOSITIONS, AND ARTICLES MADE THEREFROM

Publication Number WO/2020/089781
Publication Date 07.05.2020
International Application No. PCT/IB2019/059242
International Filing Date 28.10.2019
IPC
C08L 77/06 2006.01
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
LCOMPOSITIONS OF MACROMOLECULAR COMPOUNDS
77Compositions of polyamides obtained by reactions forming a carboxylic amide link in the main chain; Compositions of derivatives of such polymers
06Polyamides derived from polyamines and polycarboxylic acids
CPC
C08L 77/06
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
LCOMPOSITIONS OF MACROMOLECULAR COMPOUNDS
77Compositions of polyamides obtained by reactions forming a carboxylic amide link in the main chain
06Polyamides derived from polyamines and polycarboxylic acids
Applicants
  • SABIC GLOBAL TECHNOLOGIES B.V. [NL]/[NL]
Inventors
  • ZHANG, Yaqin
  • SHEN, Liang
  • GUO, Mingcheng
  • ZHANG, Wei
Priority Data
18203571.730.10.2018EP
Publication Language English (EN)
Filing Language English (EN)
Designated States
Title
(EN) HIGH FLOW POLY(PHTHALAMIDE) COMPOSITIONS, AND ARTICLES MADE THEREFROM
(FR) COMPOSITIONS DE POLY(PHTALAMIDE) À ÉCOULEMENT ÉLEVÉ, ET ARTICLES FABRIQUÉS À PARTIR DE CES DERNIÈRES
Abstract
(EN)
A reinforced poly(phthalamide) composition comprising 20-80 weight percent of a poly(phthalamide) component comprising 15-55 weight percent of a crystalline poly(phthalamide), and 5-45 weight percent of an amorphous poly(phthalamide); 0.5-60 weight percent of a reinforcing filler; and 0.1-50 weight percent of an additive composition; wherein weight percent is based on the total weight of the reinforced poly(phthalamide) composition and totals 100; and wherein the reinforced poly(phthalamide) composition has a capillary melt viscosity, measured according to ASTM D3835 (2015) at 320 º C, at 5000 s-1, that is at least 10 % lower than that of the same reinforced poly(phthalamide) composition without the amorphous poly(phthalamide), and a warpage that is at least 15 % lower than that of the same reinforced poly(phthalamide) composition without the amorphous poly(phthalamide).
(FR)
La présente invention concerne une composition de poly(phtalamide) renforcée comprenant de 20 à 80 pour cent en poids d'un composant de poly(phtalamide) comprenant de 5 à 55 pour cent en poids d'un poly(phtalamide) cristallin, et 45 pour cent en poids d'un poly(phtalamide) amorphe; de 0,5 à 60 pour cent en poids d'une charge de renfort; et de 0,1 à 50 pour cent en poids d'une composition additive; où le pourcentage en poids est basé sur le poids total de la composition de poly(phtalamide) renforcée et totalise 100; et où la composition de poly(phtalamide) renforcée présente une viscosité capillaire à l'état fondu, mesurée selon la norme ASTM D3835 (2015) à 320 °C, à 5 000 s-1, qui est d'au moins 10 % inférieure à celle de la même composition de poly(phtalamide) renforcée sans le poly(phtalamide) amorphe, et présente un gauchissement qui est au moins 15 % moindre que celui de la même composition de poly(phtalamide) renforcée sans le poly(phtalamide) amorphe.