1. WO2020066875 - POLY(BIPHENYL ETHER SULFONE) RESIN, PRODUCTION METHOD THEREFOR, AND MELT-MOLDED ARTICLE

Publication Number WO/2020/066875
Publication Date 02.04.2020
International Application No. PCT/JP2019/036919
International Filing Date 20.09.2019
IPC
C08G 65/40 2006.01
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
GMACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
65Macromolecular compounds obtained by reactions forming an ether link in the main chain of the macromolecule
34from hydroxy compounds or their metallic derivatives
38derived from phenols
40from phenols and other compounds
CPC
C08G 65/40
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
GMACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
65Macromolecular compounds obtained by reactions forming an ether link in the main chain of the macromolecule
34from hydroxy compounds or their metallic derivatives
38derived from phenols
40from phenols (I) and other compounds (II), e.g. OH-Ar-OH + X-Ar-X, where X is halogen atom, i.e. leaving group
Applicants
  • 住友化学株式会社 SUMITOMO CHEMICAL COMPANY, LIMITED [JP]/[JP]
Inventors
  • 伊藤 和幸 ITO Kazuyuki
  • 前川 健典 MAEKAWA Kensuke
Agents
  • 棚井 澄雄 TANAI Sumio
  • 佐藤 彰雄 SATO Akio
  • 鈴木 慎吾 SUZUKI Shingo
  • 加藤 広之 KATO Hiroyuki
Priority Data
2018-18056026.09.2018JP
Publication Language Japanese (JA)
Filing Language Japanese (JA)
Designated States
Title
(EN) POLY(BIPHENYL ETHER SULFONE) RESIN, PRODUCTION METHOD THEREFOR, AND MELT-MOLDED ARTICLE
(FR) RÉSINE DE POLY(BIPHÉNYL-ÉTHER-SULFONE), SON PROCÉDÉ DE PRODUCTION ET ARTICLE MOULÉ À L'ÉTAT FONDU
(JA) ポリビフェニルエーテルスルホン樹脂及びその製造方法並びに溶融成形品
Abstract
(EN)
The present invention relates to a poly(biphenyl ether sulfone) resin which substantially comprises the repeating structure of formula (1). In analysis with an NMR device for examining solid samples in which a 13C spectrum is acquired using a Torchia pulse sequence and the delay period τ in the pulse sequence is changed to cause an attenuation in the signal intensity I(τ) corresponding to a chemical shift of 129 ppm, then the spin-lattice relaxation time T1L for long components which is calculated from the attenuation is 24 s or longer. [In formula (1), n is an integer of 1 or larger.]
(FR)
La présente invention concerne une résine de poly(biphényl-éther-sulfone) qui comprend sensiblement la structure de répétition de formule (1). Lors de l'analyse avec un dispositif de RMN permettant d'examiner des échantillons solides dans lesquels un spectre de 13C est acquis à l'aide d'une séquence d'impulsions de Torchia et la période de retard τ dans la séquence d'impulsions est modifiée pour provoquer une atténuation dans l'intensité de signal I(τ) correspondant à un déplacement chimique de 129 ppm, alors le temps de relaxation de réseau de spin T1L pour des constituants longs qui est calculé à partir de l'atténuation est supérieur ou égal à 24 s. [Dans la formule (1), n représente un nombre entier supérieur ou égal à 1].
(JA)
実質的に下記式(1)の繰り返し構造からなり、固体試料測定用のNMR装置を用いて、Torchiaのパルスシーケンスにより13Cのスペクトルを取得し、前記パルスシーケンスにおける待ち時間τの値を変化させることにより、化学シフト129ppmに該当する信号強度I(τ)の減衰から算出される、長い成分のスピン-格子緩和時間T1Lが24s以上である、ポリビフェニルエーテルスルホン樹脂等に関する。〔式中、nは1以上の整数を示す。〕