Processing

Please wait...

Settings

Settings

1. WO2020003690 - MOLDED RESIN PRODUCT INCLUDING WHOLLY AROMATIC LIQUID CRYSTAL POLYESTER RESIN CAPABLE OF REDUCING DIELECTRIC LOSS TANGENT BY HEAT TREATMENT, AND ELECTRIC/ELECTRONIC COMPONENT

Publication Number WO/2020/003690
Publication Date 02.01.2020
International Application No. PCT/JP2019/015305
International Filing Date 08.04.2019
IPC
C CHEMISTRY; METALLURGY
08
ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
J
WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H142
7
Chemical treatment or coating of shaped articles made of macromolecular substances
C CHEMISTRY; METALLURGY
08
ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
G
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
63
Macromolecular compounds obtained by reactions forming a carboxylic ester link in the main chain of the macromolecule
02
Polyesters derived from hydroxy carboxylic acids or from polycarboxylic acids and polyhydroxy compounds
60
derived from the reaction of a mixture of hydroxy carboxylic acids, polycarboxylic acids and polyhydroxy compounds
H ELECTRICITY
01
BASIC ELECTRIC ELEMENTS
B
CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES
3
Insulators or insulating bodies characterised by the insulating materials; Selection of materials for their insulating or dielectric properties
18
mainly consisting of organic substances
30
plastics; resins; waxes
42
polyesters; polyethers; polyacetals
C08J 7/00 (2006.01)
C08G 63/60 (2006.01)
H01B 3/42 (2006.01)
CPC
C08G 63/60
C08J 7/00
H01B 3/42
Applicants
  • JXTGエネルギー株式会社 JXTG NIPPON OIL & ENERGY CORPORATION [JP/JP]; 東京都千代田区大手町一丁目1番2号 1-2, Otemachi 1-chome, Chiyoda-ku, Tokyo 1008162, JP
Inventors
  • 鷲野 豪介 WASHINO Gosuke; JP
Agents
  • 永井 浩之 NAGAI Hiroshi; JP
  • 中村 行孝 NAKAMURA Yukitaka; JP
  • 朝倉 悟 ASAKURA Satoru; JP
Priority Data
2018-12124826.06.2018JP
Publication Language Japanese (JA)
Filing Language Japanese (JA)
Designated States
Title
(EN) MOLDED RESIN PRODUCT INCLUDING WHOLLY AROMATIC LIQUID CRYSTAL POLYESTER RESIN CAPABLE OF REDUCING DIELECTRIC LOSS TANGENT BY HEAT TREATMENT, AND ELECTRIC/ELECTRONIC COMPONENT
(FR) PRODUIT DE RÉSINE MOULÉE COMPRENANT UNE RÉSINE DE POLYESTER À CRISTAUX LIQUIDES ENTIÈREMENT AROMATIQUE CAPABLE DE RÉDUIRE LA TANGENTE DE PERTE DIÉLECTRIQUE PAR TRAITEMENT THERMIQUE, ET COMPOSANT ÉLECTRIQUE/ÉLECTRONIQUE
(JA) 熱処理により誘電正接を低減できる全芳香族液晶ポリエステル樹脂を含む樹脂成形品および電気電子部品
Abstract
(EN)
[Problem] To provide a molded resin product including a wholly aromatic liquid crystal polyester resin, the molded resin product having high heat resistance and an extremely low dielectric loss tangent even at high frequency bands. [Solution] This molded resin product, which includes a wholly aromatic liquid crystal polyester resin and is formed by heat treatment, is characterized in that an enthalpy change ΔH1 at a melting point of cycle 1 in a heating process and an enthalpy change ΔH2 at a melting point of cycle 2, which are measured with a differential scanning calorimeter, satisfy ΔH1/ΔH2≧2.0, and a dielectric loss tangent measured with the SPDR method at a measuring frequency of 10 GHz is 0.85×10-3 or less.
(FR)
La présente invention vise à fournir un produit de résine moulé comprenant une résine de polyester à cristaux liquides entièrement aromatique, le produit de résine moulé ayant une résistance à la chaleur élevée et une tangente de perte diélectrique extrêmement faible même à des bandes de fréquences élevées. L'invention concerne par conséquent un produit de résine moulé, qui comprend une résine de polyester à cristaux liquides entièrement aromatique et qui est formé par traitement thermique, est caractérisé en ce qu'un changement d'enthalpie ΔH1 à un point de fusion du cycle 1 dans un processus de chauffage et un changement d'enthalpie ΔH2 à un point de fusion du cycle 2, qui sont mesurés avec un calorimètre à balayage différentiel, satisfont à ΔH1/ΔH2≧2,0, et une tangente de perte diélectrique mesurée avec la méthode SPDR à une fréquence de mesure de 10 GHz est de 0,85 × 10-3 ou moins.
(JA)
[課題]高周波数帯においても著しく低い誘電正接および高耐熱性を有する、全芳香族液晶ポリエステル樹脂を含む樹脂成形品の提供。 [解決手段]本発明による全芳香族液晶ポリエステル樹脂を含み、熱処理が施されてなる樹脂成形品は、示差走査熱量計で測定した昇温過程の1サイクル目の融点でのエンタルピー変化ΔHと2サイクル目の融点でのエンタルピー変化ΔHが、ΔH/ΔH≧2.0を満たし、かつ、測定周波数10GHzにおけるSPDR法で測定した誘電正接が、0.85×10-3以下であることを特徴とする。
Latest bibliographic data on file with the International Bureau