1. WO2018155248 - NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY

Publication Number WO/2018/155248
Publication Date 30.08.2018
International Application No. PCT/JP2018/004778
International Filing Date 13.02.2018
IPC
H01M 10/0587 2010.1
HELECTRICITY
01BASIC ELECTRIC ELEMENTS
MPROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
10Secondary cells; Manufacture thereof
05Accumulators with non-aqueous electrolyte
058Construction or manufacture
0587of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
CPC
H01M 10/05
HELECTRICITY
01BASIC ELECTRIC ELEMENTS
MPROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
10Secondary cells; Manufacture thereof
05Accumulators with non-aqueous electrolyte
H01M 10/0587
HELECTRICITY
01BASIC ELECTRIC ELEMENTS
MPROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
10Secondary cells; Manufacture thereof
05Accumulators with non-aqueous electrolyte
058Construction or manufacture
0587of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
Y02E 60/10
YSECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
EREDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
60Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
10Energy storage using batteries
Y02P 70/50
YSECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
PCLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
70Climate change mitigation technologies in the production process for final industrial or consumer products
50Manufacturing or production processes characterised by the final manufactured product
Applicants
  • 三洋電機株式会社 SANYO ELECTRIC CO., LTD. [JP]/[JP]
Inventors
  • 笠松 真治 KASAMATSU Shinji
  • 市川 雄太 ICHIKAWA Yuta
Agents
  • 徳田 佳昭 TOKUDA Yoshiaki
  • 西田 浩希 NISHIDA Hiroki
Priority Data
2017-03310124.02.2017JP
Publication Language Japanese (ja)
Filing Language Japanese (JA)
Designated States
Title
(EN) NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY
(FR) BATTERIE SECONDAIRE À ÉLECTROLYTE NON AQUEUX
(JA) 非水電解質二次電池
Abstract
(EN) The objective of the present invention is to prevent a negative electrode in a bent section of a flat-shaped wound electrode body from over-charging locally, and prevent a positive electrode core body in the bent section from cracking. The non-aqueous electrolyte secondary battery according to one mode of the present invention comprises: a flat-shaped electrode body in which a wound pole plate group having a positive electrode plate, a negative electrode plate, and a separator interposed therebetween; a non-aqueous electrolyte; and an exterior body. The positive electrode plate has a positive electrode core body and a positive electrode mixture layer formed on the surface thereof. The negative electrode plate has a negative electrode core body and a negative electrode mixture layer formed on the surface thereof. In a cross section orthogonal to the winding axis, at each of the end portions in the major axis direction, the electrode body has a bent section wherein the pole plate group is bent. Among the surfaces on the winding inner side of the positive electrode mixture layer within each of the bent sections, a resin tape is adhered in a section of the positive electrode plate disposed most toward the beginning of the winding. The resin tape contains an adhesive layer, and a base material layer that does not transmit lithium ions. The adhesive force of the resin tape with respect to the positive electrode mixture layer is between 0.1 N/cm and 2 N/cm inclusive.
(FR) La présente invention a pour objet d’empêcher qu’une électrode négative dans une section coudée d’un corps d’électrode enroulée de forme plane ne soit localement surchargée, et d’empêcher qu’un corps de noyau d’électrode positive dans la section coudée ne se fissure. La batterie secondaire à électrolyte non aqueux selon un mode de la présente invention comprend : un corps d’électrode de forme plane dans lequel un groupe de plaques de pôle enroulé a une plaque d’électrode positive, une plaque d’électrode négative et un séparateur entreposé entre les plaques ; un électrolyte non aqueux ; et un corps extérieur. La plaque d’électrode positive a un corps de noyau d’électrode positive et une couche de mélange d’électrode positive formée à la surface de la plaque. La plaque d’électrode négative a un corps de noyau d’électrode négative et une couche de mélange d’électrode négative formée à la surface de la plaque. Dans une section transversale orthogonale aux axes d’enroulement, à chacune des parties d’extrémité dans la direction axiale majeure, le corps d’électrode a une section coudée dans laquelle le groupe de plaques de pôle est coudé. Parmi les surfaces sur la face interne d'enroulement de la couche de mélange d’électrode positive à l’intérieur de chacune des sections coudées, un ruban de résine est collé dans une section de la plaque d’électrode positive disposée la plus vers le début de l’enroulement. Le ruban de résine contient une couche adhésive et une couche de matériau de base qui ne transmet pas d’ions lithium. La force d’adhésion du ruban de résine par rapport à la couche de mélange d’électrode positive est comprise entre 0,1 N/cm et 2 N/cm inclus.
(JA) 本発明は、偏平状の巻回電極体の湾曲部における負極の局所的な過剰充電を防止するとともに、湾曲部における正極芯体のクラックを抑制することを目的とする。本発明の一態様に係る非水電解質二次電池は、正極板、負極板、及びそれらの間に介在するセパレータを有する極板群が巻回された偏平状の電極体と、非水電解質と、外装体と、を含む。正極板は、正極芯体とその表面に形成された正極合剤層を有し、負極板は、負極芯体とその表面に形成された負極合剤層を有する。電極体は、巻回軸に垂直な断面の長径方向の両端部に極板群が湾曲している湾曲部を有する。湾曲部内の正極合剤層の巻内側の表面のうち、正極板の最も巻き始め側に配置されている部分に樹脂テープが貼着されている。樹脂テープは粘着剤層と、リチウムイオンを透過しない基材層を含んでいる。樹脂テープの正極合剤層に対する粘着力は、0.1N/cm以上2N/cm以下である。