1. WO2016151955 - METHOD FOR ESTIMATING INITIAL CREEP STRENGTH OF HEAT-RESISTANT MEMBER, AND METHOD FOR ASSESSING REMAINING SERVICE LIFE THEREOF

Publication Number WO/2016/151955
Publication Date 29.09.2016
International Application No. PCT/JP2015/084237
International Filing Date 07.12.2015
IPC
G01N 17/00 2006.01
GPHYSICS
01MEASURING; TESTING
NINVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
17Investigating resistance of materials to the weather, to corrosion or to light
G01N 3/00 2006.01
GPHYSICS
01MEASURING; TESTING
NINVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
3Investigating strength properties of solid materials by application of mechanical stress
CPC
G01N 17/00
GPHYSICS
01MEASURING; TESTING
NINVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
17Investigating resistance of materials to the weather, to corrosion, or to light
G01N 3/00
GPHYSICS
01MEASURING; TESTING
NINVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
3Investigating strength properties of solid materials by application of mechanical stress
Applicants
  • 三菱重工業株式会社 MITSUBISHI HEAVY INDUSTRIES, LTD. [JP]/[JP]
Inventors
  • 森岡 真也 MORIOKA, Shinya
  • 岩▲崎▼ 修吾 IWASAKI, Shugo
  • 堤 博一 TSUTSUMI, Hirokazu
  • 片山 哲司 KATAYAMA, Tetsuji
Agents
  • 光石 俊郎 MITSUISHI, Toshiro
Priority Data
2015-06400526.03.2015JP
Publication Language Japanese (JA)
Filing Language Japanese (JA)
Designated States
Title
(EN) METHOD FOR ESTIMATING INITIAL CREEP STRENGTH OF HEAT-RESISTANT MEMBER, AND METHOD FOR ASSESSING REMAINING SERVICE LIFE THEREOF
(FR) PROCÉDÉ D'ESTIMATION DE LA RÉSISTANCE INITIALE AU FLUAGE D'UN ÉLÉMENT RÉSISTANT À LA CHALEUR, ET PROCÉDÉ D'ÉVALUATION DE LA DURÉE DE VIE RESTANTE
(JA) 耐熱部材の初期クリープ強度推定方法およびこの残寿命推定方法
Abstract
(EN)
Provided is a method for estimating the initial creep strength of a heat-resistant member which is capable of quickly estimating the initial creep strength of a heat-resistant member by using a comparatively simple operation. The method involves: deriving a breakage-time LMP by using a relational expression on the basis of creep test results (S2); obtaining a creep strength diagram of the heat-resistant member, on the basis of the breakage-time LMP and a design creep strength diagram expressing the relationship between the LMP and stress in the heat-resistant member (S3); estimating the equivalent average operation temperature on the basis of the condition of the carbide in the heat-resistant member (S4); deriving the remaining service life of the heat-resistant member by using a relational expression, on the basis of the heat-resistant member creep strength diagram and the equivalent average operation temperature (S5); deriving the total service life of the heat-resistant member on the basis of the remaining service life of the heat-resistant member and the operation time of the heat-resistant member (S6); deriving the total service life LMP by using a relational expression, on the basis of the total service life of the heat-resistant member and the equivalent average operation temperature (S7); and deriving an initial creep strength diagram of the heat-resistant member by using the design creep strength diagram, on the basis of the total service life LMP (S8).
(FR)
L'invention concerne un procédé d'estimation de la résistance initiale au fluage d'un élément résistant à la chaleur qui permet d'estimer rapidement la résistance initiale au fluage d'un élément résistant à la chaleur à l'aide d'une opération comparativement simple. Le procédé comprend : la dérivation d'un LMP du temps à rupture à l'aide d'une expression relationnelle basée sur des résultats d'essais de fluage (S2) ; l'obtention d'un diagramme de résistance au fluage de l'élément résistant à la chaleur basé sur le LMP du temps à rupture et d'un diagramme de résistance de dimensionnement au fluage exprimant la relation entre le LMP et la contrainte dans l'élément résistant à la chaleur (S3) ; l'estimation de la température de fonctionnement moyenne équivalente basée sur l'état du carbure dans l'élément résistant à la chaleur (S4) ; la dérivation de la durée de vie restante de l'élément résistant à la chaleur à l'aide d'une expression relationnelle, basée sur le diagramme de résistance au fluage de l'élément résistant à la chaleur et la température de fonctionnement moyenne équivalente (S5) ; la dérivation de la durée de vie totale de l'élément résistant à la chaleur basée sur la durée de vie restante de l'élément résistant à la chaleur et le temps de fonctionnement de l'élément résistant à la chaleur (S6) ; la dérivation du LMP de durée de vie totale à l'aide d'une expression relationnelle, basée sur la durée de vie totale de l'élément résistant à la chaleur et la température de fonctionnement moyenne équivalente (S7) ; et la dérivation d'un diagramme de résistance initiale au fluage de l'élément résistant à la chaleur à l'aide du diagramme de résistance de dimensionnement au fluage basé sur le LMP de durée de vie totale (S8).
(JA)
 比較的簡易な作業で耐熱部材の初期クリープ強度を迅速に推定することができる耐熱部材の初期クリープ強度推定方法を提供することにある。クリープ試験結果に基づき関係式を用いて破断時LMPを導出し(S2)、破断時LMPと耐熱部材における応力およびLMPの関係を示す設計クリープ強度線図とに基づき、耐熱部材のクリープ強度線図を取得し(S3)、耐熱部材の炭化物状態から等価平均運転温度を推定し(S4)、前記耐熱部材のクリープ強度線図と前記等価平均運転温度とに基づき関係式を用いて耐熱部材の残寿命を導出し(S5)、耐熱部材の残寿命と耐熱部材の運転時間とに基づき耐熱部材の全寿命を導出し(S6)、耐熱部材の全寿命と等価平均運転温度とに基づき関係式を用いて全寿命LMPを導出し(S7)、全寿命LMPに基づき設計クリープ強度線図を用いて、耐熱部材の初期クリープ強度線図を導出した(S8)。