1. (WO2015040186) METHOD FOR PRODUCING A POROUS CARBON PRODUCT
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/2015/040186    International Application No.:    PCT/EP2014/070044
Publication Date: 26.03.2015 International Filing Date: 19.09.2014
IPC:
C04B 35/52 (2006.01), C04B 38/00 (2006.01), C04B 38/04 (2006.01), C04B 35/63 (2006.01), C04B 35/638 (2006.01)
Applicants: HERAEUS QUARZGLAS GMBH & CO. KG [DE/DE]; Quarzstrasse 8 63450 Hanau (DE)
Inventors: NEUMANN, Christian; (DE).
OTTER, Matthias; (DE).
BECKER, Jörg; (DE).
PIHAN, Sascha; (DE)
Agent: STAUDT, Armin; (DE)
Priority Data:
102013110453.3 20.09.2013 DE
Title (DE) VERFAHREN ZUR HERSTELLUNG EINES PORÖSEN KOHLENSTOFFERZEUGNISSES
(EN) METHOD FOR PRODUCING A POROUS CARBON PRODUCT
(FR) PROCÉDÉ DE FABRICATION D'UN PRODUIT POREUX À BASE DE CARBONE
Abstract: front page image
(DE)Bei einem bekannten Verfahren zur Herstellung eines porösen Kohlenstofferzeugnisses werden Templatmaterial in Form von Templat-Partikeln, die Makroporen enthalten, sowie eine polymerisierbare Vorläufersubstanz für Kohlenstoff bereitgestellt. Die Makroporen des Templats werden mit der Vorläufersubstanz in gelöster oder geschmolzener Form infiltriert. Nach dem Carbonisieren der infiltrierten Vorläufersubstanz wird das unter Bildung des porösen Kohlenstofferzeugnisses entfernt. Um das Verfahrens so zu modifizieren, dass eine Kohlen- stoffstruktur mit hierarchischer Porosität mit einem hohen Anteil an Mesoporen mit Porengrößen im Bereich von 2 bis 50nm erhalten wird, wird erfindungsgemäß vorgeschlagen, dass die Vorläufersubstanz nach dem Infiltrieren gemäß Verfahrensschritt (c) und vor dem Carbonisieren gemäß Verfahrensschritt (d) innerhalb der Makroporen des Templats einer Behandlung bei einer Schaumbildungstemperatur unterzogen wird, bei der die Vorläufersubstanz unter Polykondensation aufschäumt und dabei die Makroporen als im Wesentlichen mesoporiger Schaum auffüllt, bei dem mindestens 70 % der Poren Porengrößen im Bereich von 10 bis 150 nm haben.
(EN)In a known method for producing a porous carbon product, template material in the form of template particles, which contain macropores, and a polymerizable precursor substance for carbon are provided. The macropores of the template are infiltrated with the precursor substance in dissolved or melted form. After the carbonization of the infiltrated precursor substance, the template is removed in order to form the porous carbon product. According to the invention, in order to modify the method in such a way that a carbon structure having hierarchical porosity having a high fraction of mesopores having pore sizes in the range of 2 to 50 nm is obtained, after the infiltration according to step (c) and before the carbonization according to step (d), the precursor substance is subjected within the macropores of the template to a treatment at a foaming temperature at which the precursor substance foams under polycondensation and fills the macropores as substantially mesoporous foam, in which at least 70% of the pores have pore sizes in the range of 10 to 150 nm.
(FR)On connaît un procédé de fabrication d'un matériau poreux à base de carbone qui consiste à préparer un matériau matriciel sous la forme de particules matricielles qui contiennent des macropores, ainsi qu'un précurseur de carbone polymérisable. Les macropores du matériau matriciel sont infiltrés par le précurseur de carbone sous forme dissoute ou fondue. Après la carbonisation du précurseur infiltré, le matériau matriciel est enlevé, ce qui donne le produit poreux à base de carbone. L'invention vise à modifier ce procédé de telle manière qu'on obtienne une structure à base de carbone dotée d'une porosité hiérarchique présentant une part élevée de mésopores d'une taille comprise entre 2 et 5 nm. A cet effet, le précurseur est soumis dans les macropores du matériau matriciel, après l'infiltration selon l'étape (c) du procédé et avant la carbonisation selon l'étape (d) du procédé, à un traitement à une température de formation de mousse sous l'effet duquel le précurseur mousse par polycondensation et remplit les macropores sous la forme d'une mousse sensiblement mésoporeuse, au moins 70 % des pores présentant une taille comprise entre 10 et 150 nm.
Designated States: AE, AG, AL, AM, AO, AT, AU, AZ, BA, BB, BG, BH, BN, BR, BW, BY, BZ, CA, CH, CL, CN, CO, CR, CU, CZ, DE, DK, DM, DO, DZ, EC, EE, EG, ES, FI, GB, GD, GE, GH, GM, GT, HN, HR, HU, ID, IL, IN, IR, IS, JP, KE, KG, KN, KP, KR, KZ, LA, LC, LK, LR, LS, LU, LY, MA, MD, ME, MG, MK, MN, MW, MX, MY, MZ, NA, NG, NI, NO, NZ, OM, PA, PE, PG, PH, PL, PT, QA, RO, RS, RU, RW, SA, SC, SD, SE, SG, SK, SL, SM, ST, SV, SY, TH, TJ, TM, TN, TR, TT, TZ, UA, UG, US, UZ, VC, VN, ZA, ZM, ZW.
African Regional Intellectual Property Organization (BW, GH, GM, KE, LR, LS, MW, MZ, NA, RW, SD, SL, ST, SZ, TZ, UG, ZM, ZW)
Eurasian Patent Organization (AM, AZ, BY, KG, KZ, RU, TJ, TM)
European Patent Office (AL, AT, BE, BG, CH, CY, CZ, DE, DK, EE, ES, FI, FR, GB, GR, HR, HU, IE, IS, IT, LT, LU, LV, MC, MK, MT, NL, NO, PL, PT, RO, RS, SE, SI, SK, SM, TR)
African Intellectual Property Organization (BF, BJ, CF, CG, CI, CM, GA, GN, GQ, GW, KM, ML, MR, NE, SN, TD, TG).
Publication Language: German (DE)
Filing Language: German (DE)