1. (WO2013045327) STRUCTURALLY STABLE ACTIVE MATERIAL FOR BATTERY ELECTRODES
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/2013/045327    International Application No.:    PCT/EP2012/068430
Publication Date: 04.04.2013 International Filing Date: 19.09.2012
IPC:
H01M 4/62 (2006.01), H01M 4/134 (2010.01), H01M 10/0525 (2010.01), H01M 4/1395 (2010.01), H01M 4/133 (2010.01), H01M 4/1393 (2010.01), H01M 4/04 (2006.01), H01M 4/02 (2006.01), H01M 4/36 (2006.01), H01M 4/587 (2010.01)
Applicants: VARTA MICRO INNOVATION GMBH [AT/AT]; Stremayrgasse 9 A-8010 Graz (AT)
Inventors: SCHARFEGGER, Michaela; (AT).
KREN, Harald; (AT).
KOLLER, Stefan; (AT)
Agent: PATENTANWÄLTE RUFF, WILHELM, BEIER, DAUSTER & PARTNER; Kronenstraße 30 70174 Stuttgart (DE)
Priority Data:
11182723.4 26.09.2011 EP
Title (DE) STRUKTURSTABILES AKTIVMATERIAL FÜR BATTERIEELEKTRODEN
(EN) STRUCTURALLY STABLE ACTIVE MATERIAL FOR BATTERY ELECTRODES
(FR) MATÉRIAU ACTIF STRUCTURELLEMENT STABLE POUR ÉLECTRODES DE BATTERIES
Abstract: front page image
(DE)Verfahren zur Herstellung von Aktivmaterial für die Elektrode einer elektrochemischen Zelle. Als Komponente 1 werden Lithium interkalierende Kohlenstoffpartikel mit einer mittleren Partikelgröße zwischen 1 μm und 100 μm bereitgestellt, als Komponente 2 Siliziumpartikel mit einer mittleren Partikelgröße zwischen 5 nm und 500 nm und als Komponente 3 ein zu amorphem Kohlenstoff pyrolisierbares Polymer oder ein pyrolisierbarer Polymervorläufer, ausgewählt aus der Gruppe mit Epoxidharz, Polyurethanharz und Polyesterharz. Die Komponenten werden gemischt. Die Mischung wird anschließend unter Ausschluß von Luftsauerstoff bei einer Temperatur wärmebehandelt, bei der sich das pyrolisierbare Polymer oder der pyrolisierbare Polymervorläufer unter Bildung von amorphem Kohlenstoff zersetzt. Weiterhin beschrieben werden ein gemäß diesem Verfahren herstellbares elektrochemisches Aktivmaterial, eine Elektrode umfassend ein solches Aktivmaterial und eine elektrochemische Zelle umfassend eine solche Elektrode.
(EN)Method for producing active material for the electrode of an electrochemical cell. Lithium‑intercalating carbon particles with an average particle size of between 1 μm and 100 μm are provided as component 1, silicon particles with an average particle size of between 5 nm and 500 nm are provided as component 2, and a polymer which can be pyrolized to form amorphous carbon or a pyrolizable polymer precursor, selected from the group consisting of epoxy resin, polyurethane resin and polyester resin, is provided as component 3. The components are mixed. The mixture is then heat‑treated with exclusion of atmospheric oxygen at a temperature at which the pyrolizable polymer or the pyrolizable polymer precursor decomposes so as to form amorphous carbon. Also described are: an electrochemical active material which can be produced in accordance with this method, an electrode comprising such an active material and an electrochemical cell comprising such an electrode.
(FR)L'invention concerne un procédé de production de matériau actif pour les électrodes d'une cellule électrochimique. Comme composant 1, on utilise des particules de carbone avec lithium intercalé présentant une granulométrie moyenne comprise entre 1 et 100 µm, comme composant 2 des particules de silicium présentant une granulométrie moyenne comprise entre 5 et 500 nm, et comme composant 3 un polymère ou un précurseur de polymère pyrolysable pour donner du carbone amorphe, choisi dans le groupe constitué par une résine époxyde, une résine de polyuréthane et une résine de polyester. On mélange les composants puis on soumet le mélange à un traitement thermique, sous exclusion de l'oxygène de l'air, à une température à laquelle le polymère ou le précurseur de polymère pyrolysable se décompose en formant du carbone amorphe. L'invention concerne en outre un matériau actif électrochimique qui peut être obtenu par ce procédé, une électrode contenant un tel matériau actif, ainsi qu'une cellule électrochimique comprenant une telle électrode.
Designated States: AE, AG, AL, AM, AO, AT, AU, AZ, BA, BB, BG, BH, BN, BR, BW, BY, BZ, CA, CH, CL, CN, CO, CR, CU, CZ, DE, DK, DM, DO, DZ, EC, EE, EG, ES, FI, GB, GD, GE, GH, GM, GT, HN, HR, HU, ID, IL, IN, IS, JP, KE, KG, KM, KN, KP, KR, KZ, LA, LC, LK, LR, LS, LT, LU, LY, MA, MD, ME, MG, MK, MN, MW, MX, MY, MZ, NA, NG, NI, NO, NZ, OM, PA, PE, PG, PH, PL, PT, QA, RO, RS, RU, RW, SC, SD, SE, SG, SK, SL, SM, ST, SV, SY, TH, TJ, TM, TN, TR, TT, TZ, UA, UG, US, UZ, VC, VN, ZA, ZM, ZW.
African Regional Intellectual Property Organization (BW, GH, GM, KE, LR, LS, MW, MZ, NA, RW, SD, SL, SZ, TZ, UG, ZM, ZW)
Eurasian Patent Organization (AM, AZ, BY, KG, KZ, RU, TJ, TM)
European Patent Office (AL, AT, BE, BG, CH, CY, CZ, DE, DK, EE, ES, FI, FR, GB, GR, HR, HU, IE, IS, IT, LT, LU, LV, MC, MK, MT, NL, NO, PL, PT, RO, RS, SE, SI, SK, SM, TR)
African Intellectual Property Organization (BF, BJ, CF, CG, CI, CM, GA, GN, GQ, GW, ML, MR, NE, SN, TD, TG).
Publication Language: German (DE)
Filing Language: German (DE)