Processing

Please wait...

Settings

Settings

Goto Application

1. WO2011108660 - METHOD FOR PRODUCING MODIFIED NATURAL RUBBER

Publication Number WO/2011/108660
Publication Date 09.09.2011
International Application No. PCT/JP2011/054944
International Filing Date 03.03.2011
IPC
C08C 19/06 2006.1
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
CTREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
19Chemical modification of rubber
04Oxidation
06Epoxidation
CPC
C08C 1/04
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
CTREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
1Treatment of rubber latex
02Chemical or physical treatment of rubber latex before or during concentration
04Purifying; Deproteinising
C08C 19/06
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
CTREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
19Chemical modification of rubber
04Oxidation
06Epoxidation
C08C 2/02
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
CTREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
2Treatment of rubber solutions
02Purification
C08L 15/00
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
LCOMPOSITIONS OF MACROMOLECULAR COMPOUNDS
15Compositions of rubber derivatives
Applicants
  • 豊田合成 株式会社 TOYODA GOSEI CO., LTD. [JP]/[JP] (AllExceptUS)
  • 国立大学法人 長岡技術科学大学 NATIONAL UNIVERSITY CORPORATION NAGAOKA UNIVERSITY OF TECHNOLOGY [JP]/[JP] (AllExceptUS)
  • 岩瀬 直生 IWASE, Naoki [JP]/[JP] (UsOnly)
  • 今井 英幸 IMAI, Hideyuki [JP]/[JP] (UsOnly)
  • 瀬尾 明繁 SEO, Akishige [JP]/[JP] (UsOnly)
  • 河原 成元 KAWAHARA, Seiichi [JP]/[JP] (UsOnly)
  • 山本 祥正 YAMAMOTO, Yoshimasa [JP]/[JP] (UsOnly)
  • 塩原 圭一郎 SHIOBARA, Keiichiro [JP]/[JP] (UsOnly)
Inventors
  • 岩瀬 直生 IWASE, Naoki
  • 今井 英幸 IMAI, Hideyuki
  • 瀬尾 明繁 SEO, Akishige
  • 河原 成元 KAWAHARA, Seiichi
  • 山本 祥正 YAMAMOTO, Yoshimasa
  • 塩原 圭一郎 SHIOBARA, Keiichiro
Agents
  • 恩田 博宣 ONDA, Hironori
Priority Data
2010-04951205.03.2010JP
Publication Language Japanese (ja)
Filing Language Japanese (JA)
Designated States
Title
(EN) METHOD FOR PRODUCING MODIFIED NATURAL RUBBER
(FR) PROCÉDÉ DE PRODUCTION D'UN CAOUTCHOUC NATUREL MODIFIÉ
(JA) 改質天然ゴムの製造方法
Abstract
(EN) Disclosed is a method for producing modified natural rubber, comprising an epoxidation step, a removal step, and a reduction and ring-opening step. In the epoxidation step, in a latex in which a plant-derived rubbery polymer having a plurality of unsaturated double bonds in the main chain is dispersed in water serving as a dispersion medium, an organic peracid is reacted with the rubbery polymer. In this manner, by the epoxidation of a part of the unsaturated double bonds in the rubbery polymer, an epoxidated rubbery polymer is obtained. In the removal step, organic peracid-derived substances generated from the organic peracid in the epoxidation step are removed from the latex, whereby the content of the organic peracid-derived substances in the latex is reduced to 35 parts by mass or less based on 100 parts by mass of the epoxidated rubbery polymer. In the reduction and ring-opening step, under the conditions of pH 7 to 8 and in the presence of an organic acid salt, a part or the whole of the remaining unsaturated double bonds in the epoxidated rubbery polymer in the latex are reduced, and also a part or the whole of the epoxy groups in the epoxidated rubbery polymer are ring-opened.
(FR) La présente invention concerne un procédé de production d'un caoutchouc naturel modifié, comprenant une étape d'époxydation, une étape d'élimination, et une étape de réduction et d'ouverture de cycle. Lors de l'étape d'époxydation, dans un latex dans lequel un polymère caoutchouteux dérivé de plantes ayant une pluralité de double-liaisons insaturées dans la chaîne principale est dispersé dans l'eau servant de milieu de dispersion, un peracide organique est mis en réaction avec le polymère caoutchouteux. De cette manière, par le biais de l'époxydation d'une partie des double-liaisons insaturées dans le polymère caoutchouteux, un polymère caoutchouteux époxydé est obtenu. Lors de l'étape d'élimination, les substances dérivées du peracide organique générées à partir du peracide organique lors de l'étape d'époxydation sont éliminées du latex, la teneur des substances dérivées du peracide organique dans le latex étant de ce fait abaissée à une teneur inférieure ou égale à 35 parties en poids en se basant sur les 100 parties en poids du polymère caoutchouteux époxydé. Lors de l'étape de réduction et d'ouverture de cycle, dans des conditions de pH de 7 à 8 et en présence d'un sel d'acide organique, une partie ou la totalité des double-liaisons insaturées restantes dans le polymère caoutchouteux époxydé dans le latex sont réduites, et une partie ou la totalité des groupes époxy dans le polymère caoutchouteux époxydé subissent une ouverture de cycle.
(JA)  改質天然ゴムの製造方法は、エポキシ化工程と、除去工程と、還元・開環工程とを有する。エポキシ化工程では、主鎖に複数の不飽和二重結合を有する植物由来のゴム状重合体を、分散媒としての水に分散させたラテックス中にて、ゴム状重合体に有機過酸を反応させる。これにより、ゴム状重合体の不飽和二重結合の一部がエポキシ化することによって、エポキシ化ゴム状重合体が得られる。除去工程では、エポキシ化工程において有機過酸から生じた有機過酸由来の物質をラテックス中から除去して、ラテックス中における有機過酸由来の物質の含有量をエポキシ化ゴム状重合体100質量部に対して35質量部以下にまで低下させる。還元・開環工程では、pH7~8の条件下で、且つ有機酸塩の存在下にて、ラテックス中のエポキシ化ゴム状重合体に残存する不飽和二重結合の一部又は全部が還元されると共に、エポキシ化ゴム状重合体のエポキシ基の一部又は全部が開環される。
Related patent documents
Latest bibliographic data on file with the International Bureau