1. (WO2009135697) METHOD FOR PRODUCING A BONE CEMENT WITH BIOACTIVITY AND BONE CEMENT KIT
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/2009/135697    International Application No.:    PCT/EP2009/003453
Publication Date: 12.11.2009 International Filing Date: 06.05.2009
IPC:
A61L 24/00 (2006.01)
Applicants: MUE-BOND GMBH [DE/DE]; Friedrichstrasse 81 10117 Berlin (DE) (For All Designated States Except US).
MÜLLER, Wolf-Dieter [DE/DE]; (DE) (For US Only).
MITZNER, Elke [DE/DE]; (DE) (For US Only).
MÜLLER, Christian [DE/DE]; (DE) (For US Only)
Inventors: MÜLLER, Wolf-Dieter; (DE).
MITZNER, Elke; (DE).
MÜLLER, Christian; (DE)
Agent: GULDE HENGELHAUPT ZIEBIG & SCHNEIDER; Wallstraße 58/59 10179 Berlin (DE)
Priority Data:
10 2008 022 723.4 06.05.2008 DE
Title (DE) VERFAHREN ZUR HERSTELLUNG EINES KNOCHENZEMENTS MIT BIOAKTIVITÄT UND KNOCHENZEMENT-KIT
(EN) METHOD FOR PRODUCING A BONE CEMENT WITH BIOACTIVITY AND BONE CEMENT KIT
(FR) PROCÉDÉ DE PRÉPARATION D'UN CIMENT OSSEUX BIOACTIF ET KIT POUR CIMENT OSSEUX
Abstract: front page image
(DE)Die Erfindung betrifft ein Herstellungsverfahren eines Knochenzements mit Bioaktivität und einen entsprechenden Knochenzement-Kit. Das Verfahren besteht darin, dass ein monomerfreies Polymethylmethacrylat (PMMA) mit einer massegemittelten Molekülmasse von 30000 bis 200000 und einer Säurezahl von 10 bis 350 mg KOH pro g Polymer in einer Menge von 5 bis 13 Gew-%, mit einem Lösungsmittel für PMMA vermischt werden und der Mischung 40 bis 97 Gew-%, wenigstens ein kristallines und/oder glaskristallines Material zugegeben wird mit der Maßgabe, dass das kristalline und/oder glaskristalline Material 15 - 60 Gew-% CaO, 30 - 50 Gew-% P2O5, 0 - 9 Gew-% ZrO2 und 0 - 3 Gew-% Fluorid enthält, und das Mischen unter Rühren und bei einer Temperatur von 10 bis 500°C bis zum Erhalt einer fließfähigen Mischung mit einer offenen Verarbeitungszeit im Bereich von 1 bis 20 Minuten erfolgt. Vorteilhaft ist der Zusatz von 0,1-10 Gew-% ZnO. Die Verwendung des Materials ist bevorzugt als Zement oder Knochenfüllmaterial im Dentalbereich sowie als Zement für die Kyphoplastie oder Vertebroplastie sowie als Befestigungszement für Gelenkprothesen.
(EN)The invention relates to a method for producing a bone cement with bioactivity and a corresponding bone cement kit. The method comprises mixing a monomer-free polymethylmethacrylate (PMMA) with a mass average molecular weight of 30,000 to 200,000 and an acid number of 10 to 350 mg KOH per g polymer in am amount of 5 to 13 wt. %, with a solvent for PMMA and 40 to 97 wt. % of at least one crystalline and/or glass-crystalline material is added to the mixture with the proviso that the crystalline or glass crystalline material contains 15 - 60 wt.% CaO, 30 - 50 wt.% P2O5, 0 - 9 wt.% ZrO2 and 0 - 3 wt.% fluoride and the mixing and stirring is carried out at a temperature of 10 to 500°C to give a free-flowing mixture with an open processing time in the range 1 to 20 minutes. The addition id preferably of 0.1-10 wt.% ZnO. The material is preferably used as cement or bone filler material in dentistry and as cement for kyphoplasty or vertebroplasty and as fixing cement for joint prostheses.
(FR)L'invention concerne un procédé de préparation d'un ciment osseux bioactif, et un kit pour ciment osseux correspondant. Le procédé consiste à mélanger un polyméthylméthacrylate (PMMA) exempt de monomères présentant une masse moléculaire moyenne en masse de 30000 à 200000 et un indice d'acidité de 10 à 350 mg KOH par g de polymère, selon une proportion de 5 à 13 % en poids, avec un solvant pour PMMA et à ajouter à ce mélange de 40 à 97 % en poids d'au moins une matière cristalline et/ou cristalline vitreuse, ladite matière cristalline et/ou cristalline/vitreuse contenant de 15 à 60 % en poids de CaO, de 30 à 50 % en poids de P2O5, de 0 à 9 %en poids de ZrO2, et de 0 à 3 % en poids de fluorure, et à mélanger sous agitation, à une température 10 à 500°C jusqu'à obtention d'un mélange fluide, présentant un temps ouvert de travail se situant dans une plage de 1 à 20 minutes. Avantageusement, de 0,1 à 10 % en poids de ZnO sont ajoutés à ce mélange. Ce matériau est utilisé de préférence comme ciment ou matériau de remplissage osseux dans le domaine dentaire, et comme ciment de kyphoplastie ou de vertébroplastie ainsi que comme ciment de fixation de prothèses articulaires.
Designated States: AE, AG, AL, AM, AO, AT, AU, AZ, BA, BB, BG, BH, BR, BW, BY, BZ, CA, CH, CN, CO, CR, CU, CZ, DE, DK, DM, DO, DZ, EC, EE, EG, ES, FI, GB, GD, GE, GH, GM, GT, HN, HR, HU, ID, IL, IN, IS, JP, KE, KG, KM, KN, KP, KR, KZ, LA, LC, LK, LR, LS, LT, LU, LY, MA, MD, ME, MG, MK, MN, MW, MX, MY, MZ, NA, NG, NI, NO, NZ, OM, PG, PH, PL, PT, RO, RS, RU, SC, SD, SE, SG, SK, SL, SM, ST, SV, SY, TJ, TM, TN, TR, TT, TZ, UA, UG, US, UZ, VC, VN, ZA, ZM, ZW.
African Regional Intellectual Property Organization (BW, GH, GM, KE, LS, MW, MZ, NA, SD, SL, SZ, TZ, UG, ZM, ZW)
Eurasian Patent Organization (AM, AZ, BY, KG, KZ, MD, RU, TJ, TM)
European Patent Office (AT, BE, BG, CH, CY, CZ, DE, DK, EE, ES, FI, FR, GB, GR, HR, HU, IE, IS, IT, LT, LU, LV, MC, MK, MT, NL, NO, PL, PT, RO, SE, SI, SK, TR)
African Intellectual Property Organization (BF, BJ, CF, CG, CI, CM, GA, GN, GQ, GW, ML, MR, NE, SN, TD, TG).
Publication Language: German (DE)
Filing Language: German (DE)