1. (WO2007011973) PROCESS TO PRODUCE LOW VISCOSITY POLY-ALPHA-OLEFINS
Latest bibliographic data on file with the International Bureau

Pub. No.: WO/2007/011973 International Application No.: PCT/US2006/027943
Publication Date: 25.01.2007 International Filing Date: 19.07.2006
IPC:
C08F 210/14 (2006.01) ,C10M 143/08 (2006.01) ,C08F 210/04 (2006.01)
C CHEMISTRY; METALLURGY
08
ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
F
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
210
Copolymers of unsaturated aliphatic hydrocarbons having only one carbon-to-carbon double bond
14
Monomers containing five or more carbon atoms
C CHEMISTRY; METALLURGY
10
PETROLEUM, GAS OR COKE INDUSTRIES; TECHNICAL GASES CONTAINING CARBON MONOXIDE; FUELS; LUBRICANTS; PEAT
M
LUBRICATING COMPOSITIONS; USE OF CHEMICAL SUBSTANCES EITHER ALONE OR AS LUBRICATING INGREDIENTS IN A LUBRICATING COMPOSITION
143
Lubricating composition characterised by the additive being a macromolecular hydrocarbon or such hydrocarbon modified by oxidation
08
containing aliphatic monomer having more than 4 carbon atoms
C CHEMISTRY; METALLURGY
08
ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
F
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
210
Copolymers of unsaturated aliphatic hydrocarbons having only one carbon-to-carbon double bond
04
Monomers containing three or four carbon atoms
Applicants:
EXXONMOBIL CHEMICAL PATENTS INC. [US/US]; 5200 Bayway Drive Baytown, TX 77520-5200, US (AllExceptUS)
WU, Margaret [US/US]; US (UsOnly)
COKER, Catalina, L. [US/US]; US (UsOnly)
WALZER, John, F. [US/US]; US (UsOnly)
JIANG, Peijun [CN/US]; US (UsOnly)
Inventors:
WU, Margaret; US
COKER, Catalina, L.; US
WALZER, John, F.; US
JIANG, Peijun; US
Agent:
BELL, Catherine, L. ; ExxonMobil Chemical Company Law Technology P.O. Box 2149 Baytown, TX 77522-2149, US
Priority Data:
60/700,60019.07.2005US
Title (EN) PROCESS TO PRODUCE LOW VISCOSITY POLY-ALPHA-OLEFINS
(FR) PROCEDE POUR PRODUIRE DES POLYALPHAOLEFINES DE FAIBLE VISCOSITE
Abstract:
(EN) This invention relates to a process to produce a polyalpha-olefin comprising: 1) contacting one or more alpha-olefm monomers having 3 to 24 carbon atoms with an unbridged substituted bis cyclopentadienyl transition metal compound having: 1) at least one non-isoolefm substitution on both cyclopentadientyl rings, or 2) at least two substitutions on at least one cyclopentadienyl ring, a non-coordinating anion activator, and optionally an alkyl- aluminum compound, where the molar ratio of transition metal compound to activator is 10:1 to 0.1 :1, and if the alkyl aluminum compound is present then the molar ratio of alkyl aluminum compound to transition metal compound is 1 :4 to 4000:1, under polymerization conditions wherein: i) hydrogen is present at a partial pressure of Q.I to 50 psi, based upon the total pressure of the reactor or the concentration of the hydrogen is from 1 to 10,000 ppm or less by weight ; ii) wherein the alpha-olefin monomer(s) having 3 to 24 carbon atoms are present at 10 volume % or more based upon the total volume of the catalyst/activator/alkylaluminum compound solutions, monomers, and any diluents or solvents present in the reaction; iii) the residence time of the reaction is at least 5 minutes; iv) the productivity of the process is at least 43,000 grams of total product per gram of transition metal compound; v) the process is continuous or semi-continuous, and vi) the temperature in the reaction zone does not rise by more than 10 °C during the reaction; and vii) ethylene is not present at more than 30 volume % of the monomers entering the reaction zone; and 2) obtaining a polyalpha-olefin (PAO), optionally hydrogenating the PAO, wherein the PAO comprises at least 50 mole% of a C3 to C24 alpha-olefin monomer, and wherein the PAO has a kinematic viscosity at 1000C of 20 cSt or less.
(FR) La présente invention concerne un procédé pour produire une polyalphaoléfine comprenant les étapes consistant à: 1) mettre en contact un ou plusieurs monomères de type alphaoléfines ayant 3 à 24 atomes de carbone avec un composé de bis-cyclopentadiényle non ponté substitué d'un métal de transition ayant: 1) au moins une substitution non isooléfinique sur les deux cycles cyclopentadiényles ou 2) au moins deux substitutions sur au moins un cycle cyclopentadiényle, un activateur d'anions non coordinant et éventuellement un composé d'alkylaluminium, la proportion molaire du composé du métal de transition par rapport à l'activateur étant de 10:1 à 0,1:1 et, si le composé d'alkylaluminium est présent, la proportion molaire du composé d'alkylaluminium par rapport au composé de métal de transition étant de 1:4 à 4000:1, dans des conditions de polymérisation selon lesquelles i) l'hydrogène est présent sous une pression partielle de 0,1 à 50 psi, sur la base de la pression totale du réacteur ou la concentration de l'hydrogène va de 1 à 10 000 ppm ou moins en poids; ii) le ou les monomères de type alphaoléfines ayant 3 à 24 atomes de carbone sont présents à hauteur de 10 % en volume ou plus sur la base du volume total des solutions de catalyseur/activateur/composé d'alkylaluminium, des monomères et de tous diluants ou solvants présents dans la réaction; iii) le temps de séjour de la réaction est d'au moins 5 minutes; iv) la productivité du procédé est d'au moins 43 000 grammes de produit total par gramme du composé de métal de transition; v) le procédé est continu ou semi-continu; vi) la température dans la zone de réaction ne monte pas de plus de 10 °C au cours de la réaction; et vii) de l'éthylène n'est pas présent à hauteur de plus de 30 % en volume des monomères entrant dans la zone de réaction; et 2) obtenir une polyalphaoléfine (PAO), éventuellement hydrogéner la PAO, la PAO comprenant au moins 50 % molaires d'un monomère de type alphaoléfine en C3 à C24 et la PAO ayant une viscosité cinématique à 1000 °C inférieure ou égale à 20 cSt.
Designated States: AE, AG, AL, AM, AT, AU, AZ, BA, BB, BG, BR, BW, BY, BZ, CA, CH, CN, CO, CR, CU, CZ, DE, DK, DM, DZ, EC, EE, EG, ES, FI, GB, GD, GE, GH, GM, HN, HR, HU, ID, IL, IN, IS, JP, KE, KG, KM, KN, KP, KR, KZ, LA, LC, LK, LR, LS, LT, LU, LV, LY, MA, MD, MG, MK, MN, MW, MX, MZ, NA, NG, NI, NO, NZ, OM, PG, PH, PL, PT, RO, RS, RU, SC, SD, SE, SG, SK, SL, SM, SY, TJ, TM, TN, TR, TT, TZ, UA, UG, US, UZ, VC, VN, ZA, ZM, ZW
African Regional Intellectual Property Organization (ARIPO) (BW, GH, GM, KE, LS, MW, MZ, NA, SD, SL, SZ, TZ, UG, ZM, ZW)
Eurasian Patent Organization (AM, AZ, BY, KG, KZ, MD, RU, TJ, TM)
European Patent Office (AT, BE, BG, CH, CY, CZ, DE, DK, EE, ES, FI, FR, GB, GR, HU, IE, IS, IT, LT, LU, LV, MC, NL, PL, PT, RO, SE, SI, SK, TR)
African Intellectual Property Organization (BF, BJ, CF, CG, CI, CM, GA, GN, GQ, GW, ML, MR, NE, SN, TD, TG)
Publication Language: English (EN)
Filing Language: English (EN)
Also published as:
MXMX/a/2008/000841EP1910432JP2009503147CA2616009AU2006269945