1. (WO2003072617) POLYMERIZATION PROCESS FOR PREPARING SYNDIOTACTIC 1,2-POLYBUTADIENE
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/2003/072617    International Application No.:    PCT/US2003/002889
Publication Date: 04.09.2003 International Filing Date: 31.01.2003
Chapter 2 Demand Filed:    01.09.2003    
IPC:
C08F 136/06 (2006.01)
Applicants: BRIDGESTONE CORPORATION [JP/JP]; 10-1, Kyobashi 1-Chome, Chuo-Ku, Tokyo, Tokyo 104 (JP) (For All Designated States Except US).
LUO, Steven [US/US]; (US) (For US Only)
Inventors: LUO, Steven; (US)
Agent: VASUTA, John; Bridgestone/Firestone Americas Holding, Inc., 50 Century Blvd., Nashville, TN 37214 (US).
ALBRECHT, Thomas; Kraus & Weisert, Thomas-Wimmer-Ring 15, 80539 Munich (DE)
Priority Data:
10/079,205 20.02.2002 US
Title (EN) POLYMERIZATION PROCESS FOR PREPARING SYNDIOTACTIC 1,2-POLYBUTADIENE
(FR) PROCEDE DE POLYMERISATION POUR PREPARER DU 1,2-POLYBUTADIENE SYNDIOTACTIQUE
Abstract: front page image
(EN)A process for synthesizing syndiotactic 1,2-polybutaidene, the process comprising the steps of (1) polymerizing monomer consisting essentially of 1,3-butadeine monomer within an organic solvent that includes at least 50% by weight of aliphatic solvent by using an iron-based catalyst composition, where said step of polymerizing occurs at a temperature above about 65°C, thereby forming a supersaturated solution of syndiotactic 1,2-polybutaidene, (2) maintaining the supersaturated solution of syndiotactic 1,2-polybutaidene at a temperature above about 65°C until isolation of the syndiotactic 1,2-polybutadiene is desired, and (3) isolating the syndiotactic 1,2-polybutaidene from the supersaturated solution.
(FR)L'invention concerne un procédé de synthèse de 1,2-polybutadiène syndiotactique, ce procédé consistant à (1) polymériser un monomère constitué essentiellement d'un monomère de 1,3-butadiène dans un solvant organique contenant au moins 50 % en poids d'un solvant aliphatique au moyen d'une composition catalytique à base de fer, cette étape de polymérisation ayant lieu à une température supérieure à 65 °C approximativement, de façon à former une solution sursaturée de 1,2-polybutadiène syndiotactique, (2) maintenir cette solution sursaturée de 1,2-polybutadiène syndiotactique à une température supérieure à 65 °C approximativement jusqu'à ce que l'isolement du 1,2-polybutadiène syndiotactique soit souhaité et (3) isoler le 1,2-polybutadiène syndiotactique de la solution sursaturée.
Designated States: JP, US.