1. (WO2001002631) POLYURETHANEUREA ELASTIC FIBER
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/2001/002631    International Application No.:    PCT/KR2000/000678
Publication Date: 11.01.2001 International Filing Date: 29.06.2000
IPC:
D01F 1/10 (2006.01), D01F 6/70 (2006.01)
Applicants: KOLON INDUSTRIES, INC. [KR/KR]; Kolon Tower, 1-23, Byulyang-dong, Kwacheon-city, Kyunggi-do 427-040 (KR) (For All Designated States Except US).
KWON, Il, Cheon [KR/KR]; (KR) (For US Only).
RYU, Seok, Chul [KR/KR]; (KR) (For US Only).
HUH, Hyung, Don [KR/KR]; (KR) (For US Only)
Inventors: KWON, Il, Cheon; (KR).
RYU, Seok, Chul; (KR).
HUH, Hyung, Don; (KR)
Agent: CHO, Hwal, Rai; Suite 1507, Yoksam Heights, 642-19, Yoksam-dong, Kangnam-ku, Seoul-city 135-080 (KR)
Priority Data:
1999/26438 02.07.1999 KR
2000/35828 28.06.2000 KR
Title (EN) POLYURETHANEUREA ELASTIC FIBER
(FR) FIBRE ELASTIQUE A BASE DE POLYURETHANEUREE ET PROCEDE DE FABRICATION
Abstract: front page image
(EN)This invention relates to a polyurethaneurea elastic fiber of which the weatherability is excellent and the preparing method thereof. The invention prepares the polyurethaneurea elastic fiber by adding the formamidine type ultraviolet absorber of formula I to the spinning dope and the strength maintenance rate of the polyurethaneurea elastic fiber is over 90 % after being left for 24 hours at the Fade-O-Meter in which the sunshine carbon arc is installed, wherein, R1 and R2 represent an each alkyl group of 1 to 5 carbon atoms.
(FR)Cette invention concerne une fibre élastique à base de polyuréthaneurée qui possède une excellente résistance aux intempéries, ainsi qu'un procédé de fabrication de cette fibre. Cette fibre élastique à base de polyuréthaneurée est obtenue en ajoutant à la solution à filer un adsorbeur ultraviolet de type formamidine qui correspond à la formule (I) où R et R représentent chacun un groupe alkyle comportant de 1 à 5 atomes de carbone. Cette fibre élastique à base de polyuréthaneurée possède un taux de conservation de sa résistance de plus de 90 % après avoir été laissée pendant 24 heures dans un fadéomètre où se trouve l'arc au carbone brillant.