1. (WO2000025839) METHOD FOR PREPARING BONE MATERIAL
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/2000/025839    International Application No.:    PCT/EP1999/008056
Publication Date: 11.05.2000 International Filing Date: 25.10.1999
Chapter 2 Demand Filed:    24.05.2000    
IPC:
A61F 2/28 (2006.01), A61F 2/30 (2006.01), A61K 35/32 (2006.01), A61K 38/17 (2006.01), A61L 24/00 (2006.01), A61L 27/36 (2006.01), A61L 31/00 (2006.01)
Applicants: TUTOGEN MEDICAL GMBH [DE/DE]; Industriestrasse 6 D-91077 Neunkirchen am Brand (DE) (For All Designated States Except US).
KÜBLER, Norbert [DE/DE]; (DE) (For US Only)
Inventors: KÜBLER, Norbert; (DE)
Agent: MANITZ, FINSTERWALD & PARTNER GBR; Postfach 22 16 11 D-80506 München (DE)
Priority Data:
198 49 984.1 29.10.1998 DE
Title (DE) VERFAHREN ZUR PRÄPARATION VON KNOCHENMATERIAL
(EN) METHOD FOR PREPARING BONE MATERIAL
(FR) PROCEDE POUR LA PREPARATION DE MATIERE OSSEUSE
Abstract: front page image
(DE)Bei einem Verfahren zur Präparation von Knochenmaterial wird das demineralisierte Knochenmaterial einem autolytischen Abbau sowie einer Extraktion seiner zellulären Komponenten unterworfen unter gleichzeitiger Erhaltung seiner osteoinduktiven Matrixproteine. Dies wird durch Inkubation in einer Phosphatpufferlösug in Kombination mit einer Mischung aus Enzyminhibitoren erreicht, wobei die Verweilzeit in der Pufferlösung 24 Stunden nicht überschreitet.
(EN)The invention relates to a method for preparing bone material. According to said method, the demineralized bone material is subjected to an autolytic decomposition and an extraction of its cellular components while at the same time its osteoinductive matrix proteins are maintained. To this end, the bone material is incubated in a phosphate buffer solution in combination with a mixture of enzyme inhibitors. The dwelling time in the buffer solution does not exceed 24 hours.
(FR)L'invention concerne un procédé pour la préparation de matière osseuse, dans lequel on soumet la matière osseuse déminéralisée à une décomposition autolytique ainsi qu'à une extraction de ses composants cellulaires, tout en conservant ses porines ostéo-inductives. A cet effet, on procède à une incubation dans une solution tampon de phosphate en combinaison avec un mélange d'inhibiteurs d'enzymes, le temps de séjour dans la solution tampon ne dépassant pas 24 heures.
Designated States: CA, CZ, IL, KR, NO, TR, US, ZA.
European Patent Office (AT, BE, CH, CY, DE, DK, ES, FI, FR, GB, GR, IE, IT, LU, MC, NL, PT, SE).
Publication Language: German (DE)
Filing Language: German (DE)