1. (WO1999011712) THERMOPLASTIC POLYURETHANE ADDITIVES FOR IMPROVED POLYMER MATRIX COMPOSITES AND METHODS OF MAKING AND USING THEREFOR
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1999/011712    International Application No.:    PCT/US1998/018054
Publication Date: 11.03.1999 International Filing Date: 31.08.1998
Chapter 2 Demand Filed:    11.12.1998    
IPC:
C08L 67/00 (2006.01), C08L 67/02 (2006.01), C08L 69/00 (2006.01)
Applicants: EASTMAN CHEMICAL COMPANY [US/US]; 100 North Eastman Road Kingsport, TN 37660 (US)
Inventors: BRINK, Andrew, Edwin; (US).
OWENS, Jeffrey, Todd; (US)
Agent: BOSHEARS, Betty, Joy; P.O. Box 511 Kingsport, TN 37662-5075 (US)
Priority Data:
60/057,894 04.09.1997 US
09/140,514 26.08.1998 US
Title (EN) THERMOPLASTIC POLYURETHANE ADDITIVES FOR IMPROVED POLYMER MATRIX COMPOSITES AND METHODS OF MAKING AND USING THEREFOR
(FR) ADDITIFS DE POLYURETHANNE THERMOPLASTIQUE POUR COMPOSITES MATRICIELS POLYMERES ET PROCEDES DE FABRICATION ET D'UTILISATION CORRESPONDANTS
Abstract: front page image
(EN)The present invention relates to a composite made by the process of melt mixing (a) a polymer having at least one isocyanate reactive group, wherein the polymer is from 30 to 90 % by weight of the composite; (b) a thermoplastic polyurethane at from 0.1 to less than 10 % by weight of the composite; and (c) a reinforcing fiber at from 9.9 to 60 % by weight of the composite, wherein the sum of the weight percentages of components (a)-(c) is equal to 100 %, wherein the polymer (a) is not a polyamide. The invention further relates to a composite prepared by the process of melt mixing (a) a polymer having at least one isocyanate reactive group, wherein the polymer is from 25 to 90 % by weight of the composite; (b) a thermoplastic polyurethane at from 0.1 to 10 % by weight of the composite; (c) a reinforcing fiber at from 9.8 to 60 % by weight of the composite, and (d) an epoxy compound at from 0.1 to 5 % by weight of the composite, wherein the sum of the weight percentages of components (a)-(d) is equal to 100 %. The invention further relates to the methods for making the composites of the present invention. The invention further relates to articles containing the composites of the present invention.
(FR)La présente invention se rapporte à un composite que l'on fabrique en mélangeant à l'état fondu (a) un polymère possédant au moins un groupe réactif isocyanate et constituant 30 à 90 % en poids du composite; (b) un polyuréthanne thermoplastique en quantité représentant 0,1 à moins de 10 % en poids du composite; et (c) une fibre de renforcement en quantité représentant 9,9 à 60 % en poids du composite, la somme des pourcentages en poids des composants (a) à (c) étant égale à 100 % et le polymère (a) n'étant pas un polyamide. L'invention se rapporte également à un composite que l'on prépare en mélangeant à l'état fondu (a) un polymère possédant au moins un groupe réactif isocyanate et constituant 25 à 90 % en poids du composite; (b) un polyuréthanne thermoplastique en quantité représentant 0,1 à moins de 10 % en poids du composite; et (c) une fibre de renforcement en quantité représentant 9,8 à 60 % en poids du composite et (d) un composé époxy en quantité représentant 0,1 à 5 % en poids du composite, la somme des pourcentages en poids des composants (a) à (d) étant égale à 100 %. Cette invention se rapporte en outre à des procédés de fabrication des composites décrits ci-dessus, ainsi qu'aux articles fabriqués à partir de ces composites.
Designated States: JP.
European Patent Office (AT, BE, CH, CY, DE, DK, ES, FI, FR, GB, GR, IE, IT, LU, MC, NL, PT, SE).