Search International and National Patent Collections
Some content of this application is unavailable at the moment.
If this situation persists, please contact us atFeedback&Contact
1. (WO1998052982) A PROCESS FOR PREPARING AN IN SITU POLYETHYLENE BLEND
Latest bibliographic data on file with the International Bureau

Pub. No.: WO/1998/052982 International Application No.: PCT/US1998/010253
Publication Date: 26.11.1998 International Filing Date: 19.05.1998
Chapter 2 Demand Filed: 15.10.1998
IPC:
C08F 210/16 (2006.01)
C CHEMISTRY; METALLURGY
08
ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
F
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
210
Copolymers of unsaturated aliphatic hydrocarbons having only one carbon-to-carbon double bond
16
Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
Applicants:
UNION CARBIDE CHEMICALS & PLASTICS TECHNOLOGY CORPORATION [US/US]; 39 Old Ridgebury Road Danbury, CT 06817-0001, US
Inventors:
KUPPERBLATT, Sandra, Ann; US
EALER, George, Edward; US
TILSTON, Michael, William; US
Agent:
JOHNSON WIGGINS, Karen; Union Carbide Chemicals & Plastics Technology Corporation 39 Old Ridgebury Road Danbury, CT 06817-0001, US
HAYES Adrian Chetwynd et al.; Boult Wade Tennant 27 Furnival Street London EC4A 1PQ, GB
Priority Data:
08/858,95120.05.1997US
Title (EN) A PROCESS FOR PREPARING AN IN SITU POLYETHYLENE BLEND
(FR) PROCEDE DE PREPARATION D'UN MELANGE DE POLYETHYLENE IN SITU
Abstract:
(EN) A process comprising contacting ethylene and one or two alpha-olefin comonomers, each having 3 to 8 carbon atoms, with a transition metal catalyst system including a hydrocarbylaluminum cocatalyst in each of two fluidized bed reactors connected in series, in the gas phase, under polymerization conditions. The copolymer formed in the first reactor has a flow index in the range of about 0.1 to about 75 grams per 10 minutes and a density in the range of 0.865 to 0.930 gram per cubic centimeter and the copolymer formed in the second reactor has a melt index in the range of about 0.2 to about 100 grams per 10 minutes and a density in the range of about 0.900 to about 0.965 gram per cubic centimeter, the weight ratio of the first reactor copolymer to second reactor copolymer being in the range of about 70:30 to about 30:70, and the in situ blend has a flow index in the range of about 5 to 100 grams per 10 minutes; a melt flow ratio in the range of about 10 about 100; a density in the range of 0.880 to 0.960 gram per cubic centimeter; and an Mw/Mn ratio in the range of about 2 to about 20.
(FR) Cette invention concerne un procédé qui consiste à mettre de l'éthylène ainsi qu'un ou deux comonomères d'alpha-oléfine, qui possèdent chacun de 3 à 8 atomes de carbone, en contact avec un système catalyseur à base d'un métal de transition qui comprend un cocatalyseur à base d'hydrocarbylaluminium. Cette mise en contact se fait dans deux réacteurs à lit fluidisé qui sont connectés en série, dans une phase gazeuse et dans des conditions de polymérisation. Le copolymère formé dans le premier réacteur possède un indice de fluidité qui varie environ de 0,1 à 75 grammes par 10 minutes, et une densité qui varie de 0,865 à 0,930 grammes par centimètre cube. Le copolymère formé dans le second réacteur possède un indice de fusion qui varie environ de 0,2 à 100 grammes par 10 minutes, et une densité qui varie environ de 0,900 à 0,965 grammes par centimètre cube. Le rapport en poids entre le copolymère du premier réacteur et le copolymère du second réacteur varie environ de 70:30 à 30:70. Le mélange in situ possède un indice de fluidité qui varie environ de 5 à 100 grammes par 10 minutes, un rapport fusion-fluidité qui varie environ de 10 à 100, une densité qui varie de 0,880 à 0,960 grammes par centimètre cube, et rapport Mw/Mn qui varie environ de 2 à 20.
Designated States: AU, BR, CA, JP, MX
European Patent Office (AT, BE, CH, CY, DE, DK, ES, FI, FR, GB, GR, IE, IT, LU, MC, NL, PT, SE)
Publication Language: English (EN)
Filing Language: English (EN)
Also published as:
MXPA/a/1999/010672EP0983307JP2001526725 CA2291106AU1998075804