1. (WO1998049352) METHOD FOR THERMAL TREATMENT OF GRANULATED IRON ORE BEFORE REDUCTION
Latest bibliographic data on file with the International Bureau

Pub. No.: WO/1998/049352 International Application No.: PCT/EP1998/002298
Publication Date: 05.11.1998 International Filing Date: 17.04.1998
Chapter 2 Demand Filed: 05.10.1998
IPC:
C21B 13/00 (2006.01)
C CHEMISTRY; METALLURGY
21
METALLURGY OF IRON
B
MANUFACTURE OF IRON OR STEEL
13
Making spongy iron or liquid steel, by direct processes
Applicants:
METALLGESELLSCHAFT AKTIENGESELLSCHAFT [DE/DE]; Bockenheimer Landstrasse 73 - 77 D-60325 Frankfurt am Main, DE (AT, AU, BE, BR, CA, CH, CY, DE, DK, ES, FI, FR, GB, GR, ID, IE, IT, KR, LU, MC, MX, NL, PT, RU, SE, TT, UA)
BEYZAVI, Ali [IR/DE]; DE (UsOnly)
HIRSCH, Martin [DE/DE]; DE (UsOnly)
Inventors:
BEYZAVI, Ali; DE
HIRSCH, Martin; DE
Agent:
METALLGESELLSCHAFT AKTIENGESELLSCHAFT; Bockenheimer Landstrasse 73 - 77 D-60325 Frankfurt am Main, DE
Common
Representative:
METALLGESELLSCHAFT AKTIENGESELLSCHAFT; Bockenheimer Landstrasse 73 - 77 D-60325 Frankfurt am Main, DE
Priority Data:
197 18 136.830.04.1997DE
Title (DE) VERFAHREN ZUM THERMISCHEN BEHANDELN VON KÖRNIGEM EISENERZ VOR DER REDUKTION
(EN) METHOD FOR THERMAL TREATMENT OF GRANULATED IRON ORE BEFORE REDUCTION
(FR) PROCEDE DE TRAITEMENT THERMIQUE DE MINERAI DE FER GRANULE AVANT REDUCTION
Abstract:
(DE) Das körnige feuchte Eisenerz wird zunächst durch eine Trocknungszone geleitet, wobei das Erz mit einer Temperatur von 120 bis 400 °C aus der Trocknungszone kommt. Anschließend wird das Erz im direkten Kontakt mit heißem Gas auf Temperaturen von 700 bis 1100 °C erhitzt, bevor man es einer Reduktionszone aufgibt. Das aus der Trocknungszone kommende Erz wird ganz oder teilweise durch eine Trenneinrichtung geführt, wobei man in eine grobkörnige und eine feinkörnige Erzfraktion trennt. Die feinkörnige Erzfraktion gibt man einer Granuliereinrichtung auf und erzeugt Eisenerzgranulat, welches man in die Trocknungszone führt. Die grobkörnige Erzfraktion wird auf Temperaturen von 700 bis 1100 °C erhitzt, bevor man sie in die Reduktionszone leitet.
(EN) The wet granulated iron ore is initially conducted through a drying zone. The ore leaves the drying zone at a temperature of 120-400 °C. The ore is then heated in direct contact with hot gas to temperatures of 700-1,100 °C before being delivered to a reduction zone. The ore coming out of the drying zone is fully or partially guided through a separating device so as to separate the ore into fine and coarse grain fractions. The fine-grained ore fraction is conveyed to a granulating device so as to produce an iron ore granulate which is conducted to the drying zone. The coarse-grained ore fraction is heated to temperatures of 700-1,100 °C before it is guided into the reduction zone.
(FR) Le minerai de fer humide granulé est tout d'abord guidé à travers une zone de séchage, d'où le fer ressort à une température comprise entre 120 et 400 °C. Le fer est ensuite mis en contact direct avec un gaz chaud pour être porté à des températures comprises entre 700 et 1100 °C, avant d'être placé dans une zone de réduction. Le fer qui sort de la zone de séchage est guidé en totalité ou en partie à travers un dispositif de séparation, pour dissocier le minerai en une fraction à gros grains et en une fraction à grains fins. La fraction à grains fins est placée dans un dispositif de granulation pour produire un granulat de minerai de fer qui est guidé dans la zone de séchage. La fraction à gros grains est portée à des températures comprises entre 700 et 1100 °C, avant d'être acheminée dans la zone de réduction.
front page image
Designated States: AU, BR, CA, ID, KR, MX, RU, TT, UA, US
European Patent Office (AT, BE, CH, CY, DE, DK, ES, FI, FR, GB, GR, IE, IT, LU, MC, NL, PT, SE)
Publication Language: German (DE)
Filing Language: German (DE)
Also published as:
MXPA/a/1999/010014KR1020010020393BRPI9809434AR010154EP0979313RU02203960
US6352572CA2288217AU1998076453MYPI 98001886ID024.813