1. (WO1998002271) ALLOY FOIL FOR LIQUID-PHASE DIFFUSION BONDING BONDABLE IN OXIDIZING ATMOSPHERE
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1998/002271    International Application No.:    PCT/JP1997/002422
Publication Date: 22.01.1998 International Filing Date: 11.07.1997
Chapter 2 Demand Filed:    04.12.1997    
IPC:
B23K 35/02 (2006.01), B23K 35/30 (2006.01)
Applicants: NIPPON STEEL CORPORATION [JP/JP]; 6-3, Otemachi 2-chome, Chiyoda-ku, Tokyo 100-71 (JP) (For All Designated States Except US).
HASEGAWA, Yasushi [JP/JP]; (JP) (For US Only).
TSURU, Eiji [JP/JP]; (JP) (For US Only).
SATOU, Yuuichi [JP/JP]; (JP) (For US Only).
OZAKI, Shigekatsu [JP/JP]; (JP) (For US Only)
Inventors: HASEGAWA, Yasushi; (JP).
TSURU, Eiji; (JP).
SATOU, Yuuichi; (JP).
OZAKI, Shigekatsu; (JP)
Agent: ISHIDA, Takashi; A. Aoki & Associates, Toranomon 37 Mori Building, 5-1, Toranomon 3-chome, Minato-ku, Tokyo 105 (JP)
Priority Data:
8/183603 12.07.1996 JP
Title (EN) ALLOY FOIL FOR LIQUID-PHASE DIFFUSION BONDING BONDABLE IN OXIDIZING ATMOSPHERE
(FR) FEUILLE METALLIQUE D'ALLIAGE POUR LIAISONS PAR DIFFUSION EN PHASE LIQUIDE SOUS ATMOSPHERE OXYDANTE
Abstract: front page image
(EN)A nickel-base alloy foil for liquid-phase diffusion bonding bondable in an oxidizing atmosphere which, when various alloys or iron-base materials are used as an object to be bonded, can ensure a joint having a homogeneous texture and a satisfactory joint strength in a short time in the air. The nickel-base alloy foil has a composition comprising indispensable diffusion elements of, in terms of atomic percentage, either 1.0 to 20.0 % of B or P or 1.0 to 20.0 % of B and 1.0 to 20.0 % of P, less than 0.5 to 15 % or less than 0.5 to 10.0 % of Si, and 0.1 to 20.0 % of V with the balance consisting essentially of Ni and unavoidable impurities, the thickness of the alloy foil being 3 to 100 m. If necessary, at least one member selected among Cr, Mn (or Mo), and Co and/or at least one member selected among W, Nb, and Ti may be incorporated each in a suitable amount. The crystal structure of the texture is substantially amorphous and more effective.
(FR)L'invention concerne une feuille métallique d'alliage à base de nickel pour assurer une liaison par diffusion en phase liquide, sous une atmosphère oxydante. Lorsque divers alliages ou matériaux à base de fer doivent être assemblés, cette feuille permet d'obtenir rapidement un assemblage présentant une texture homogène et une résistance satisfaisante à l'air. Cette feuille présente une composition comprenant des éléments de diffusion indispensables qui, en termes de pourcentage atomique, représentent 1,0 à 20,0 % de B ou P ou 1,0 à 20,0 % de B et 1,0 à 20,0 % de P; moins de 0,5 à 15 % ou moins de 0,5 à 10,0 % de Si, et 0,1 à 20,0 % de V, le reste se composant sensiblement de nickel et d'impuretés inévitables, et l'épaisseur de la feuille métallique d'alliage étant comprise entre 3 et 100 m. Si nécessaire, au moins un élément sélectionné parmi le Cr, Mn (ou Mo), et Co et/ou au moins un élément parmi W, Nb et Ti peuvent être incorporés chacun en une quantité appropriée. La structure cristalline de la texture est sensiblement amorphe et plus efficace.
Designated States: KR, US.
European Patent Office (AT, BE, CH, DE, DK, ES, FI, FR, GB, GR, IE, IT, LU, MC, NL, PT, SE).
Publication Language: Japanese (JA)