Machine translation
1. (WO1997039153) ALLOY HAVING HIGH CORROSION RESISTANCE IN ENVIRONMENT OF HIGH CORROSIVENESS, STEEL PIPE OF THE SAME ALLOY AND METHOD OF MANUFACTURING THE SAME STEEL PIPE
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1997/039153    International Application No.:    PCT/JP1997/001302
Publication Date: 23.10.1997 International Filing Date: 15.04.1997
IPC:
B22F 7/08 (2006.01), B32B 1/08 (2006.01), B32B 15/01 (2006.01), C21D 8/10 (2006.01), C22C 30/00 (2006.01), C22C 33/02 (2006.01), C22C 38/00 (2006.01), C22C 38/40 (2006.01), C22C 38/44 (2006.01)
Applicants: NIPPON STEEL CORPORATION [JP/JP]; 6-3, Otemachi 2-chome, Chiyoda-ku, Tokyo 100-71 (JP) (For All Designated States Except US).
ISHITSUKA, Tetsuo [JP/JP]; (JP) (For US Only).
NOSE, Koichi [JP/JP]; (JP) (For US Only)
Inventors: ISHITSUKA, Tetsuo; (JP).
NOSE, Koichi; (JP)
Agent: ISHIDA, Takashi; A. Aoki & Associates, Toranomon 37 Mori Building, 5-1, Toranomon 3-chome, Minato-ku, Tokyo 105 (JP)
Priority Data:
8/94547 16.04.1996 JP
8/193758 23.07.1996 JP
9/8106 20.01.1997 JP
Title (EN) ALLOY HAVING HIGH CORROSION RESISTANCE IN ENVIRONMENT OF HIGH CORROSIVENESS, STEEL PIPE OF THE SAME ALLOY AND METHOD OF MANUFACTURING THE SAME STEEL PIPE
(FR) ALLIAGE PRESENTANT UNE RESISTANCE ELEVEE A LA CORROSION DANS UN MILIEU EXTREMEMENT CORROSIF, CONDUIT EN ACIER FABRIQUE AVEC CET ALLIAGE ET PROCEDE DE FABRICATION DE CE CONDUIT
Abstract: front page image
(EN)An alloy of a high corrosion resistance used for a steel pipe for a boiler in equipment in which a fossil fuel or waste matter is burnt to generate energy, a steel pipe using this alloy, and a method of manufacturing the same steel pipe are provided. An alloy comprising not more than 0.05% of C, 1.0-2.6% of Si, 0.02-1.0% of Mn, 20.0-28.0% of Cr, 18.0-30.0% of Ni, not more than 4.0% of Mo, not more than 0.05% of Al, 0.05-0.30% of N, and the rest comprising Fe and unavoidable impurities. A double-layer steel pipe comprising a steel pipe for a standardized boiler as a base layer member, and this alloy as a material for a liner member; and a method of manufacturing the same steel pipe.
(FR)Alliage présentant une résistance élevée à la corrosion et utilisé pour fabriquer un conduit en acier pour une chaudière dans une installation dans laquelle un combustible fossile ou des déchets sont brûlés afin de générer de l'énergie, conduit en acier mettant cet alliage en application et procédé de fabrication dudit conduit. Alliage contenant une quantité égale à 0,05 % de C, 1-2,6 % de Si, 0,02-1 % de Mn, 20-28 % de Cr, 18-30 % de Ni, 4 % maximum de Mo, 0,05 % maximum de Al, 0,05-0,30 % de N et le reste composé de Fe et d'impuretés inévitables. Conduit en acier à double couche constitué par un conduit en acier conçu pour une chaudière normalisée en tant qu'élément de couche de base, et cet alliage en tant que matériau de l'élément de doublure; procédé de fabrication dudit conduit en acier.
Designated States: US.
European Patent Office (AT, BE, CH, DE, DK, ES, FI, FR, GB, GR, IE, IT, LU, MC, NL, PT, SE).
Publication Language: Japanese (JA)