1. (WO1997038061) METHOD OF MANUFACTURING AN OPTICAL COMPONENT
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1997/038061    International Application No.:    PCT/IB1997/000282
Publication Date: 16.10.1997 International Filing Date: 21.03.1997
IPC:
C09K 19/38 (2006.01), G02B 5/30 (2006.01)
Applicants: PHILIPS ELECTRONICS N.V. [NL/NL]; Groenewoudseweg 1, NL-5621 BA Eindhoven (NL).
PHILIPS NORDEN AB [SE/SE]; Kottbygatan 7, Kista, S-164 85 Stockholm (SE) (SE only)
Inventors: CAMPS, Ivo, Godgried, Jozef; (NL).
TOUWSLAGER, Fredericus, Johannes; (NL)
Agent: VAN DER VEER, Johannis, L.; Internationaal Octrooibureau B.V., P.O. Box 220, NL-5600 AE Eindhoven (NL)
Priority Data:
96200979.1 09.04.1996 EP
Title (EN) METHOD OF MANUFACTURING AN OPTICAL COMPONENT
(FR) PROCEDE DE FABRICATION D'UN ELEMENT OPTIQUE
Abstract: front page image
(EN)The invention relates to a method of manufacturing an optical component. In this method, a substrate, for example of glass, is successively provided with an orientation layer and an optically anisotropic layer of a material containing monomers which are provided with at least one covalently bonded reactive group, whereafter the optically anisotropic layer is polymerized. In accordance with the present invention, the applied orientation layer also comprises covalently bonded reactive groups. As a result, a good adhesion between the optically anisotropic layer and the orientation layer of the substrate is achieved. This has a favorable effect on the optical quality of the component. For the reactive groups use is preferably made of (meth)acrylate compounds which are polymerized by exposing them to radiation. Good results are achieved if for the orientation layer use is predominantly made of polyimide with covalently bonded reactive groups. Preferably, a glass plate is used as the substrate, and a bonding layer based on an organosilane compound is provided between the substrate and the orientation layer.
(FR)L'invention concerne un procédé servant à fabriquer un élément optique. Ce procédé consiste à recouvrir successivement un substrat en verre, par exemple, d'une couche d'orientation et d'une couche optiquement anisotrope d'un matériau contenant des monomères possédant au moins un groupe réactif à liaison covalente, puis à polymériser ladite couche optiquement anisotrope. D'après l'invention, la couche d'orientation appliquée comprend également des groupes réactifs à liaison covalente. Ceci permet d'obtenir une adhérence correcte entre la couche optiquement anisotrope et la couche d'orientation du substrat, ce qui exerce un effet favorable sur la qualité optique de l'élément. Pour les groupes réactifs, on utilise, de préférence, des composés de méthacrylate polymérisés par exposition à un rayonnement. On obtient des résultats avantageux en utilisant pour la couche d'orientation, de façon prédominante, du polyimide possédant des groupes réactifs à liaison covalente. On utilise, de préférence, une plaque de verre en tant que substrat et une couche d'adhérence à base d'un composé d'organosilane est située entre le substrat et la couche d'orientation.
Designated States: JP.
European Patent Office (AT, BE, CH, DE, DK, ES, FI, FR, GB, GR, IE, IT, LU, MC, NL, PT, SE).
Publication Language: English (EN)
Filing Language: English (EN)