1. (WO1997036956) HIGHLY SATURATED NITRILE COPOLYMER RUBBER, PROCESS FOR THE PRODUCTION THEREOF, HEAT-RESISTANT RUBBER COMPOSITIONS COMPRISING THE RUBBER AND COMPOSITES COMPRISING THE RUBBER AND FIBERS
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1997/036956    International Application No.:    PCT/JP1997/001099
Publication Date: 09.10.1997 International Filing Date: 31.03.1997
Chapter 2 Demand Filed:    22.09.1997    
IPC:
C08K 5/00 (2006.01), C08K 5/18 (2006.01), C08L 15/00 (2006.01)
Applicants: NIPPON ZEON CO., LTD. [JP/JP]; 6-1, Marunouchi 2-chome, Chiyoda-ku, Tokyo 100 (JP) (For All Designated States Except US).
FUJII, Yoshinori [JP/JP]; (JP) (For US Only).
IKEDA, Atsumi [JP/JP]; (JP) (For US Only)
Inventors: FUJII, Yoshinori; (JP).
IKEDA, Atsumi; (JP)
Agent: UCHIDA, Yukio; Uchida & Associates, Sunny Port Shiba 1005, 5-10, Shiba 2-chome, Minato-ku, Tokyo 105 (JP)
Priority Data:
8/104349 29.03.1996 JP
Title (EN) HIGHLY SATURATED NITRILE COPOLYMER RUBBER, PROCESS FOR THE PRODUCTION THEREOF, HEAT-RESISTANT RUBBER COMPOSITIONS COMPRISING THE RUBBER AND COMPOSITES COMPRISING THE RUBBER AND FIBERS
(FR) CAOUTCHOUC COPOLYMERE A BASE DE NITRILE HAUTEMENT SATURE, PROCEDE DE PRODUCTION, COMPOSITIONS DE CAOUTCHOUC RESISTANT A LA CHALEUR ET COMPRENANT LEDIT CAOUTCHOUC, ET MATERIAUX COMPOSITES COMPRENANT CE CAOUTCHOUC ET DES FIBRES
Abstract: front page image
(EN)A highly saturated nitrile copolymer rubber lowered in Mooney viscosity by 15 or more points by applying a high shearing stress thereto in the presence of an age resister, which has a Mooney viscosity of 5 to 135 and a ratio of weight-average molecular weight (Mw) to number-average molecular weight (Mn) of 3 to 5 and exhibits an increase in Mooney viscosity of as little as 10 or less points as measured after the rubber has been allowed to stand in the air at room temperature for 30 days after the above lowering of the Mooney viscosity. This rubber exhibits little viscosity change with the lapse of time and is excellent in processability and storage stability. The rubber can be blended with other heat-resistant rubbers to give heat-resistant rubber compositions, while it can be filled with fibers to give composites excellent in strength characteristics.
(FR)Cette invention concerne un caoutchouc copolymère à base de nitrile hautement saturé et dont l'indice de viscosité de Mooney a été abaissé de 15 points, ou plus, en exerçant des forces de cisaillement en présence d'un agent anti-vieillissement. Ce caoutchouc possède un indice de viscosité de Mooney variant entre 5 et 135, tandis que le rapport entre le poids moléculaire moyen en poids (Mw) et le poids moléculaire moyen en nombre (Mn) varie entre 3 et 5. L'indice de viscosité de Mooney n'augmente que de 10 points ou moins, tel que mesuré après l'exposition du caoutchouc à l'air libre et à température ambiante, une fois effectué l'abaissement susmentionné de l'indice de viscosité de Mooney. L'indice de viscosité de ce caoutchouc ne varie que très peu dans le temps, ce caoutchouc possédant d'excellentes caractéristiques de traitement ainsi qu'une excellente stabilité lors de son stockage. Ce caoutchouc peut être mélangé à d'autres caoutchoucs résistant à la chaleur de manière à obtenir des compositions de caoutchouc qui résistent à la chaleur; il peut encore être mélangé à des fibres de manière à fabriquer des matériaux composites possédant d'excellentes caractéristiques de résistance.
Designated States: JP, US.
European Patent Office (AT, BE, CH, DE, DK, ES, FI, FR, GB, GR, IE, IT, LU, MC, NL, PT, SE).