1. (WO1996009330) ULTRAHIGH-MOLECULAR-WEIGHT POLYETHYLENE MOLDING FOR ARTIFICIAL JOINT AND PROCESS FOR PRODUCING THE MOLDING
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1996/009330    International Application No.:    PCT/JP1995/001858
Publication Date: 28.03.1996 International Filing Date: 18.09.1995
IPC:
A61L 27/16 (2006.01), B29C 35/08 (2006.01), B29C 43/00 (2006.01), B29C 43/16 (2006.01), C08F 8/50 (2006.01), C08F 110/02 (2006.01)
Applicants: BMG Incorporated [JP/JP]; 45 Higashikujo Minamimatsunoki-cho, Minami-ku, Kyoto-shi, Kyoto 601 (JP) (For All Designated States Except US).
HYON, Suong-Hyu [--/JP]; (JP) (For US Only).
OKA, Masanori [JP/JP]; (JP) (For US Only)
Inventors: HYON, Suong-Hyu; (JP).
OKA, Masanori; (JP)
Agent: ASAHINA, Sohta; NS Building, 2-22, Tanimachi 2-chome, Chuo-ku, Osaka-shi, Osaka 540 (JP)
Priority Data:
6/254564 21.09.1994 JP
Title (EN) ULTRAHIGH-MOLECULAR-WEIGHT POLYETHYLENE MOLDING FOR ARTIFICIAL JOINT AND PROCESS FOR PRODUCING THE MOLDING
(FR) PIECE MOULEE EN POLYETHYLENE A POIDS MOLECULAIRE ULTRA ELEVE UTILE POUR LES ARTICULATIONS ARTIFICIELLES ET SON PROCEDE DE FABRICATION
Abstract: front page image
(EN)An ultrahigh-molecular-weight polyethylene molding for artificial joints, which has molecular or crystalline orientation, is lowly frictional and has an excellent wear resistance; and a process for producing the molding which comprises irradiating ultrahigh-molecular-weight polyethylene with a low-dose radiation to introduce a trace of cross-linking points into the molecular chain, melting the polymer at a high temperature near the melting point thereof, imparting compression deformation thereto, and solidifying the same by cooling.
(FR)Une pièce moulée en polyéthylène à poids moléculaire ultra élevée utile pour articulations artificielles présente une orientation cristalline ou moléculaire, un faible coefficient de friction et une excellente résistance à l'usure. Selon un procédé de production de cette pièce moulée, on irradie du polyéthylène à poids moléculaire ultra élevé avec une faible dose de rayonnements afin d'introduire des traces de points de réticulation croisée dans la chaîne moléculaire, on fait fondre le polymère à une température élevée proche de son point de fusion, on le déforme par compression avant de le refroidir pour de le solidifier.