1. (WO1994000384) PREPARATION OF ZEOLITES USING LOW SILICA/ALUMINA ZEOLITES AS A SOURCE OF ALUMINUM
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1994/000384    International Application No.:    PCT/US1993/006188
Publication Date: 06.01.1994 International Filing Date: 23.07.1993
IPC:
B01J 29/70 (2006.01), C01B 39/04 (2006.01), C01B 39/42 (2006.01), C01B 39/48 (2006.01)
Applicants: CHEVRON RESEARCH AND TECHNOLOGY COMPANY, A DIVISION OF CHEVRON U.S.A. INC. [US/US]; Post Office Box 7141, San Francisco, CA 94120-7141 (US)
Inventors: ZONES, Stacey; (US).
NAKAGAWA, Yumi; (US)
Agent: SHERIDAN, Richard, J.; Chevron Corporation, Law Department, Post Office Box 7141, San Francisco, CA 94120-7141 (US)
Priority Data:
Title (EN) PREPARATION OF ZEOLITES USING LOW SILICA/ALUMINA ZEOLITES AS A SOURCE OF ALUMINUM
(FR) PREPARATION DE ZEOLITES AU MOYEN DE ZEOLITES A FAIBLE TENEUR EN SILICE/ALUMINE EN TANT QUE SOURCE D'ALUMINIUM
Abstract: front page image
(EN)An improved method of synthesizing large pore zeolites is disclosed and claimed. The method comprises preparing a reaction mixture containing a source zeolite on alkali metal, nitrogen containing organic cation, a source of silica, and water, and having the following composition in terms of the mole ratios: M?+¿/SiO¿2? = 0.01-1.00, OH?-¿/SiO¿2? = 0.15-0.80, H¿2?O/SiO¿2? = 20-120; Q/SiO¿2? = 0.10-1.00, SiO¿2?/Y¿2?O¿3? = greater than 8; wherein M?+¿ is an alkali metal not supplied by the source zeolite, Q is an organic template, and Y is a mixture of aluminum from the source zeolite, wherein said source zeolite contains soda lite substructures having tetrahedra atom densities of less than about 15 TO¿2? per 1000 Å?3¿; maintaining the reaction mixture at crystallization temperature until crystals are formed; and recovering the crystals.
(FR)L'invention concerne un procédé amélioré de synthèse de zéolites présentant des pores de grande dimension. Le procédé comprend la préparation d'un mélange réactionnel contenant une zéolite source sur un métal alcalin, un cation organique contenant de l'azote, une source de silice et de l'eau, ledit mélange possédant la composition suivante exprimée en rapports molaires: M?+¿/SiO¿2? = 0.01-1.00; OH?-¿/SiO¿2? = 0.15-0.80; H¿2?O/SiO¿2? = 20-120; Q/SiO¿2? = 0.10-1.00; et SiO¿2?/Y¿2?O¿3? > 8; dans laquelle M?+¿ représente un métal alcalin non fourni par la zéolite source, Q représente un gabarit organique et Y représente un mélange d'aluminium provenant de la zéolite source, ladite zéolite source contenant des sous-structures de sodalite possédant des densités atomiques tétraédriques inférieures à 15 environ TO¿2? par 1000 Å?3¿; le maintien du mélange réactionnel à une température de cristallisation jusqu'à la formation de cristaux; la récupération des cristaux.