1. (WO1991008170) PROCESS FOR THE HYDROTHERMAL PRODUCTION OF POTASSIUM SILICATE SOLUTIONS.
Latest bibliographic data on file with the International Bureau

Pub. No.: WO/1991/008170 International Application No.: PCT/EP1990/001948
Publication Date: 13.06.1991 International Filing Date: 14.11.1990
Chapter 2 Demand Filed: 21.03.1991
IPC:
C01B 33/32 (2006.01)
C CHEMISTRY; METALLURGY
01
INORGANIC CHEMISTRY
B
NON-METALLIC ELEMENTS; COMPOUNDS THEREOF
33
Silicon; Compounds thereof
20
Silicates
32
Alkali metal silicates
Applicants:
HENKEL KOMMANDITGESELLSCHAFT AUF AKTIEN [DE/DE]; D-40191 Düsseldorf, DE (AllExceptUS)
NOVOTNY, Rudolf [DE/DE]; DE (UsOnly)
HOFF, Alfred [DE/DE]; DE (UsOnly)
SCHÜRTZ, Jost [DE/DE]; DE (UsOnly)
Inventors:
NOVOTNY, Rudolf; DE
HOFF, Alfred; DE
SCHÜRTZ, Jost; DE
Common
Representative:
HENKEL KOMMANDITGESELLSCHAFT AUF AKTIEN; TFP-Patentabteilung D-40191 Düsseldorf, DE
Priority Data:
P 39 38 789.523.11.1989DE
Title (DE) VERFAHREN ZUR HYDROTHERMALEN HERSTELLUNG VON KALIUMSILIKATLÖSUNGEN
(EN) PROCESS FOR THE HYDROTHERMAL PRODUCTION OF POTASSIUM SILICATE SOLUTIONS.
(FR) PROCEDE D'OBTENTION HYDROTHERMALE DE SOLUTIONS DE SILICATE DE POTASSIUM.
Abstract:
(DE) Offenbart wird ein Verfahren zur hydrothermalen Herstellung von Kaliumsilikatlösungen mit hohen SiO2 : K2O-Molverhältnissen, durch hydrothermale Umsetzung von Quarzsand mit wäßrigen Kaliumhydroxidlösungen bei Temperaturen im Bereich von 150 bis 300 °C und den diesen Temperaturen entsprechenden Drücken von gesättigtem Wasserdampf in einem Druckreaktor, das dadurch gekennzeichnet ist, daß man die hierbei erhaltenen Kaliumsilikatlösungen, die SiO2 : K2O-Molverhältnisse von weniger als 2,75 : 1 aufweisen, anschließend mit einem bei Temperaturen im Bereich von über 1100 °C bis zum Schmelzpunkt getemperten Quarz umsetzt, wobei gleichfalls Temperaturen und Drücke in den genannten Bereichen eingehalten werden.
(EN) The invention concerns a process for the hydrothermal production of potassium silicate solutions with high SiO2 mol ratios by the hydrothermal reaction of quartz sand with aqueous potassium hydroxide solutions in the range from 150 to 300 °C and the pressures of satured water vapour corresponding to these temperatures in a pressure reactor, in which the potassium silicate solutions thus obtained, which have SiO2:K2O mol ratios of less than 2.75:1, are then converted with a quartz tempered at temperatures in the range from over 1100 °C to the melting point, whereby the temperatures and pressures are also kept within the aforementioned ranges.
(FR) L'invention concerne un procédé d'obtention hydrothermale de solutions de silicate de potassium à rapports molaires SiO2:K2O élevés, par réaction hydrothermale du sable quartzeux avec des solutions aqueuses d'hydroxyde de potassium à des températures comprises entre 150 et 300 °C et sous des pressions de vapeur d'eau saturée correspondant à ces températures, en opérant dans un réacteur à pression, caractérisé en ce qu'on fait réagir ensuite les solutions de silicate de potassium ainsi obtenues, lesquelles présentent des rapports molaires SiO2:K2) inférieurs à 2,75:1, avec un quartz recuit à des températures comprises entre des valeurs supérieures à 1100 °C et le point de fusion, les températures et les pressions intervenant dans la réaction étant, de même, maintenues dans les plages précitées.
Designated States: AU, BR, CA, FI, HU, JP, KR, NO, RO, SU, US
European Patent Office (AT, BE, CH, DE, DK, ES, FR, GB, GR, IT, LU, NL, SE)
Publication Language: German (DE)
Filing Language: German (DE)
Also published as:
FI922321NO19921211ES2061226AR245425EP0502109US5238668
JPH05503067CA2069489AU1991069552DK0502109