1. (WO1987001107) METHOD FOR OBTAINING HYDROALUMINATE OF ALKALINE METAL
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1987/001107    International Application No.:    PCT/SU1985/000074
Publication Date: 26.02.1987 International Filing Date: 22.08.1985
IPC:
C01F 7/04 (2006.01), C01F 7/06 (2006.01)
Applicants: VSESOJUZNY NAUCHNO-ISSLEDOVATELSKY I PROEKTNY INST [SU/SU]; ITUT ALJUMINIEVOI, MAGNIEVOI I ELEKTRODNOI PROMYSH, LENNOSTI;, Sredny pr., 86;, Leningrad, 199026 (SU)
Inventors: RAIZMAN, Viktor Lazarevich; (SU).
VLASENKO, Jury Kuzmich; (SU).
KAZAKOV, Vladimir Grigorievich; (SU).
NISSE, Leonid Semenovich; (SU).
PEVZNER, Ilya Zakharovich; (SU).
VOLKOV, Vladimir Alexandrovich; (SU).
SIZYAKOV, Viktor Mikhailovich; (SU).
UDALOV, Valery Rafailovich; (SU).
POTAPOV, Nikolai Grigorievich; (SU).
SAZHIN, Viktor Sergeevich; (SU).
MALTS, Naum Solomonovich; (SU).
ABRAMOV, Vladimir Yakovlevich; (SU).
SABADASH, Nina Nikolaevna; (SU).
MOZZHUKHINA, Ljudmila Ivanovna; (SU)
Agent: THE USSR CHAMBER OF COMMERCE AND INDUSTRY; ul. Kuibysheva, 5/2, Moscow, 103012 (SU)
Priority Data:
Title (EN) METHOD FOR OBTAINING HYDROALUMINATE OF ALKALINE METAL
(FR) PROCEDE POUR L'OBTENTION D'HYDROALUMINATE D'UN METAL ALCALIN
Abstract: front page image
(EN)The method comprises leaching a raw material containing aluminium oxides and an alkaline metal while obtaining the alkaline solution which is then desiliconized and concentrated by evaporation, the alkaline solution with a molar ratio of the alkaline metal oxide and aluminium oxide Me2O:Al2O3 of 1.1-1.7 being the subject of that concentration by evaporation. The concentration by evaporation is effected at a temperature of 120-150oC up to a concentration of the alkaline metal oxide of 350-400 g/l. After concentration by evaporation the solution at a temperature of 95-150oC is subjected to crystallization on a moving filtration surface having a temperature of 10-95oC so that a rapid crystallization of the product and its separation from the mother liquor takes place on the filtration surface. The resulting mother liquor is returned for the leaching of the raw material.
(FR)Le procédé consiste à lessiver une matière première contenant des oxydes d'aluminium et un métal alcalin, pour obtenir une solution alcaline dont le silicium est éliminé et qui est concentrée par évaporation. La concentration par évaporation est réalisée sur une solution alcaline dont le rapport molaire oxyde métallique alcalin/oxyde d'aluminium Me2O:Al2O3 est de 1,1 à 1,7, et est effectuée à une température de 120 à 150oC jusqu'à une concentration de l'oxyde métallique alcalin de 350 à 400 g/l. Après concentration par évaporation, la solution dont la température est de 95 à 150oC est soumise à une cristallisation sur une surface de filtration mobile dont la température est de 10 à 95oC, de sorte qu'une cristallisation rapide du produit ainsi que sa séparation de la lessive-mère ont lieu sur la surface de filtration. La lessive-mère obtenue est recirculée en vue du lessivage de la matière première.