1. (WO1984004333) HIGH TEMPERATURE PRE-TREATMENT BY MEANS OF AN AQUEOUS ALCOLYNE SOLUTION OF CLAYISH GANGUE ORE CONTAINING AT LEAST ONE VALUABLE ELEMENT
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1984/004333    International Application No.:    PCT/FR1984/000110
Publication Date: 08.11.1984 International Filing Date: 18.04.1984
IPC:
C22B 3/14 (2006.01), C22B 3/22 (2006.01), C22B 34/22 (2006.01), C22B 34/34 (2006.01), C22B 60/02 (2006.01)
Applicants:
Inventors:
Priority Data:
  30.12.1899 null
Title (EN) HIGH TEMPERATURE PRE-TREATMENT BY MEANS OF AN AQUEOUS ALCOLYNE SOLUTION OF CLAYISH GANGUE ORE CONTAINING AT LEAST ONE VALUABLE ELEMENT
(FR) PRETRAITEMENT A HAUTE TEMPERATURE AU MOYEN D"UNE SOLUTION AQUEUSE ALCALINE DE MINERAIS A CHANGUE ARGILEUSE CONTENANT AU MOINS UN ELEMENT VALORISABLE
Abstract: front page image
(EN)High temperature pre-treatment process using a so called pre-treatment aqueous solution of crashed ore containing at least one valuable metal element of which the gangue contains clayish compounds capable of forming during the valorizing attack of the ore a water-stable plastic suspension making practically impossible to further separate the liquid phase from the solid phase due to its infiltrable and/or undecantable character, which is characterized in that, to cause a stabilisation of the clayish gangue before the valorizing attack of the ore and to obtain after the attack easy separations of the liquid and solid phases, the mineral ore, of which the grain size is at the most equal to the release mesh of the metal(s) to be valorized and before being subjected to the valorizing attack, is contacted with an aqueous pre-treatment solution containing at least 2.10-5 j/l of OH- ions and the medium thus formed is immediately brought at the minimum pre-treatment temperature of at least 120oC within 30 minutes at the most from the time where the ore is contacted with the aqueous pre-treatment solution.
(FR)Procédé de prétraitement à haute température au moyen d"une solution aqueuse dite de prétraitement, de minerais broyés contenant au moins un élément métallique valorisable dont la gangue contient des composés argileux susceptibles de former lors de l"attaque valorisante du minerai une suspension plastique stable en présence d"eau rendant pratiquement impossible la séparation ultérieure des phases liquide et solide en raison de son caractère infiltrable et/ou indécantable, qui se caractérise en ce que, pour provoquer une stabilisation de la gangue argileuse avant l"attaque valorisante du minerai et obtenir après l"attaque des séparations aisées des phases liquide et solide, le minerai, dont la granulométrie est au plus égale à la maille de libération du ou des métaux à valoriser et avant d"être soumis à l"attaque valorisante, est mis en contact avec une solution aqueuse de prétraitement contenant au moins 2.10-5g/l d"ions OH- puis le milieu formé est immédiatement porté à la température minimale de prétraitement d"au moins 120oC en un temps d"au plus 30 minutes compté à partir de la mise en contact du minerai avec la solution aqueuse de prétraitement.