1. (WO1983002253) A METHOD OF FORMING A YIELDABLE THERMAL BOND IN AN AUTOCLAVABLE MEDICAL PRODUCT IMPLEMENT AND THE LIKE
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1983/002253    International Application No.:    PCT/US1982/001512
Publication Date: 07.07.1983 International Filing Date: 25.10.1982
IPC:
A61J 1/05 (2006.01), A61M 5/158 (2006.01), B29C 65/76 (2006.01), C08J 5/12 (2006.01), C08K 5/54 (2006.01)
Applicants: BAXTER TRAVENOL LABORATORIES, INC. [US/US]; One Baxter Parkway, Deerfield, IL 60015 (US)
Inventors: GARVER, Sr., Edward, B.; (US).
ZABIELSKI, Kenneth, D.; (US)
Agent: RYAN, Daniel, D. @; One Baxter Parkway, Deerfield, IL 60015 (US)
Priority Data:
335,420 29.12.1981 US
Title (EN) A METHOD OF FORMING A YIELDABLE THERMAL BOND IN AN AUTOCLAVABLE MEDICAL PRODUCT IMPLEMENT AND THE LIKE
(FR) PROCEDE DE FORMAGE D'UNE LIAISON THERMIQUE SOUPLE DANS UN INSTRUMENT MEDICAL AUTO-CLAVABLE ET ANALOGUE
Abstract: front page image
(EN)The thermal bonding characteristics of a polyvinyl chloride series resin composition is altered by the incorporation of measured amounts of silicone and, preferably, coated calcium carbonate. This alteration of the resin composition permits the formation of a thermal bond (45) between the resin composition (46) and a compatible material (28), which bond is selectively breakable in response to the application of force which does not cause permanent deformation of the materials, regardless of repeated or prolonged heat exposure. The method is ideally suited for forming frangible connections (45) in medical product implements (10) which must undergo sterilization by autoclaving.
(FR)Les caractéristiques de liaison thermique d'une composition de résine de série de chlorure de polyvinyle sont modifiées par l'adjonction de quantités mesurées de silicone et, de préférence, de carbonate de calcium revêtu. Cette modification de la composition de la résine permet la formation d'un lien thermique (45) entre la composition de résine (46) et un matériau compatible (28), cette liaison étant cassable de manière sélective par l'application d'une force qui ne provoque pas une déformation permanente des matériaux, indépendamment de l'exposition répétée ou prolongée à la chaleur. Ce procédé convient idéalement à la formation de connexions cassables (45) dans des instruments médicaux (10) que l'on doit pouvoir stériliser par auto-clavage.
Designated States: AU, BR, JP.