1. (WO1981001298) A METHOD OF ACID PICKLING IRON AND IRON ALLOYS AND A COMPOSITION FOR CARRYING OUT THE METHOD
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1981/001298    International Application No.:    PCT/SE1980/000273
Publication Date: 14.05.1981 International Filing Date: 05.11.1980
IPC:
C23G 1/08 (2006.01)
Applicants:
Inventors:
Priority Data:
7909187 06.11.1979 SE
Title (EN) A METHOD OF ACID PICKLING IRON AND IRON ALLOYS AND A COMPOSITION FOR CARRYING OUT THE METHOD
(FR) PROCEDE DE DECAPAGE ACIDE DU FER ET DES ALLIAGES DE FER, ET COMPOSITION D"APPLICATION DU PROCEDE
Abstract: front page image
(EN)Method of acid pickling metallic material having an iron content of at least about 80 per cent by weight, while simultaneously inhibiting exposed metal surfaces against dissolution by acid attack. The method comprises bringing the material into contact with an aqueous solution containing phosphoric acid and one or both of the mineral acids hydrochloric acid and sulphuric acid. The phosphoric acid concentration is adjusted to at least about 0.01 mole per litre and at most about 1 mole per litre, while the total acid concentration is adjusted to the range between about 0.5 and 4 mole per litre. The invention also relates to a pickling agent for carrying out the method. The agent contains one or both of the mineral acids hydrochloric acid and sulphuric acid and has a total acid concentration of between about 0.5 and 4 mole per litre. The agent contains as an inhibitor phosphoric acid in an amount of at least about 0.01 mole per litre and at most about 1 mole per litre. The agent may also contain Fe (II)-ions.
(FR)Procede de decapage a l"acide d"un materiau metallique ayant une teneur en fer d"au moins 30% en poids environ, tout en inhibant simultanement les surfaces metalliques exposees contre la dissolution par l"attaque acide. Le procede consiste a amener le materiau en contact avec une solution aqueuse contenant de l"acide phosphorique et un ou les deux acides mineraux suivants: l"acide chlorhydrique et l"acide sulfurique. La concentration en acide phosphorique est ajustee en a moins 0,01 mole par litre environ et au plus 1 mole par litre environ, la concentration d"acide totale etant ajustee dans une plage comprise entre 0,5 et 4 moles par litre environ. Un agent de decapage permet l"application du procede. L"agent contient un ou les deux acides mineraux suivants: l"acide chlorhydrique et l"acide sulfurique, et possede une concentration en acide totale comprise entre 0,5 et 4 moles par litre environ. L"agent contient comme inhibiteur de l"acide phosphorique en une quantite comprise entre au moins 0,01 mole par litre environ et au plus 1 mole par litre environ. L"agent peut egalement contenir des ions Fe (II).