1. (WO1981000728) PURIFICATION PROCESS FOR SPENT PICKLING BATHS
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1981/000728    International Application No.:    PCT/SE1980/000220
Publication Date: 19.03.1981 International Filing Date: 04.09.1980
IPC:
B01J 41/04 (2006.01), C23C 2/30 (2006.01), C23G 1/36 (2006.01)
Applicants:
Inventors:
Priority Data:
7907619 13.09.1979 SE
Title (EN) PURIFICATION PROCESS FOR SPENT PICKLING BATHS
(FR) PROCEDE DE PURIFICATION DE BAINS DE DECAPAGE USES
Abstract: front page image
(EN)Purification process for spent, preferably hydrochloric acid based pickling baths, which have been used for pickling of steel articles in a hot dip galvanization process. Metal ions present in the pickling bath in the form of iron chloride complexes or zinc chloride complexes are brought in contact with an anion adsorbing material, preferably a conventional chloride ion-saturated anion exchanger, whereby the zinc chloride complex is selectively adsorbed. The solution containing the iron chloride complex can be used directly for the preparation of water purification chemicals. The ion exchanger is eluted or washed with water, whereby the zinc chloride complexes disintegrate, hydrochloric acid and zinc chloride are obtained in the washing solution, at the same time as the ion exchanger is regenerated while maintaining the same activity. The washing solution can, by a multistep washing in counter-current, be given a high enough concentration of zinc chloride so that it can be recirculated without further treatment to the flux bath in the hot dip galvanization process. If the chloride content of the spent pickling bath is not sufficient sot hat all metal ions will be present in complex form, this can be adjusted simply by addition of hydrochloric acid.
(FR)Procede de purification de bains de decapage uses de preference a base d"acide chlorhydrique, qui ont ete utilises pour le decapage d"articles en acier dans un procede de galvanisation par immersion a chaud. Les ions metalliques presents dans le bain de decapage sous forme de complexes de chlorure de fer ou de complexes de chlorure de zinc sont amenes au contact d"un materiau absorbant d"anions de preference un echangeur d"anions conventionnel sature d"ions chlorure, de maniere a absorber selectivement le complexe de chlorure de zinc. La solution contenant le complexe de chlorure de fer peut etre utilisee directement pour la preparation de produits chimiques de purification de l"eau. L"echangeur d"ions est elue ou lave a l"eau, ce qui entraine la dissociation des complexes de chlorure de zinc, et de l"acide chlorhydrique et du chlorure de zinc sont obtenus dans la solution de lavage, en meme temps que l"echangeur d"ions est regenere tout en maintenant la meme activite. La solution de lavage peut, par un lavage en plusieurs etapes a contre-courant, atteindre une concentration suffisamment elevee en chlorure de zinc pour qu"elle puisse etre ramenee sans traitement supplementaire au bain dans le procede de galvanisation par immersion a chaud. Si la teneur en chlorures du bain de decapage use n"est pas suffisante pour que tous les ions metalliques soient presents sous forme de complexes, elle peut etre ajustee simplement par addition d"acide chlorhydrique.