1. (WO1980000456) PROCESS FOR PRODUCING HIGH-STRENGTH COLD-ROLLED STEEL PLATE FOR PRESS WORKING
Latest bibliographic data on file with the International Bureau   

Pub. No.:    WO/1980/000456    International Application No.:    PCT/JP1979/000227
Publication Date: 20.03.1980 International Filing Date: 25.08.1979
IPC:
C21D 8/02 (2006.01), C21D 9/48 (2006.01), C22C 38/04 (2006.01)
Applicants:
Inventors:
Priority Data:
78/104172 26.08.1978 JP
Title (EN) PROCESS FOR PRODUCING HIGH-STRENGTH COLD-ROLLED STEEL PLATE FOR PRESS WORKING
(FR) PROCEDE DE PREPARATION DE TOLE D"ACIER LAMINEE A FROID A HAUTE RESISTANCE POUR LE TRAVAIL A LA PRESSE
Abstract: front page image
(EN)A process for producing a high-strength cold-rolled steel plate for press working having a tensile strength of 35-45 kg/mm2 and a yield ratio of 0.4-0.6, which comprises hot-rolling steel comprising 0.005-0.080% of C, not more than 0.30% of Si, 1.6-3.5% of Mn, 0.02-0.08% of sol. A1, 0.005-0.020% of N, and balance of Fe and unavoidable impurities, and, after cold-rolling, annealing at 660-750 C for not shorter than 30 minutes.
(FR)Procede de preparation de tole d"acier laminee a froid a haute resistance pour le travail a la presse ayant une resistance a la traction de 35-45 kg/m2 et un module d"elasticite de 0,4-0,6 qui comprend un acier lamine a chaud contenant 0,0005-0,080%, de C, pas plus de 0,30% de Si, 1,6-3,5% de Mn, 0,020-0,08% d"A1, 0,005-0,02% de N et le complement en Fe et impuretes inevitables et apres laminage a froid, l"on recuit a 660-750 C pendant au moins 30 minutes.