Processing

Please wait...

Settings

Settings

Goto Application

1. US20100307706 - REDUCED SHEAR CELLULOSE REACTIVE SIZING AGENT FOR WET END APPLICATIONS

Office United States of America
Application Number 11817722
Application Date 27.10.2005
Publication Number 20100307706
Publication Date 09.12.2010
Publication Kind A1
IPC
D21H 21/16
DTEXTILES; PAPER
21PAPER-MAKING; PRODUCTION OF CELLULOSE
HPULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C, D21D84; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G97; PAPER NOT OTHERWISE PROVIDED FOR
21Non-fibrous material added to the pulp, characterised by its function, form or properties; Paper impregnating or coating material, characterised by its function, form or properties
14characterised by function or properties in or on the paper
16Sizing or water-repelling agents
Applicants KEMIRA OYJ
Inventors Pawlowska Lucyna
Dilts Kimberly C.
Long Thomas
Hunter Charles R.
Proverb Robert
Agents CANTOR COLBURN LLP
Priority Data US05038609 27.10.2005 WO
Title
(EN) REDUCED SHEAR CELLULOSE REACTIVE SIZING AGENT FOR WET END APPLICATIONS
Abstract
(EN)

The invention relates to a method for sizing a paper product that involves the steps of (a) providing a paper stock system; (b) forming, in the absence of high shearing forces, an aqueous sizing emulsion comprising an alkenylsuccinic anhydride component; (c) submitting the emulsion formed from step b to a post-dilution step in the presence of a cationic component under conditions, in the absence of high shearing forces, that produce a post-diluted emulsion having improved sizing efficacy; (d) adding the post-diluted emulsion to the paper stock; and (e) forming a paper web.