PATENTSCOPE will be unavailable a few hours for maintenance reason on Tuesday 19.11.2019 at 4:00 PM CET
Search International and National Patent Collections
Some content of this application is unavailable at the moment.
If this situation persists, please contact us atFeedback&Contact
1. (KR1020180067637) 고순도 5염화텅스텐 및 그 합성 방법

Office : Republic of Korea
Application Number: 1020187013467 Application Date: 13.01.2017
Publication Number: 1020180067637 Publication Date: 20.06.2018
Publication Kind : A
Prior PCT appl.: Application Number: ; Publication Number:WO2017130745 Click to see the data
IPC:
C01G 41/04
C CHEMISTRY; METALLURGY
01
INORGANIC CHEMISTRY
G
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F94
41
Compounds of tungsten
04
Halides
Applicants: 제이엑스금속주식회사
Inventors: 다카하시 히데유키
모모이 하지메
Agents: 특허법인코리아나
Priority Data: JP-P-2016-014662 28.01.2016 JP
Title: (KO) 고순도 5염화텅스텐 및 그 합성 방법
Abstract:
(KO) Bi, Hg, Sb, Ti, Al, P, As 로 이루어지는 군에서 선택된 환원제와, 6염화텅스텐을, 6염화텅스텐 : 환원제의 몰비가 2.8 : 1.0 ∼ 3.2 : 1.0 으로, 불활성 분위기 중에서 균일하게 혼합하여, 혼합물을 얻는 공정, 환원제와 6염화텅스텐의 혼합물을, 13 ㎩ 이하에서 80 ∼ 210 ℃ 로 가열하여 환원시키는 공정, 환원제와 6염화텅스텐의 혼합물의 환원물을, 66 ㎩ 이하에서 120 ∼ 290 ℃ 로 가열하고, 감압 증류시켜 불순물을 제거하는 공정, 감압 증류에 의해 불순물 제거된 환원물을, 13 ㎩ 이하에서 140 ∼ 350 ℃ 로 가열하고, 승화 정제하여, 5염화텅스텐을 얻는 공정을 포함하는, 5염화텅스텐의 제조 방법에 의해, 종래보다 고수율이며 안전하게, 고순도 5염화텅스텐을 합성한다.