1. JP2020089862 - 塗膜の形成方法

Office Japan
Application Number 2018230171
Application Date 07.12.2018
Publication Number 2020089862
Publication Date 11.06.2020
Publication Kind A
IPC
B05D 1/36
BPERFORMING OPERATIONS; TRANSPORTING
05SPRAYING OR ATOMISING IN GENERAL; APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL
DPROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL
1Processes for applying liquids or other fluent materials
36Successively applying liquids or other fluent materials, e.g. without intermediate treatment
B05D 3/00
BPERFORMING OPERATIONS; TRANSPORTING
05SPRAYING OR ATOMISING IN GENERAL; APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL
DPROCESSES FOR APPLYING LIQUIDS OR OTHER FLUENT MATERIALS TO SURFACES, IN GENERAL
3Pretreatment of surfaces to which liquids or other fluent materials are to be applied; After-treatment of applied coatings, e.g. intermediate treating of an applied coating preparatory to subsequent applications of liquids or other fluent materials
Applicants 花王株式会社
Inventors 福田 輝幸
Agents 片岡 誠
佐々木 渉
大竹 有美子
Title
(JA) 塗膜の形成方法
Abstract
(JA)

【課題】簡便でかつ精密に光学的な特性を発揮し得る塗膜の形成方法を提供する。
【解決手段】溶媒A、溶媒B、及びポリマーCを含有する液体組成物Iを基材に付与する工程1と、工程1で付与された基材上の液体組成物Iに、水を含有する液体IIの液滴を付与する工程2とを含み、該溶媒Aの沸点が99℃未満であり、該溶媒Aの水に対するハンセン溶解度パラメータの距離Raが36以下であり、該溶媒Bの沸点が150℃以上であり、該溶媒Bの水に対するハンセン溶解度パラメータの距離Raが40以上であり、該溶媒Bが該溶媒Aと相溶し、かつ該ポリマーCが該溶媒Aに可溶で該溶媒Bに不溶であり、該液滴の平均直径dが0.01μm以上50μm以下である、塗膜の形成方法である。
【選択図】なし