1. IN3545/DELNP/2013 - CONDUCTIVE ANILINE POLYMER METHOD FOR PRODUCING SAME AND METHOD FOR PRODUCING CONDUCTIVE FILM

Office India
Application Number 3545/DELNP/2013
Application Date 22.04.2013
Publication Number 3545/DELNP/2013
Publication Date 14.11.2014
Publication Kind A
IPC
C08G 73/00
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
GMACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
73Macromolecular compounds obtained by reactions forming in the main chain of the macromolecule a linkage containing nitrogen, with or without oxygen or carbon, not provided for in groups C08G12/-C08G71/238
C08J 5/18
CCHEMISTRY; METALLURGY
08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
JWORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H142
5Manufacture of articles or shaped materials containing macromolecular substances
18Manufacture of films or sheets
Applicants Mitsubishi Rayon Co. Ltd.
Inventors YAMADA Kohei
HORIUCHI Yasushi
HACHIYA Yukiko
UZAWA Masashi
SAKAI Takahiro
TAKAGI Tamae
Priority Data 2010240039 26.10.2010 JP
2011006849 17.01.2011 JP
2011032053 17.02.2011 JP
2011071517 29.03.2011 JP
2011083579 05.04.2011 JP
Title
(EN) CONDUCTIVE ANILINE POLYMER METHOD FOR PRODUCING SAME AND METHOD FOR PRODUCING CONDUCTIVE FILM
Abstract
(EN)
When measuring the molecular mass distribution of conductive anilinepolymer of formula (1) by GPC and converting its retention time into molecular mass(M) in terms of sodium polystyrene sulfonate, for the molecular mass (M), the area ratio(X/Y) of the area (X) of a region of 15,000 Da or more to the area (Y) of a region of lessthan 15,000 Da is 1.20 or more. A method for producing such a polymer includes:^ t polymerization step (Zl) where specific aniline derivative (A) is polymerized in asolution containing basic compound (B), solvent (C), and oxidizing agent (D) at a liquidtemperature lower than 25 °C; or polymerization step (Z2) where specific anilinederivative (A) and oxidizing agent (D) are added to and polymerized in a solution of aconductive aniline polymer (P-l) with a unit of formula (1) dissolved or dispersed in asolvent (C). [Chemical formula 1]