1. (WO2009033465) VERFAHREN ZUR HERSTELLUNG CARBOXYLIERTER ETHYLENPOLYMERBLENDS
Aktuellste beim Internationalen Büro vorliegende bibliographische Daten   

TranslationÜbersetzung: Original-->Deutsch
Veröff.-Nr.:    WO/2009/033465    Internationale Veröffentlichungsnummer:    PCT/DE2008/001506
Veröffentlichungsdatum: 19.03.2009 Internationales Anmeldedatum: 09.09.2008
IPC:
C08F 2/36 (2006.01), C08F 255/02 (2006.01), C08F 255/04 (2006.01), C08L 23/04 (2006.01), C08L 51/06 (2006.01)
Anmelder: KOMETRA KUNSTSTOFF-MODIFIKATOREN UND -ADDITIV GMBH [DE/DE]; Friedensstr. 1, 06429 Neugattersleben (DE) (For All Designated States Except US).
BESSER, Klaus [DE/DE]; (DE) (For US Only).
GERECKE, Jochen [DE/DE]; (DE) (For US Only).
HÄUSSLER, Lutz [DE/DE]; (DE) (For US Only).
LEITNER, Bianka [DE/DE]; (DE) (For US Only).
RAPTHEL, Inno [DE/DE]; (DE) (For US Only)
Erfinder: BESSER, Klaus; (DE).
GERECKE, Jochen; (DE).
HÄUSSLER, Lutz; (DE).
LEITNER, Bianka; (DE).
RAPTHEL, Inno; (DE)
Vertreter: SPERLING, FISCHER & HEYNER; Bruno-Wille-Str. 9, 39108 Magdeburg (DE)
Prioritätsdaten:
10 2007 043 972.7 11.09.2007 DE
Titel (DE) VERFAHREN ZUR HERSTELLUNG CARBOXYLIERTER ETHYLENPOLYMERBLENDS
(EN) METHOD FOR PRODUCING CARBOXYLATED ETHYLENE POLYMER BLENDS
(FR) PROCÉDÉ DE PRODUCTION DE MÉLANGES DE POLYMÈRES D'ÉTHYLÈNE CARBOXYLÉS
Zusammenfassung: front page image
(DE)Verfahren zur Herstellung carboxylierter Ethylenpolymerblends, indem in einer 1. Stufe in einem Fluidmischreaktor auf 100 Masseteile eines unter Ethylenhomo- (HDPE, LDPE) und/oder linearen Ethylencopolymeren mit 2 bis ≤ 20 Masse-% einpolymerisierten C3- bis C12-Olefineinheiten (LLDPE, EOP) ausgewählten partikulären Ethylenpolymers mit einer Schmelzflussrate MFR (190 °C/2,16 kg) ≥ 20 g/10 min 0,05 bis 15 Masseteile einer α,ß-ethylenisch ungesättigten Mono- und/oder Dicarbonsäure bzw. deren Anhydrid (Carboxylmonomer) oder einer mindestens ein Carboxylmonomer enthaltenden Monomermischung sowie 0,01 bis 10 Masseteile eines radikalischen Initiators oder Initiatorgemischs hinzugefügt und bei Reaktionstemperaturen zwischen 30 und 120 °C über eine Reaktionszeit zwischen 5 und 120 min pfropfpolymerisiert und anschließend in einer 2. Stufe ein Gemisch aus 100 Masseteilen des in der 1. Festphasenstufe erhaltenen modifizierten Ethylenpolymers, 150 bis 4000 Masseteilen eines eine Schmelzflussrate MFR (190 °C/2,16 kg) < 20 g/10 min aufweisenden Ethylenpolymers oder -polymerblends sowie 0 bis 4000 Masseteilen eines olefinischen Elastomers kontinuierlich einem Reaktionsextruder zugeführt, bei Temperaturen zwischen 160 und 260 °C umgesetzt und das einen Carboxylierungsgrad zwischen 0,05 und 1 Masse-% besitzende pfropfmodifizierte Ethylenpolymerblend kontinuierlich ausgetragen wird. Die erhaltenen Produkte sind besonders als Haftvermittler und/oder Klebemittel für verschiedene Unterlagen, vorzugsweise auf und zwischen metallischen Oberflächen, geeignet.
(EN)The invention relates to a method for producing carboxylated ethylene polymer blends by adding 0.05 to 15 parts by weight of an α,ß-ethylenically unsaturated mono- and/or dicarboxylic acid or the anhydride thereof (carboxylic monomer) or a monomer mixture containing at least one carboxylic monomer and 0.01 to 10 parts by weight of a radical initiator or initiator mixture in a first stage in a fluid mixer to 100 parts by weight of a particulate ethylene polymer having a melt flow rate MFR (190 °C/2.16 kg) ≥ 20 g/10 min, said ethylene polymer being selected from ethylene homopolymers (HDPE, LDPE) and/or linear ethylene copolymers with 2 to ≤ 20% by weight of C3 to C12 olefin units (LLDPE, EOP) polymerized into it, and graft-polymerizing said mixture for a reaction time of between 5 and 120 min at a reaction temperature of between 30 and 120°C. In a second stage, a mixture of 100 parts by weight of the modified ethylene polymer obtained in the first solid phase stage, 150 to 4000 parts by weight of an ethylene polymer or ethylene polymer blend having a melt flow rate MFR (190 °C/2.16 kg) < 20 g/10 min and 0 to 4000 parts by weight of an olefinic elastomer are continuously added to a reaction extruder, reacted at temperatures of between 160 and 260 °C and the graft-modified ethylene polymer blend having a carboxylation degree of between 0.05 and 1% by weight is continuously extruded. The products so obtained are especially useful as bonding agents and/or adhesives for various bases, preferably on and between metal surfaces.
(FR)Procédé de production de mélanges de polymères d'éthylène carboxylés, caractérisé en ce que, dans une première étape, on introduit dans un réacteur à mélange de fluide, pour 100 parties en masse d'un polymère d'éthylène en particules, ayant un indice de fluidité à chaud MFR (190°C/2,16 kg) ≥ 20 g/10 min, sélectionné à partir d'homopolymères d'éthylène (HDPE, LDPE) et/ou de copolymères d'éthylène linéaires à motifs oléfine en C3 à C12 (LLDPE, EOP) copolymérisés à 2 à ≤ 20% en masse, 0,05 à 15 parties en masse d'un acide monocarboxylique et/ou dicarboxylique éthyléniquement insaturé en α, β, ou de son anhydride (monomère carboxylé), ou d'un mélange monomère renfermant au moins un monomère carboxylé, et 0,01 à 10 parties en masse d'un initiateur radicalaire ou d'un mélange d'initiateurs radicalaires, en ce qu'on polymérise avec greffage le produit obtenu, à des températures de réaction comprises entre 30 et 120°C, et pendant une durée de réaction de 5 à 120 minutes, et en ce que, dans une seconde étape, on introduit en continu, dans un extrudeur de réaction, un mélange comprenant 100 parties en masse du polymère d'éthylène modifié, obtenu dans la première étape en phase solide, 150 à 4000 parties en masse d'un polymère d'éthylène présentant un indice de fluidité à chaud MFR (190°C/2,16 kg) < 20 g/10 min, ou d'un mélange de tels polymères, et 0 à 4000 parties en masse d'un élastomère oléfinique, en ce qu'on fait réagir le produit à des températures comprises entre 160 et 260 °C, et en ce qu'on recueille en continu le mélange de polymère d'éthylène modifié par greffage, présentant un degré de carboxylation compris entre 0,05 et 1 % en masse. Les produits obtenus conviennent pour l'utilisation comme promoteurs d'adhérence et/ou comme agents adhésifs pour différents substrats, de préférence sur/et entre / des surfaces métalliques.
Designierte Staaten: AE, AG, AL, AM, AO, AT, AU, AZ, BA, BB, BG, BH, BR, BW, BY, BZ, CA, CH, CN, CO, CR, CU, CZ, DK, DM, DO, DZ, EC, EE, EG, ES, FI, GB, GD, GE, GH, GM, GT, HN, HR, HU, ID, IL, IN, IS, JP, KE, KG, KM, KN, KP, KR, KZ, LA, LC, LK, LR, LS, LT, LU, LY, MA, MD, ME, MG, MK, MN, MW, MX, MY, MZ, NA, NG, NI, NO, NZ, OM, PG, PH, PL, PT, RO, RS, RU, SC, SD, SE, SG, SK, SL, SM, ST, SV, SY, TJ, TM, TN, TR, TT, TZ, UA, UG, US, UZ, VC, VN, ZA, ZM, ZW.
African Regional Intellectual Property Organization (BW, GH, GM, KE, LS, MW, MZ, NA, SD, SL, SZ, TZ, UG, ZM, ZW)
Eurasian Patent Organization (AM, AZ, BY, KG, KZ, MD, RU, TJ, TM)
European Patent Office (AT, BE, BG, CH, CY, CZ, DE, DK, EE, ES, FI, FR, GB, GR, HR, HU, IE, IS, IT, LT, LU, LV, MC, MT, NL, NO, PL, PT, RO, SE, SI, SK, TR)
African Intellectual Property Organization (BF, BJ, CF, CG, CI, CM, GA, GN, GQ, GW, ML, MR, NE, SN, TD, TG).
Veröffentlichungssprache: German (DE)
Anmeldesprache: German (DE)